# US 2010/0247778 A1 · Process for producing polyurethane coated gloves

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2010/0247778 A1
- Document ID: US20100247778A1
- Status: Published application
- Kind: A1
- Application number: 12/418,254
- Filed: 2009-04-03
- Published: 2010-09-30
- Earliest claimed: 2009-03-30
- Inventors: Xiaolin Sha
- Web page: https://patentgrep.com/patent/US20100247778A1

## CPC

- C09D 175/04: Polyurethanes
- A41D 19/0065: {with a textile layer underneath}
- C09D: COATING COMPOSITIONS, e.g. PAINTS, VARNISHES OR LACQUERS; FILLING PASTES; CHEMICAL PAINT OR INK REMOVERS; INKS; CORRECTING FLUIDS; WOODSTAINS; PASTES OR SOLIDS FOR COLOURING OR PRINTING; USE OF MATERIALS THEREFOR (cosmetics A61K; processes for applying liquids or other fluent materials to surfaces, in general, B05D; staining wood B27K5/02; glazes or vitreous enamels C03C; natural resins, French polish, drying-oils, driers, turpentine, per se, C09F; polishing compositions other than French polish, ski waxes C09G; adhesives or use of materials as adhesives C09J; materials for sealing or packing joints or covers C09K3/10; materials for stopping leaks C09K3/12; processes for the electrolytic or electrophoretic production of coatings C25D)
- A41D: OUTERWEAR; PROTECTIVE GARMENTS; ACCESSORIES

## Abstract

A process for producing a polyurethane coated glove includes steps of: coating a knitted glove with a solvent, wherein the solvent is prepared by a polyurethane resin and a component selected from the group consisting of N-methyl pyrrolidone (NMP), dimethylacetamide (DMAC), and dimethyl sulfoxide (DMSO), wherein the component participates in synthesizing the polyurethane resin; treating the knitted glove with water bath; drying the knitted glove under 100˜110° C., for 50˜60 minutes; and recycling the component in the solvent from the water after treating with water bath by vacuum decompression.

## Claims

### Claim 1

A process for producing a polyurethane coated glove, comprising steps of:
(a) coating a knitted glove with a solvent, wherein the solvent is prepared by a polyurethane resin and a component selected from the group consisting of N-methyl pyrrolidone, dimethylacetamide, and dimethyl sulfoxide, wherein the component participates in synthesizing the polyurethane resin; and
(b) treating the knitted glove with water bath.

### Claim 2 (depends on 1)

The process, as recited in claim 1, wherein step (a) comprises: (a.1) dipping the knitted glove into the solvent for 10˜60 s, and (a.2) flushing the knitted glove for 1˜10 minutes.

### Claim 3 (depends on 1)

The process, as recited in claim 1, wherein the knitted glove is treated with the water bath in three sinks, wherein the first sink has a water temperature of 30˜35° C., each of the second and the third sinks has a water temperature of 50˜55° C.

### Claim 4 (depends on 2)

The process, as recited in claim 2, wherein the knitted glove is treated with the water bath in three sinks, wherein the first sink has a water temperature of 30˜35° C., each of the second and the third sinks has a water temperature of 50˜55° C.

### Claim 5 (depends on 1)

The process, as recited in claim 1, further comprising: after step (b), drying the knitted glove under 100˜110° C., for 50˜60 minutes.

### Claim 6 (depends on 4)

The process, as recited in claim 4, further comprising: after step (b), drying the knitted glove under 100˜110° C., for 50˜60 minutes.

### Claim 7 (depends on 1)

The process, as recited in claim 1, further comprising: after step (b), recycling the component in the solvent from the water by vacuum decompression.

### Claim 8 (depends on 6)

The process, as recited in claim 6, further comprising: after step (b), recycling the component in the solvent from the water by vacuum decompression.

### Claim 9 (depends on 1)

The process, as recited in claim 1, wherein the component is the N-methyl pyrrolidone, wherein a ratio of the polyurethane resin to the N-methyl pyrrolidone is 1:1.3˜1:1.8, and a viscosity of the solvent is 500˜600 poise.

### Claim 10 (depends on 8)

The process, as recited in claim 8, wherein the component is the N-methyl pyrrolidone, wherein a ratio of the polyurethane resin to the N-methyl pyrrolidone is 1:1.3˜1:1.8, and a viscosity of the solvent is 500˜600 poise.

### Claim 11 (depends on 1)

The process, as recited in claim 1, wherein the component is the dimethylacetamide, wherein a ratio of the polyurethane resin to the dimethylacetamide is 1:1.3˜1:1.9, and a viscosity of the solvent is 500˜600 poise.

### Claim 12 (depends on 8)

The process, as recited in claim 8, wherein the component is the dimethylacetamide, wherein a ratio of the polyurethane resin to the dimethylacetamide is 1:1.3˜1:1.9, and a viscosity of the solvent is 500˜600 poise.

### Claim 13 (depends on 1)

The process, as recited in claim 1, wherein the component is the dimethyl sulfoxide, a ratio of the polyurethane resin to the dimethyl sulfoxide is 1:1.4˜1:1.9, and a viscosity of the solvent is 500˜600 poise.

### Claim 14 (depends on 8)

The process, as recited in claim 8, wherein the component is the dimethyl sulfoxide, wherein a ratio of the polyurethane resin to the dimethyl sulfoxide is 1:1.4˜1:1.9, and a viscosity of the solvent is 500˜600 poise.

### Claim 15 (depends on 13)

The process, as recited in claim 13, further comprising: keeping a temperature of the solvent above 20° C.

### Claim 16 (depends on 14)

The process, as recited in claim 14, further comprising: keeping a temperature of the solvent above 20° C.

### Claim 17

A solvent for coating on a knitted glove, comprising a polyurethane resin and a component selected from the group consisting of N-methyl pyrrolidone, dimethylacetamide, and dimethyl sulfoxide, wherein the component participates in synthesizing the polyurethane resin.

### Claim 18 (depends on 17)

The solvent, as recited in claim 17, wherein the component is the N-methyl pyrrolidone, wherein a ratio of the polyurethane resin to the N-methyl pyrrolidone is 1:1.3˜1:1.8, and a viscosity of the solvent is 500˜600 poise.

### Claim 19 (depends on 17)

The solvent, as recited in claim 17, wherein the component is the dimethylacetamide, wherein a ratio of the polyurethane resin to the dimethylacetamide is 1:1.3˜1:1.9, and a viscosity of the solvent is 500˜600 poise.

### Claim 20 (depends on 17)

The solvent, as recited in claim 17, wherein the component is the dimethyl sulfoxide, wherein a ratio of the polyurethane resin to the dimethyl sulfoxide is 1:1.4˜1:1.9, and a viscosity of the solvent is 500˜600 poise.