# US 2010/0245730 A1 · Cellulose acylate film and method for producing same, retardation film, polarizer and image display device

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2010/0245730 A1
- Document ID: US20100245730A1
- Status: Published application
- Kind: A1
- Application number: 12/750,801
- Filed: 2010-03-31
- Published: 2010-09-30
- Earliest claimed: 2009-03-31
- Assignees: FUJIFILM Corporation
- Inventors: Shigeaki NIMURA; Kousuke YAMAKI; Akihiro MATSUFUJI; Yoji ITO
- Web page: https://patentgrep.com/patent/US20100245730A1

## CPC

- C08J 5/18: Manufacture of films or sheets
- B29C 55/14: successively
- C08L 1/10: Esters of organic acids {, i.e. acylates}
- C08L 1/12: Cellulose acetate
- C08L 1/14: Mixed esters, e.g. cellulose acetate-butyrate
- G02B 5/3033: {in the form of a thin sheet or foil, e.g. Polaroid}
- B29C 41/24: for making articles of indefinite length
- B29K 2001/00: Use of cellulose, modified cellulose or cellulose derivatives, e.g. viscose, as moulding material
- B29K 2001/12: {Cellulose acetate}
- B29K 2995/0034: Polarising
- C08J 2301/12: Cellulose acetate
- C09K 2323/00: Functional layers of liquid crystal optical display excluding electroactive liquid crystal layer characterised by chemical composition
- G02F 1/13363: Birefringent elements, e.g. for optical compensation
- C08J: WORKING-UP; GENERAL PROCESSES OF COMPOUNDING; AFTER-TREATMENT NOT COVERED BY SUBCLASSES C08B, C08C, C08F, C08G or C08H (working, e.g. shaping, of plastics B29)
- B29C: SHAPING OR JOINING OF PLASTICS; SHAPING OF MATERIAL IN A PLASTIC STATE, NOT OTHERWISE PROVIDED FOR; AFTER-TREATMENT OF THE SHAPED PRODUCTS, e.g. REPAIRING (making preforms B29B11/00; making laminated products by combining previously unconnected layers which become one product whose layers will remain together B32B37/00 - B32B41/00)
- C08L: COMPOSITIONS OF MACROMOLECULAR COMPOUNDS (compositions based on polymerisable monomers C08F, C08G; artificial filaments or fibres D01F; textile treating compositions D06)
- G02B: OPTICAL ELEMENTS, SYSTEMS OR APPARATUS
- B29K: INDEXING SCHEME ASSOCIATED WITH SUBCLASSES B29B, B29C OR B29D, RELATING TO MOULDING MATERIALS OR TO MATERIALS FOR {MOULDS, } REINFORCEMENTS, FILLERS OR PREFORMED PARTS, e.g. INSERTS
- C09K: MATERIALS FOR MISCELLANEOUS APPLICATIONS, NOT PROVIDED FOR ELSEWHERE
- G02F: OPTICAL DEVICES OR ARRANGEMENTS FOR THE CONTROL OF LIGHT BY MODIFICATION OF THE OPTICAL PROPERTIES OF THE MEDIA OF THE ELEMENTS INVOLVED THEREIN; NON-LINEAR OPTICS; FREQUENCY-CHANGING OF LIGHT; OPTICAL LOGIC ELEMENTS; OPTICAL ANALOGUE/DIGITAL CONVERTERS

## Abstract

A method for producing a cellulose acylate film, comprising casting a polymer solution that comprises a plasticizer having a number-average molecular weight of 200-10000 and a cellulose acylate to form a web; stretching the web having a residual solvent amount of 100-300% by mass in one direction at from −30° C. to 30° C.; drying the stretched web to reduce the residual solvent amount from 6-120% by mass to less than 12% by mass while controlling the surface temperature of the web so as not to reach 200° C. or higher; and stretching the resulting film at 60-200° C. in a direction different form the stretching direction of the first stretching.

## Claims

### Claim 1

A method for producing a cellulose acylate film, comprising in the following order:
casting a polymer solution that comprises a plasticizer having a number-average molecular weight of from 200 to 10000 and a cellulose acylate to form a web,
stretching the web having a residual solvent amount of from 100 to 300% by mass in one direction at from −30° C. to 30° C., drying the stretched web to reduce the residual solvent amount from 6 to 120% by mass to less than 12% by mass while controlling the surface temperature of the web so as not to reach 200° C. or higher, and
stretching the resulting film at from 60° C. to 200° C. in a direction different form the stretching direction of the first stretching.

### Claim 2 (depends on 1)

The method for producing a cellulose acylate film according to claim 1, wherein the residual solvent amount is reduced by the drying from 8 to 100% by mass to from 2 to 10% by mass.

### Claim 3 (depends on 1)

The method for producing a cellulose acylate film according to claim 1, wherein the web is stretched in the machine direction of the first stretching.

