# US 2010/0168489 A1 · Bound phosphorus-modified zeolite catalyst, method of preparing and method of using thereof

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2010/0168489 A1
- Document ID: US20100168489A1
- Status: Published application
- Kind: A1
- Application number: 12/657,152
- Filed: 2010-01-14
- Published: 2010-07-01
- Earliest claimed: 2005-12-22
- Assignees: Saudi Basic Industries Corporation
- Inventors: Ashim Kumar Ghosh; Pamela Harvey; Neeta Kulkami
- Web page: https://patentgrep.com/patent/US20100168489A1

## CPC

- B01J 29/40: of the pentasil type, e.g. types ZSM-5, ZSM-8 or ZSM-11, as exemplified by patent documents US3702886, GB1334243 and US3709979, respectively
- B01J 37/28: Phosphorising
- C07C 2/66: Catalytic processes
- B01J 2229/37: Acid treatment
- B01J 2229/42: Addition of matrix or binder particles
- C07C 2529/40: of the pentasil type, e.g. types ZSM-5, ZSM-8 or ZSM-11
- B01J: CHEMICAL OR PHYSICAL PROCESSES, e.g. CATALYSIS OR COLLOID CHEMISTRY; THEIR RELEVANT APPARATUS
- C07C: ACYCLIC OR CARBOCYCLIC COMPOUNDS

## Abstract

Disclosed is a bound phosphorus-modified zeolite catalyst. Zeolite is treated with a phosphorus compound to form the phosphorus-treated zeolite. Binder material is treated with a mineral acid prior to being bound with the phosphorus-modified zeolite. The binder material includes inorganic oxide materials, such as alumina, clay, aluminum phosphate and silica-alumina, in particular, a binder of alumina or clay or their combinations. The mineral acid includes hydrochloric acid, nitric acid, phosphoric acid or sulfuric acid. The phosphorus-treated zeolite is combined with the acid-treated inorganic oxide binder material to form a zeolite-binder mixture. Water is added to form an extrudable paste which maybe shaped and is heated to a temperature of about 400° C. or higher to form a bound phosphorus-modified zeolite catalyst. For aromatic alkylation, the bound phosphorus-modified zeolite catalyst is contacted with an aromatic alkylation feed of an aromatic compound and an alkylating agent under reaction conditions suitable for aromatic alkylation.

## Claims

### Claim at position 1

1-43. (canceled)

### Claim 44

A method of preparing an alkyl aromatic product comprising:
a) treating a zeolite containing 10-oxygen ring pores with a phosphorus compound to form a phosphorus-treated zeolite;
b) treating an inorganic oxide binder material with a mineral acid;
c) combining the phosphorus-treated zeolite with an inorganic oxide binder material to form a zeolite-binder mixture;
d) heating the zeolite-binder mixture at temperature of about 400° C. or higher to form a bound zeolite catalyst; and
e) contacting the bound zeolite catalyst with an aromatic alkylation feed of an aromatic compound and an alkylating agent under reaction conditions suitable for aromatic alkylation.

### Claim 45 (depends on 44)

The method of claim 44 wherein the binder material includes at least one of alumina, clay, aluminum phosphate and silica-alumina.

### Claim 46 (depends on 44)

The method of claim 44 wherein the binder material is an alumina-containing material.

### Claim 47 (depends on 44)

The method of claim 44 wherein the binder material is present in an amount of from about 1% to about 99% by weight of the bound zeolite catalyst.

### Claim 48 (depends on 44)

The method of claim 44 wherein the binder material contains from about 1% to 99% by weight alumina or clay or their combinations.

### Claim 49 (depends on 44)

The method of claim 44 wherein the zeolite is a ZSM-5 zeolite.

### Claim 50 (depends on 44)

The method of claim 44 wherein the phosphorus-treated zeolite is heated to a temperature of about 300° C. or higher.

### Claim 51 (depends on 44)

The method of claim 44 wherein the zeolite-binder mixture is heated to a temperature of from 400° C. to about 700° C.

### Claim 52 (depends on 44)

The method of claim 44 further comprising adding water to the zeolite-binder mixture and shaping the zeolite-binder mixture

### Claim 53 (depends on 44)

The method of claim 44 wherein the aromatic compound is toluene.

### Claim 54 (depends on 44)

The method of claim 44 wherein the aromatic compound is toluene and the alkylating agent is methanol.

### Claim 55 (depends on 44)

The method of claim 44 further comprising steaming the bound zeolite at a temperature of 300° C. or less prior to contacting with the aromatic alkylation feed.

### Claim 56 (depends on 44)

The method of claim 44 wherein the zeolite is treated with a phosphorus compound to form a phosphorus-treated zeolite having a phosphorus content of from 0.01 to about 0.15 gram of phosphorus per gram of zeolite.

### Claim 57 (depends on 56)

The method of claim 56 wherein the zeolite is a ZSM-5 zeolite.

### Claim 58 (depends on 57)

The method of claim 57 wherein the binder material includes at least one of alumina, clay, aluminum phosphate and silica-alumina.

### Claim 59 (depends on 57)

The method of claim 57 wherein the binder material is an alumina-containing material.

### Claim 60 (depends on 57)

The method of claim 57 wherein the binder material is present in an amount of from about 1% to about 99% by weight of the bound ZSM-5 zeolite catalyst.

### Claim 61 (depends on 57)

The method of claim 57 wherein the binder material contains from about 1% to 99% by weight alumina.

### Claim 62 (depends on 57)

The method of claim 57 wherein the phosphorus-treated ZSM-5 zeolite is heated to a temperature of about 300° C. or higher.

### Claim 63 (depends on 56)

The method of claim 56 wherein the zeolite-binder mixture is heated to a temperature of from 400° C. to about 700° C.

### Claim 64 (depends on 54)

The method of claim 54 further comprising steaming the bound ZSM-5 zeolite at a temperature of 300° C. or less prior to contacting with the feed of toluene.

### Claim 65 (depends on 44)

The method of claim 44 wherein the mineral acid is hydrochloric acid, nitric acid, phosphoric acid or sulfuric acid

### Claim 66 (depends on 65)

The method of claim 65 wherein the mineral acid is nitric acid.