# US 2010/0248466 A1 · Method for making a stressed non-volatile memory device

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2010/0248466 A1
- Document ID: US20100248466A1
- Status: Published application
- Kind: A1
- Application number: 12/414,778
- Filed: 2009-03-31
- Published: 2010-09-30
- Earliest claimed: 2009-03-31
- Assignees: Freescale Semiconductor, Inc.
- Inventors: Konstantin V. Loiko; Brian A. Winstead; Taras A. Kirichenko
- Web page: https://patentgrep.com/patent/US20100248466A1

## CPC

- H10D 30/681: {having only two programming levels (Floating gate IGFETs programmable by two single electrons H10D30/688)}
- B82Y 10/00: Nanotechnology for information processing, storage or transmission, e.g. quantum computing or single electron logic
- H10D 30/6892: {having at least one additional gate other than the floating gate and the control gate, e.g. program gate, erase gate or select gate}
- H10D 30/796: {having memorised stress for introducing strain in the channel regions, e.g. recrystallised polysilicon gates}
- H10D 64/035: {comprising conductor-insulator-conductor-insulator-semiconductor structures}
- H10D: INORGANIC ELECTRIC SEMICONDUCTOR DEVICES
- B82Y: SPECIFIC USES OR APPLICATIONS OF NANOSTRUCTURES; MEASUREMENT OR ANALYSIS OF NANOSTRUCTURES; MANUFACTURE OR TREATMENT OF NANOSTRUCTURES

## Abstract

A method of making a semiconductor device on a semiconductor layer includes: forming a gate dielectric over the semiconductor layer; forming a layer of gate material over the gate dielectric; etching the layer of gate material to form a select gate; forming a storage layer that extends over the select gate and over a portion of the semiconductor layer; depositing an amorphous silicon layer over the storage layer; etching the amorphous silicon layer to form a control gate; and annealing the semiconductor device to crystallize the amorphous silicon layer.

## Claims

### Claim 1

A method of making a semiconductor device on a semiconductor layer, comprising:
forming a gate dielectric over the semiconductor layer;
forming a layer of gate material over the gate dielectric;
etching the layer of gate material to form a select gate;
forming a storage layer that extends over the select gate and over a portion of the semiconductor layer;
depositing an amorphous silicon layer over the storage layer;
etching the amorphous silicon layer to form a control gate; and
annealing the semiconductor device to crystallize the amorphous silicon layer.

### Claim 2 (depends on 1)

The method of claim 1, further comprising forming a capping layer over the semiconductor device, the capping layer formed prior to the step of annealing the semiconductor device.

### Claim 3 (depends on 2)

The method of claim 2, further comprising removing the capping layer from over the semiconductor device after the step of annealing the semiconductor device.

### Claim 4 (depends on 2)

The method of claim 2, wherein forming the capping layer further comprises forming a capping layer that causes a channel region in the semiconductor layer to be laterally tensile stressed.

### Claim 5 (depends on 2)

The method of claim 2, wherein forming the capping layer further comprises forming the capping layer from tensile stressed silicon nitride.

### Claim 6 (depends on 1)

The method of claim 1, wherein the step of depositing a silicon layer comprises sputtering silicon and an impurity, wherein the impurity comprises one of group consisting of nickel, gold, aluminum, silver, and palladium.

### Claim 7 (depends on 1)

The method of claim 1, wherein annealing the semiconductor device to crystallize the amorphous silicon layer further comprises annealing the semiconductor device at a temperature in a range of 500 to 1100 degrees Celsius.

### Claim 8 (depends on 1)

The method of claim 1, wherein depositing the amorphous silicon layer over the storage layer further comprises depositing the amorphous silicon layer to have a thickness in a range of 50 to 250 nanometers.

### Claim 9 (depends on 1)

The method of claim 1, wherein etching the amorphous silicon layer to form the control gate further comprises etching the amorphous silicon layer to form the control gate having a portion formed over a portion of the select gate.

### Claim 10 (depends on 1)

The method of claim 1, wherein forming the storage layer is further characterized by the storage layer comprising nanocrystals.

### Claim 11 (depends on 1)

The method of claim 1, wherein the step of depositing the amorphous silicon layer is performed by sputtering.

### Claim 12

A method of making a semiconductor device on a semiconductor layer, comprising:
forming a gate dielectric over the semiconductor layer;
forming a layer of gate material over the gate dielectric;
etching the layer of gate material to form a select gate;
forming a charge storage layer that extends over the select gate and over a portion of the semiconductor layer;
depositing an amorphous silicon layer over the charge storage layer;
etching the amorphous silicon layer to form a control gate;
forming a liner on the semiconductor device;
forming a capping layer over the liner; and
annealing the semiconductor device to crystallize the amorphous silicon layer.

### Claim 13 (depends on 12)

The method of claim 12, further comprising removing the capping layer from over the semiconductor device after the step of annealing the semiconductor device.

### Claim 14 (depends on 12)

The method of claim 12 wherein forming the capping layer further comprises forming the capping layer from tensile stressed silicon nitride.

### Claim 15 (depends on 12)

The method of claim 12, wherein forming the capping layer further comprises depositing a silicon nitride layer having a thickness in a range of 20 to 200 nanometers.

### Claim 16 (depends on 12)

The method of claim 12, wherein annealing the semiconductor device to crystallize the amorphous silicon layer further comprises annealing the semiconductor device at a temperature in a range of 500 to 1100 degrees Celsius.

### Claim 17 (depends on 12)

The method of claim 12, wherein depositing the amorphous silicon layer over the charge storage layer is further characterized by sputtering silicon and an impurity.

### Claim 18 (depends on 12)

The method of claim 12, wherein forming the charge storage layer is further characterized by the charge storage layer comprising nanocrystals.

### Claim 19

A method of making a semiconductor device on a semiconductor layer, comprising:
forming a gate dielectric over the semiconductor layer;
forming a polysilicon layer over the gate dielectric;
etching the polysilicon layer to form a select gate;
forming a charge storage layer that extends over the select gate and over a portion of the semiconductor layer, wherein the charge storage layer comprises nanocrystals;
depositing an amorphous silicon layer over the charge storage layer;
etching the amorphous silicon layer to form a control gate, the control gate having a portion formed over a portion of the select gate;
forming an insulating liner on the semiconductor device;
forming a tensile stressed silicon nitride layer over the insulating liner;
annealing the semiconductor device to crystallize the amorphous silicon layer; and
removing the tensile stressed silicon nitride layer.

### Claim 20 (depends on 19)

The method of claim 19, wherein:
forming the tensile stressed silicon nitride layer further comprises depositing a silicon nitride layer having a thickness in a range of 20 to 200 nanometers;
annealing the semiconductor device to crystallize the amorphous silicon layer further comprises annealing the semiconductor device at a temperature in a range of 500 to 1100 degrees Celsius; and
depositing the amorphous silicon layer over the charge storage layer is by sputtering.