# US 2010/0245715 A1 · Method of making antiglare film, antiglare film, polarizing plate, image display device, and transmissive/semi-transmissive liquid crystal display

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2010/0245715 A1
- Document ID: US20100245715A1
- Status: Published application
- Kind: A1
- Application number: 12/749,916
- Filed: 2010-03-30
- Published: 2010-09-30
- Earliest claimed: 2009-03-30
- Assignees: FUJIFILM Corporation
- Inventors: Jun WATANABE; Hiroyuki YONEYAMA; Takato SUZUKI
- Web page: https://patentgrep.com/patent/US20100245715A1

## CPC

- G02B 5/02: Diffusing elements; Afocal elements
- G02F 1/133502: {Antiglare, refractive index matching layers}
- G02B: OPTICAL ELEMENTS, SYSTEMS OR APPARATUS
- G02F: OPTICAL DEVICES OR ARRANGEMENTS FOR THE CONTROL OF LIGHT BY MODIFICATION OF THE OPTICAL PROPERTIES OF THE MEDIA OF THE ELEMENTS INVOLVED THEREIN; NON-LINEAR OPTICS; FREQUENCY-CHANGING OF LIGHT; OPTICAL LOGIC ELEMENTS; OPTICAL ANALOGUE/DIGITAL CONVERTERS

## Abstract

In a method for making an antiglare film including the casting, the releasing, the drying, the applying and the curing as defined herein, the transparent particles have an average primary particle size of greater than 2.5 μm and not greater than 12 μm, the transparent base has on at least one side thereof flat portions substantially parallel to a film-forming plane and rounded protrusions arising from the transparent particles, the protrusions having a maximum height Rt from the flat portions of from 1 to 15 μm, and the cured layer has an average thickness of from 1 to 15.0 μm and a surface profile with an arithmetic average roughness Ra, a mean spacing between peaks Sm, and an average slope θa, all as measured in accordance with JIS B0601, satisfying the relationships (1) to (3) as defined herein.

## Claims

### Claim 1

A method for making an antiglare film comprising:
(1) casting a dope containing at least a thermoplastic resin and transparent particles on a support, releasing the cast film from the support and drying the cast film, to make a transparent base;
(2) applying a coating solution containing at least a curing compound, a polymerization initiator and a solvent on the transparent base and removing the solvent by drying; and
(3) curing the curing compound to form a cured layer, wherein:
the transparent particles have an average primary particle size of greater than 2.5 μm and not greater than 12 μm,
the transparent base has on at least one side thereof flat portions substantially parallel to a film-forming plane and rounded protrusions arising from the transparent particles, the protrusions having a maximum height Rt from the flat portions of from 1 to 15 μm, and
the cured layer has an average thickness of from 1 to 15.0 μm and a surface profile with an arithmetic average roughness Ra, a mean spacing between peaks Sm, and an average slope θa, all as measured in accordance with JIS B0601, satisfying relationships (1) to (3):
0.01 μm≦Ra≦0.2 μm (1)
10 μm≦Sm≦300 μm (2)
0.3°≦θa≦1.5° (3)

### Claim 2

A method for making an antiglare film comprising:
(1) casting a dope containing at least a thermoplastic resin and transparent particles on a support, releasing the cast film from the support and drying the cast film, to make a transparent base;
(2) applying a coating solution containing at least a curing compound, a polymerization initiator and a solvent on the transparent base and removing the solvent by drying; and
(3) curing the curing compound to form a cured layer, wherein:
the transparent particles have an average primary particle size of greater than 2.5 μm and not greater than 12 μm,
the transparent base has on at least one side thereof flat portions substantially parallel to a film-forming plane and rounded protrusions arising from the transparent particles, the protrusions having a maximum height Rt from the flat portions of from 1 to 15 μm, and
the cured layer has an average thickness of 1 to 15.0 μm and a surface profile with a slope distribution satisfying conditions (a) to (c):
(a) The integral value of the frequency of slopes from 0° to less than 0.3° is 0% to 25%.
(b) The integral value of the frequency of slopes from 0.3° to less than 5.0° is 65% to less than 100%.
(c) The integral value of the frequency of slopes of 5.0° or more is 0% to 10%.

### Claim 3 (depends on 1)

The method according to claim 1, wherein the casting of a dope is casting at least two dopes simultaneously or successively, and the transparent particles are present in the dope adapted to form a layer adjacent to the cured layer.

### Claim 4 (depends on 1)

The method according to claim 1, which does not comprise winding after the casting of a dope until the production of the antiglare film.

### Claim 5

An antiglare film comprising a transparent base containing a thermosetting resin and transparent particles with an average primary particle size of greater than 2.5 μm and not greater than 12 μm and a cured layer with an average thickness of 1 to 15.0 μm on the transparent base,
the transparent base having, on its side having the cured layer, flat portions substantially parallel to a film-forming plane and rounded protrusions arising from the transparent particles, the protrusions having a maximum height Rt from the flat portions of from 1 to 15 μm.

### Claim 6 (depends on 5)

The antiglare film according to claim 5, wherein the surface of the cured layer and the surface of the transparent base on its side having the cured layer have an arithmetic average roughness difference ΔRa of 0.1 to 1.0 μm, the arithmetic average roughness being determined in accordance with JIS B0601.

### Claim 7 (depends on 5)

The antiglare film according to claim 5, wherein the cured layer has a ratio of its minimum thickness tmin to its maximum thickness tmax (tmin/tmax) of 0.01 to less than 0.8.

### Claim 8 (depends on 5)

The antiglare film according to claim 5, wherein the transparent particles are nearly spherical resin particles.

### Claim 9 (depends on 5, 6, 7, 8)

The antiglare film according to any one of claims 5 to 8, wherein the transparent base and the transparent particles have an absolute difference in refractive index of less than 0.09.

### Claim 10 (depends on 5)

The antiglare film according to claim 5, which has light scattering properties such that the antiglare film provides an image clarity of 20% to 75% as measured using an image clarity meter at an optical comb width of 0.5 mm in accordance with JIS K7105.

### Claim 11 (depends on 5)

The antiglare film according to claim 5, which has an internal haze of 0.1% to 30% and a surface haze of 0.5% to 5.0%.

### Claim 12 (depends on 5)

A polarizing plate comprising a polarizing film and a protective film on at least one side of the polarizing film, wherein the protective film is the antiglare film according to claim 5.

### Claim 13 (depends on 5)

An image display device comprising the antiglare film according to claim 5.

### Claim 14 (depends on 12)

A transmissive or semi-transmissive liquid crystal display comprising a liquid crystal cell and a polarizing plate, wherein the polarizing plate is the polarizing plate according to claim 12 and is disposed on a front side of the liquid crystal cell.

### Claim 15 (depends on 12)

A transmissive or semi-transmissive liquid crystal display comprising a liquid crystal cell and a polarizing plate, wherein the polarizing plate is the polarizing plate according to claim 12 and is disposed on a backlight side of the liquid crystal cell.

### Claim 16 (depends on 12)

A transmissive or semi-transmissive liquid crystal display comprising a liquid crystal cell and a polarizing plate, wherein the polarizing plate is the polarizing plate according to claim 12 and is disposed on each of a front side and a backlight side of the liquid crystal cell.