# US 2010/0168368 A1 · Epoxy Resin, Method for Producing Same and Epoxy Resin Composition Thereof

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2010/0168368 A1
- Document ID: US20100168368A1
- Status: Published application
- Kind: A1
- Application number: 12/491,548
- Filed: 2009-06-25
- Published: 2010-07-01
- Earliest claimed: 2004-06-17
- Assignees: Kukdo Chemical Co., Ltd. (Korean Corporation)
- Inventors: Masayoshi HANAFUSA; Shuya SHINOHARA
- Web page: https://patentgrep.com/patent/US20100168368A1

## CPC

- C08G 59/022: {characterised by the preparation process or apparatus used}
- C08G 59/063: {with epihalohydrins}
- C08G 2650/56: Polyhydroxyethers, e.g. phenoxy resins
- C08G: MACROMOLECULAR COMPOUNDS OBTAINED OTHERWISE THAN BY REACTIONS ONLY INVOLVING UNSATURATED CARBON-TO-CARBON BONDS

## Abstract

An epoxy resin represented by general formula (I), which satisfies numerical formula (1) mentioned below and comprises hydrolytic halogen of 0.05 wt. % or less, said epoxy resin being produced by the procedure as follows: after dissolving 0.8 to 1.3 mole of epihalohydrin to 1 mole of divalent phenol in a solvent, a pre-reaction is performed over 30 to 70 minutes by adding dropwise 0.25-0.35 mole of 30˜50% aqueous solution of alkali metal hydroxide over 30 to 70 minutes thereto, and thereafter, 0.65-0.75 mole of the remaining 30˜50% aqueous solution of alkali metal hydroxide is added dropwise over about 1 hour to complete the reaction over 1 to 3 hours. wherein n is an integer of 0 or more; A1 and A2 are residue of divalent phenol, and can be same or different; both R1 and R2 are H or wherein, X: epoxy equivalent (g/eq); Y: phenolic hydroxyl group equivalent (g/eq).

## Claims

### Claim 1

An epoxy resin represented by general formula (I), which satisfies numerical formula (1) below and comprises hydrolytic halogen of 0.05 wt. % or less, said epoxy resin being produced by the procedure as follows: after dissolving 0.8 to 1.3 mole of epihalohydrin to 1 mole of divalent phenol in a solvent, a pre-reaction is performed over 30 to 70 minutes by adding dropwise 0.25-0.35 mole of 30˜50% aqueous solution of alkali metal hydroxide over 30 to 70 minutes thereto, and thereafter, 0.65-0.75 mole of the remaining 30˜50% aqueous solution of alkali metal hydroxide is added dropwise over approximately 1 hour to complete the reaction over approximately 1 to 3 hours.
wherein n is an integer of 0 or more;
A1 and A2 are residue of divalent phenol, and can be same or different;
both R1 and R2 are H or
wherein,
X: epoxy equivalent (g/eq);
Y: phenolic hydroxyl group equivalent (g/eq).

### Claim 2 (depends on 1)

The epoxy resin of claim 1 wherein the divalent phenol is bisphenol.

### Claim 3 (depends on 1)

The epoxy resin of claim 1 wherein the epoxy equivalent of the resin is 3000 g/eq or less and the phenolic hydroxyl group equivalent of the resin is 5000 g/eq or less.

### Claim 4 (depends on 1)

An epoxy resin composition containing an epoxy resin according to claim 1 as an essential component.