### Claim 4 (depends on 1)

The method for producing a cellulose acylate film according to claim 1, wherein the surface temperature of the web is controlled to be in the range of from 50 to 120° C. during the drying.

### Claim 5 (depends on 1)

The method for producing a cellulose acylate film according to claim 1, wherein the degree of acyl substitution of the cellulose acylate film is from 2.7 to 3.0.

### Claim 6 (depends on 1)

The method for producing a cellulose acylate film according to claim 1, wherein the acyl group in the cellulose acylate is an acetyl group.

### Claim 7 (depends on 1)

The method for producing a cellulose acylate film according to claim 1, wherein the polymer solution comprises a plasticizer having a negative intrinsic birefringence.

### Claim 8 (depends on 7)

The method for producing a cellulose acylate film according to claim 7, wherein the plasticizer having a negative intrinsic birefringence has a weight-average molecular weight of from 1000 to 10000.

### Claim 9 (depends on 1)

The method for producing a cellulose acylate film according to claim 1, wherein the polymer solution comprises a plasticizer having a number-average molecular weight of from 500 to 10000 and having a recurring unit.

### Claim 10 (depends on 1)

The method for producing a cellulose acylate film accordig to claim 1, wherein the polymer solution comprises a polyester-type plasticizer.

### Claim 11 (depends on 1)

The method for producing a cellulose acylate film according to claim 1, wherein the polymer solution comprises the plasticizer in an amount of from 2 to 30% by mass of the cellulose acylate therein.

### Claim 12

A cellulose acylate film produced by:
casting a polymer solution that comprises a plasticizer having a number-average molecular weight of from 200 to 10000 and a cellulose acylate to form a web,
stretching the web having a residual solvent amount of from 100 to 300% by mass in one direction at from −30° C. to 30° C.,
drying the stretched web to reduce the residual solvent amount from 6 to 120% by mass to less than 12% by mass while controlling the surface temperature of the web so as not to reach 200° C. or higher, and
stretching the resulting film at from 60° C. to 200° C. in a direction different form the stretching direction of the first stretching.

### Claim 13 (depends on 12)

The cellulose acylate film according to claim 12, of which the heat of crystallization ΔHc is from 0 to 1.0 J/g.

### Claim 14 (depends on 12)

The cellulose acylate film according to claim 12, of which the in-plane retardation (Re) is from 60 nm to 300 nm.

### Claim 15 (depends on 12)

The cellulose acylate film of according to claim 12, of which the direction of the slow axis is perpendicular to the machine direction in the stretching.

### Claim 16 (depends on 12)

The cellulose acylate film according to claim 12, of which the thickness-direction retardation (Rth) is from −10 nm to 80 nm.

### Claim 17

A retardation film comprising a laminate of an optically anisotropic layer of a liquid crystal composition and a cellulose acylate film, wherein the cellulose acylate film is produced by:
casting a polymer solution that comprises a plasticizer having a number-average molecular weight of from 200 to 10000 and a cellulose acylate to form a web,
stretching the web having a residual solvent amount of from 100 to 300% by mass in one direction at from −30° C. to 30° C.,
drying the stretched web to reduce the residual solvent amount from 6 to 120% by mass to less than 12% by mass while controlling the surface temperature of the web so as not to reach 200° C. or higher, and
stretching the resulting film at from 60° C. to 200° C. in a direction different form the stretching direction of the first stretching.

### Claim 18

A polarizer comprising a cellulose acylate film produced by:
casting a polymer solution that comprises a plasticizer having a number-average molecular weight of from 200 to 10000 and a cellulose acylate to form a web,
stretching the web having a residual solvent amount of from 100 to 300% by mass in one direction at from −30° C. to 30° C.,
drying the stretched web to reduce the residual solvent amount from 6 to 120% by mass to less than 12% by mass while controlling the surface temperature of the web so as not to reach 200° C. or higher, and
stretching the resulting film at from 60° C. to 200° C. in a direction different form the stretching direction of the first stretching.

### Claim 19

An image display device comprising a polarizer, wherein the polarizer comprises a cellulose acylate film produced by:
casting a polymer solution that comprises a plasticizer having a number-average molecular weight of from 200 to 10000 and a cellulose acylate to form a web,
stretching the web having a residual solvent amount of from 100 to 300% by mass in one direction at from −30° C. to 30° C.,
drying the stretched web to reduce the residual solvent amount from 6 to 120% by mass to less than 12% by mass while controlling the surface temperature of the web so as not to reach 200° C. or higher, and
stretching the resulting film at from 60° C. to 200° C. in a direction different form the stretching direction of the first stretching.

### Claim 20 (depends on 19)

The image display device according to claim 19 having a liquid crystal cell, of which the display mode is in-plane switching or twisted nematic mode.