# US 2010/0168409 A1 · Thermoplastic resin film and method for producing same

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2010/0168409 A1
- Document ID: US20100168409A1
- Status: Published application
- Kind: A1
- Application number: 12/160,855
- Filed: 2007-01-11
- Published: 2010-07-01
- Earliest claimed: 2006-01-13
- Inventors: Akihide Fujita
- Web page: https://patentgrep.com/patent/US20100168409A1

## CPC

- B29C 43/222: {characterised by the shape of the surface}
- B29C 48/04: Particle-shaped (making granules B29B9/00)
- B29C 48/21: the layers being joined at their surfaces
- B29C 48/395: using screws surrounded by a cooperating barrel, e.g. single screw extruders
- B29C 48/40: using two or more parallel screws {or at least two parallel non-intermeshing screws}, e.g. twin screw extruders
- B29C 48/495: Feedblocks (extrusion moulding of multi-component articles B29C48/16)
- B29C 48/53: having a varying channel depth, e.g. varying the diameter of the longitudinal screw trunk
- B29C 48/625: characterised by the ratio of the threaded length of the screw to its outside diameter [L/D ratio]
- B29C 48/914: {Cooling drums}
- B29C 48/919: {using a bath, e.g. extruding into an open bath to coagulate or cool the material}
- B29C 48/92: Measuring, controlling or regulating
- B29C 55/143: {firstly parallel to the direction of feed and then transversely thereto}
- B29C 43/00: Compression moulding, i.e. applying external pressure to flow the moulding material; Apparatus therefor {(by liberation of internal stresses B29C61/006)}
- B29C 48/0018: {combined with shaping by orienting, stretching or shrinking, e.g. film blowing (B29C48/0017 takes precedence)}
- B29C 48/08: flexible, e.g. films
- B29C 48/307: {specially adapted for bringing together components, e.g. melts within the die}
- B29C 48/906: {using roller calibration}
- B29C 2948/922: Viscosity; Melt flow index [MFI]; Molecular weight
- B29C 2948/924: Barrel or housing
- B29C 2948/92514: Pressure
- B29C 2948/92523: Force; Tension
- B29C 2948/9259: Angular velocity
- B29C 2948/92647: Thickness
- B29C 2948/92704: Temperature
- B29C 2948/92895: Barrel or housing
- B29C 2948/92904: Die; Nozzle zone
- B29C 2948/92923: Calibration, after-treatment or cooling zone
- B29C 2948/92933: Conveying, transporting or storage of articles
- B29K 2001/00: Use of cellulose, modified cellulose or cellulose derivatives, e.g. viscose, as moulding material
- B29K 2001/12: {Cellulose acetate}
- B29K 2995/0031: Refractive
- B29K 2995/0053: bi-axially
- B29L 2007/008: {Wide strips, e.g. films, webs}
- B29L 2009/00: Layered products
- B29L 2031/3475: {Displays, monitors, TV-sets, computer screens}
- G02B 5/3083: {Birefringent or phase retarding elements (G02B5/3008, G02B5/3016 take precedence; systems for polarisation control G02B27/286; manufacturing phase modulating patterns by lithographic processes G03F7/001)}
- B29C: SHAPING OR JOINING OF PLASTICS; SHAPING OF MATERIAL IN A PLASTIC STATE, NOT OTHERWISE PROVIDED FOR; AFTER-TREATMENT OF THE SHAPED PRODUCTS, e.g. REPAIRING (making preforms B29B11/00; making laminated products by combining previously unconnected layers which become one product whose layers will remain together B32B37/00 - B32B41/00)
- B29K: INDEXING SCHEME ASSOCIATED WITH SUBCLASSES B29B, B29C OR B29D, RELATING TO MOULDING MATERIALS OR TO MATERIALS FOR {MOULDS, } REINFORCEMENTS, FILLERS OR PREFORMED PARTS, e.g. INSERTS
- B29L: INDEXING SCHEME ASSOCIATED WITH SUBCLASS B29C, RELATING TO PARTICULAR ARTICLES
- G02B: OPTICAL ELEMENTS, SYSTEMS OR APPARATUS

## Abstract

To provide a thermoplastic resin film, and process for producing the same, which can obtain a film having high optical properties in which the occurrence of residual strain and the exhibition of retardation during film forming are suppressed. A film (12) is produced by extruding melted thermoplastic resins in sheet form through a die (24), and sandwiching the sheet between a pair of rollers (26), (28) configured so that at least one of the rollers is an elastic roller (26) made from metal, to cool and solidify the sheet into the film, the thickness Z of a metal tube (44) constituting an outer shell of the elastic roller (26) being in a range of 0.05 mm<z<7.0 mm, wherein the sheet is formed as a laminate sheet having two or more layers by using two or more of the thermoplastic resins A, B, and in the laminate sheet a glass transition temperature Tg (° C.) of the thermoplastic resin B forming an inner layer is 3 to 50° C. less than the glass transition temperature Tg (° C.) of the thermoplastic resin A forming an outer layer.

