# US 2010/0247025 A1 · Optical element

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2010/0247025 A1
- Document ID: US20100247025A1
- Status: Published application
- Kind: A1
- Application number: 12/733,875
- Filed: 2008-09-26
- Published: 2010-09-30
- Earliest claimed: 2007-09-28
- Assignees: Sumitomo Osaka Cement Co., Ltd.
- Inventors: Katsutoshi Kondou; Susumu Murata; Junichiro Ichikawa
- Web page: https://patentgrep.com/patent/US20100247025A1

## CPC

- G02B 6/125: Bends, branchings or intersections
- G02F 1/21: by interference
- G02F 1/212: {Mach-Zehnder type}
- G02F 2202/20: LiNbO3, LiTaO3
- G02F 2202/28: Adhesive materials or arrangements
- G02F 2203/20: Intrinsic phase difference, i.e. optical bias, of an optical modulator; Methods for the pre-set thereof
- G02F 2203/50: Phase-only modulation
- G02F 2203/60: Temperature independent
- G02F 2203/69: Arrangements or methods for testing or calibrating a device
- G02B: OPTICAL ELEMENTS, SYSTEMS OR APPARATUS
- G02F: OPTICAL DEVICES OR ARRANGEMENTS FOR THE CONTROL OF LIGHT BY MODIFICATION OF THE OPTICAL PROPERTIES OF THE MEDIA OF THE ELEMENTS INVOLVED THEREIN; NON-LINEAR OPTICS; FREQUENCY-CHANGING OF LIGHT; OPTICAL LOGIC ELEMENTS; OPTICAL ANALOGUE/DIGITAL CONVERTERS

## Abstract

Disclosed is an optical element which includes a support substrate and a thin plate of single crystal stacked on the support substrate through a thermoplastic adhesive, having the advantages of easily regulating the phase of light waves and restoring the regulated state to the original state. The optical element includes a support substrate 4 and a thin plate 1 of single crystal stacked on the support substrate 4 through a thermoplastic adhesive 3. The optical characteristics of the optical element are regulated by applying stress within an elastic limit to at least a part of the thin plate in a state where the thermoplastic adhesive is softened by heating the optical element, forming a concavo-convex part 10 in the thin plate, and then cooling the optical element to fix the concavo-convex part.

## Claims

### Claim 1

An optical element comprising:
a support substrate; and
a thin plate of single crystal stacked on the support substrate through a thermoplastic adhesive,
wherein the optical characteristics of the optical element are regulated by applying stress within an elastic limit to at least a part of the thin plate in a state where the thermoplastic adhesive is softened by heating the optical element, forming a concavo-convex part in the thin plate, and then cooling the optical element to fix the concavo-convex part.

### Claim 2 (depends on 1)

The optical element according to claim 1, further comprising:
fixing means for maintaining the shape of the concavo-convex part formed in the thin plate of single crystal,
wherein the fixing means is formed of a material having thermoplasticity lower than that of the thermoplastic adhesive or a material having no thermoplasticity.

### Claim 3 (depends on 2)

The optical element according to claim 2,
wherein the fixing means is provided in contact with the concavo-convex part or above the concavo-convex part.

### Claim 4 (depends on 1)

The optical element according to claim 1,
wherein an optical waveguide is formed in the thin plate of single crystal.

### Claim 5 (depends on 4)

The optical element according to claim 4,
wherein the concavo-convex part is formed above or near the optical waveguide to regulate the optical characteristics.

### Claim 6 (depends on 5)

The optical element according to claim 5,
wherein the optical waveguide is a Mach-Zehnder type optical waveguide.

### Claim 7 (depends on 6)

The optical element according to claim 6,
wherein the concavo-convex part is arranged near or above two branch waveguides constituting the Mach-Zehnder type optical waveguide so as to regulate the phase of light propagating through the branch waveguides.

### Claim 8

An optical element comprising:
a support substrate; and
a thin plate of single crystal stacked on the support substrate through a thermoplastic adhesive,
wherein the thin plate has a thickness equal to or smaller than 50 μm,
stress within an elastic limit is applied to at least a part of the thin plate,
a circular concavo-convex part having a radius r and a depth d is formed, and
the shape of the concavo-convex part satisfies the condition of the following expression:
tan [2d/(d2+r2)×(r+π/kn)]≦2rd/(r2−d2)
wherein k is a wave number under vacuum, and n is a refractive index.

### Claim 9 (depends on 2)

The optical element according to claim 2,
wherein an optical waveguide is formed in the thin plate of single crystal.

### Claim 10 (depends on 3)

The optical element according to claim 3,
wherein an optical waveguide is formed in the thin plate of single crystal.