# US 2010/0168364 A1 · Multi-branched polypropylene

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2010/0168364 A1
- Document ID: US20100168364A1
- Status: Published application
- Kind: A1
- Application number: 12/226,365
- Filed: 2007-04-16
- Published: 2010-07-01
- Earliest claimed: 2006-04-18
- Assignees: Borealis Technology Oy
- Inventors: Eberhard Ernst; Manfred Stadlbauer
- Web page: https://patentgrep.com/patent/US20100168364A1

## CPC

- C08F 10/06: Propene
- C08F 210/06: Propene
- C08F 210/16: Copolymers of ethene with alpha-alkenes, e.g. EP rubbers
- C08F 4/65912: {in combination with an organoaluminium compound}
- C08F 110/06: Propene
- Y10S 526/941: having the transition metal bonded directly to carbon
- Y10S 526/943: Polymerization with metallocene catalysts
- C08F: MACROMOLECULAR COMPOUNDS OBTAINED BY REACTIONS ONLY INVOLVING CARBON-TO-CARBON UNSATURATED BONDS
- Y10S: TECHNICAL SUBJECTS COVERED BY FORMER USPC CROSS-REFERENCE ART COLLECTIONS [XRACs] AND DIGESTS

## Abstract

Multi-branched polypropylene having a g′ of less than 1.00

## Claims

### Claim 1

Polypropylene having a multi-branching index (MBI) of at least 0.15, wherein the multi-branching index (MBI) is defined as the slope of strain hardening index (SHI) as function of the logarithm to the basis 10 of the Hencky strain rate/lg(dε/dt)), wherein
dε/dt is the deformation rate,
ε is the Hencky strain, and
the strain hardening index (SHI) is measured at 180° C., wherein the strain hardening index (SHI) is defined as the slope of the logarithm to the basis 10 of the tensile stress growth function (lg(ηE+)) as function of the logarithm to the basis 10 of the Hencky strain (lg(ε)) in the range of Hencky strains between 1 and 3.

### Claim 2 (depends on 1)

Polypropylene according to claim 1, wherein the polypropylene has a branching index g′ of less than 1.00.

### Claim 3 (depends on 1)

Polypropylene according to claim 1, wherein the polypropylene has a strain hardening index (SHI@1 s−1) of at least 0.30 measured by a deformation rate (dε/dt) of 1.00 s−1 at a temperature of 180° C.

### Claim 4 (depends on 1)

Polypropylene according to claim 1, wherein the polypropylene has melt flow rate MFR2 measured at 230° C. in the range 010.01 to 1000.00 g/10 min.

### Claim 5 (depends on 1)

Polypropylene according to claim 1, wherein the polypropylene has mmmm pentad concentration of higher than 90%.

### Claim 6 (depends on 1)

Polypropylene according to claim 1, wherein the polypropylene has a melting point Tm of at least 125° C.

### Claim 7 (depends on 1)

Polypropylene according to claim 1, wherein the polypropylene is multimodal.

### Claim 8 (depends on 1)

Polypropylene according to claim 1, wherein the polypropylene is a propylene homopolymer.

### Claim 9 (depends on 1)

Polypropylene according to claim 1, wherein the polypropylene is propylene copolymer.

### Claim 10 (depends on 9)

Propylene according to claim 9, wherein the comonomer is ethylene.

### Claim 11 (depends on 9)

Polypropylene according to claim 9, wherein the total amount of comonomer in the propylene copolymer is up to 30 wt %.

### Claim 12 (depends on 9)

Polypropylene according to claim 9, wherein the propylene copolymer comprises a polypropylene matrix and an ethylene-propylene rubber (EPR).

### Claim 13 (depends on 1)

Polypropylene according to claim 1, wherein the propylene is a propylene copolymer comprising a polypropylene matrix and up to 70 wt % of an ethylene-propylene rubber (EPR).

### Claim 14 (depends on 12)

Polypropylene according to claim 12, wherein the ethylene-propylene rubber (EPR) has an ethylene content of up to 50 wt %.

### Claim 15 (depends on 1)

Polypropylene according to claim 1 wherein the polypropylene has been produced in the presence of a catalyst system comprising an asymmetric catalyst, wherein the catalyst system has a porosity of less than 1.40 ml/g.

### Claim 16 (depends on 15)

Polypropylene according to claim 15, wherein the asymmetric catalyst is dimethylsilandiyl [(2-methyl-(4′-tert. butyl)-4-phenyl-indenyl)(2-isopropyl-(4′tert. butyl)-4-phenyl-indenyl)]zirconium dichloride and the catalytic system has a porosity of less than 1.40 ml/g.