## Claims

### Claim 1

A method for producing a thermoplastic resin film including the steps of:
forming a film by extruding melted thermoplastic resins in sheet form through a die; and
cooling and solidifying the sheet into the film by sandwiching the sheet between a pair of rollers configured so that at least one of the rollers is an elastic roller made from metal, the thickness Z of a metal tube constituting an outer shell of the elastic roller being in a range of 0.05 mm<z<7.0 mm, wherein
the sheet is formed as a laminate sheet having two or more layers by using two or more of the thermoplastic resins, and in the laminate sheet a glass transition temperature Tg (° C.) of the thermoplastic resin forming an inner layer is 3 to 50° C. less than the glass transition temperature Tg (° C.) of the thermoplastic resin forming an outer layer.

### Claim 2 (depends on 1)

The method for producing a thermoplastic resin film according to claim 1, wherein
the pair of rollers satisfies both the following equations (1) and (2):
when the glass transition temperature Tg (° C.) of the thermoplastic resin forming the outer layer minus the temperature (° C.) of the elastic roller is represented as “X” (° C.), and the line speed is represented as “Y” (m/min),
0.0043X2+1.2X+1.1<Y<0.019X2+0.73X+24 (1)
and when the length along which the pair of rollers are in contact with each other via the laminate sheet is represented as “Q” (cm), and the linear pressure sandwiching the laminate sheet by the pair of rollers is represented as “P” (kg/cm).
3 kg/cm2<P/Q<50 kg/cm2 (2).

### Claim 3 (depends on 1)

The method for producing a thermoplastic resin film according to claim 1, wherein
at least one roller of the pair of rollers has a surface having an arithmetic average roughness Ra of no greater than 100 nm.

### Claim 4 (depends on 1)

The method for producing a thermoplastic resin film according to claim 1, wherein
the laminate sheet is formed by co-extrusion.

### Claim 5 (depends on 1)

The method for producing a thermoplastic resin film according to claim 1, wherein
the laminate sheet has an A/B/A tri-layer structure consisting of a thermoplastic resin A forming the outer layers and a thermoplastic resin B forming the inner layer, and a glass transition temperature Tg (° C.) of the thermoplastic resin B is 3 to 50° C. less than a glass transition temperature Tg (° C.) of the thermoplastic resin A.

### Claim 6 (depends on 1)

The method for producing a thermoplastic resin film according to claim 1, wherein
the laminate sheet has an A/B/C/B/A five-layer structure consisting of a thermoplastic resin layer A forming the outer layers and thermoplastic resins B and C forming the inner layers, and glass transition temperatures Tg (° C.) of the thermoplastic resins B and C are 3 to 50° C. less than a glass transition temperature Tg (° C.) of the thermoplastic resin A.

### Claim 7 (depends on 1)

The method for producing a thermoplastic resin film according to claim 1, wherein
the laminate sheet has an A/B bi-layer structure consisting of a thermoplastic resin A forming the outer layer and a thermoplastic resin B forming the inner layer, and when one of the pair of rollers is an elastic resin, the thermoplastic resin A in contact with the elastic roller serves as the outer layer.

### Claim 8 (depends on 1)

The method for producing a thermoplastic resin film according to claim 1, wherein
the thermoplastic resins, when discharged through the die, have a zero shear viscosity no greater than 2,000 Pa·sec.

### Claim 9 (depends on 1)

The method for producing a thermoplastic resin film according to claim 1, wherein
the thickness of the thermoplastic resin forming the outer layer is in a range of 10 to 90% of the film total thickness.

### Claim 10 (depends on 1)

The method for producing a thermoplastic resin film according to claim 1, wherein
the width of the thermoplastic resin forming the outer layer is 99% or more of the film total width.

### Claim 11 (depends on 1)

The method for producing a thermoplastic resin film according to claim 1, wherein
the film has a thickness of 20 to 300 μm, an in-plane retardation Re no greater than 20 nm and a thickness direction retardation Rth no greater than 20 nm.

### Claim 12 (depends on 1)

The method for producing a thermoplastic resin film according to claim 1, wherein
the thermoplastic resin is a cellulose acylate resin.

### Claim 13 (depends on 12)

The method for producing a thermoplastic resin film according to claim 12, wherein
the cellulose acylate resin has an average molecular weight of 20,000 to 80,000, and when “A” represents the degree of substitution of an acyl group and “B” represents the sum of the degree of substitution of an acyl group having 3 to 7 carbon atoms, satisfies 2.05≦A+B≦3.0, 0≦A≦2.0 and 1.2≦B<2.9.

### Claim 14 (depends on 1)

A thermoplastic resin film produced by the production process according to claim 1.

### Claim 15 (depends on 14)

An optical compensatory film for a liquid crystal display plate comprising the thermoplastic resin film according to claim 14 as a substrate.

### Claim 16 (depends on 14)

A polarizing plate formed using at least one ply of the thermoplastic resin film according to claim 14 as a protective film of a polarizing film.