# US 2010/0168333 A1 · Thermoplastic Resin Having Excellent Heat Resistance and Impact Strength and Method of Preparing the Same

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2010/0168333 A1
- Document ID: US20100168333A1
- Status: Published application
- Kind: A1
- Application number: 12/647,596
- Filed: 2009-12-28
- Published: 2010-07-01
- Earliest claimed: 2008-12-29
- Assignees: Cheil Industries Inc.
- Inventors: Jae Keun HONG; Byeong Do LEE; Ho Ryong SUN; Young Sub JIN; Hwan Seok PARK; Sung Kwan KIM; Sa Chun BAE
- Web page: https://patentgrep.com/patent/US20100168333A1

## CPC

- C08L 51/04: grafted on to rubbers
- C08L 35/06: Copolymers with vinyl aromatic monomers
- C08L 2205/02: containing two or more polymers of the same C08L -group
- C08L: COMPOSITIONS OF MACROMOLECULAR COMPOUNDS (compositions based on polymerisable monomers C08F, C08G; artificial filaments or fibres D01F; textile treating compositions D06)

## Abstract

The present invention provides a thermoplastic resin composition that can have excellent heat resistance and impact strength comprising a rubber-modified styrene resin and a copolymer of N-substituted maleimide compound and aromatic vinyl compound.

## Claims

### Claim 1

A thermoplastic resin composition that can have excellent heat resistance and impact strength comprising a rubber-modified styrene resin and a copolymer of N-substituted maleimide compound and aromatic vinyl compound.

### Claim 2 (depends on 1)

The thermoplastic resin composition of claim 1, wherein said thermoplastic resin composition is prepared by adding a solution phase of the copolymer of N-substituted maleimide compound and aromatic vinyl compound during continuous polymerization of the rubber-modified styrene resin.

### Claim 3 (depends on 2)

The thermoplastic resin composition of claim 2, wherein the solution phase of said copolymer of N-substituted maleimide compound and aromatic vinyl compound comprises said copolymer melted in an unsaturated nitrile compound.

### Claim 4 (depends on 1)

The thermoplastic resin composition of claim 1, wherein said thermoplastic resin composition includes about 1 to about 14.3 parts by weight of the copolymer of N-substituted maleimide compound and aromatic vinyl compound based on about 100 parts by weight of the rubber-modified styrene resin.

### Claim 5 (depends on 4)

The thermoplastic resin composition of claim 4, wherein said rubber-modified styrene resin further comprises about 0.005 to about 0.5 parts by weight of a multi-functional vinyl monomer.

### Claim 6 (depends on 5)

The thermoplastic resin composition of claim 5, wherein said multi-functional vinyl compound comprises divinylbenzene, ethylene glycol dimethacrylate, allyl methacrylate, diallyl phthalate, diallyl maleate, triallylisocyanurate or a combination thereof.

### Claim 7 (depends on 1)

The thermoplastic resin composition of claim 1, wherein said rubber-modified styrene resin comprises a graft copolymer resin prepared by graft copolymerizing an aromatic vinyl monomer and a unsaturated nitrile monomer onto a rubbery polymer, and a copolymer resin prepared by copolymerizing an aromatic vinyl monomer, unsaturated nitrile monomer and heat resistant aromatic vinyl monomer.

### Claim 8 (depends on 7)

The thermoplastic resin composition of claim 7, wherein said rubbery polymer comprises a conjugated diene rubber and a rubbery aromatic copolymer.

### Claim 9 (depends on 8)

The thermoplastic resin composition of claim 8, wherein said rubbery aromatic copolymer is prepared by copolymerizing about 50 to about 80% by weight of a conjugated diene compound and about 20 to about 50% by weight of an aromatic vinyl compound, and wherein said conjugated diene compound comprises 1,3-butadiene, 2-methyl-1,3-butadiene(isoprene), 2-ethyl-1,3-butadiene, 2,3-dimethyl-1,3-butadiene, 1,3-pentadiene, 3-butyl-1,3-oxtadiene or a combination thereof.

### Claim 10 (depends on 6)

The thermoplastic resin composition of claim 6, wherein said rubber-modified styrene resin comprises about 5 to about 20% by weight of the conjugated diene rubber, about 0.5 to about 8% by weight of the rubbery aromatic copolymer, about 15 to about 29% by weight of the heat resistant aromatic vinyl monomer, about 10 to about 50% by weight of the aromatic vinyl monomer and about 10 to about 30% by weight of the unsaturated nitrile monomer.

### Claim 11 (depends on 7)

The thermoplastic resin composition of claim 7, wherein said aromatic vinyl monomer comprises α-methyl styrene.

### Claim 12 (depends on 1)

The thermoplastic resin composition of claim 1, wherein said copolymer of N-substituted maleimide compound and aromatic vinyl compound is prepared by copolymerizing about 40 to about 60% by weight of the N-substituted maleimide compound and about 40 to about 60% by weight of the aromatic vinyl compound.

### Claim 13 (depends on 3)

The thermoplastic resin composition of claim 3, wherein said thermoplastic resin has a weight average molecular weight of about 100,000 to about 150,000.

### Claim 14 (depends on 1)

The thermoplastic resin composition of claim 1, wherein said thermoplastic resin has a polydispersity index of about 2 to about 4.

### Claim 15 (depends on 1)

The thermoplastic resin composition of claim 1, wherein said thermoplastic resin has a Izod impact strength (kgf·cm/cm, ⅛″ Notched) measured according to ASTM D256 of about 15 to about 35, a melt flow index (220° C., 10 kg) measured according to ASTM D1238 of about 3 to about 7, and a vicat softening temperature (5 kg, 50° C./hr) measured according to ISO R 306 of about 107 to about 115° C.

### Claim 16

A method of preparing a thermoplastic resin composition that can have excellent heat resist and impact strength comprising:
continuously feeding a first feed stream including a first reactant comprising a conjugated diene rubber, an aromatic rubbery copolymer, a heat resistant aromatic vinyl compound, an aromatic vinyl compound, a multi-functional vinyl compound and an initiator and a second feed stream that is different from the first feed stream including a second reactant comprising an unsaturated nitrile compound, a N-substituted maleimide compound and an aromatic vinyl compound to a reactor that is part of a plurality of reactors linked in series; and
thereafter polymerizing the first reactant and the second reactant to prepare a polymer.

### Claim 17

The method of 16, wherein the temperature of each of said reactors is maintained at about 90 to about 150° C.

### Claim 18

The method of 16, wherein the plurality of reactors includes a final polymerization reactor, and wherein the final polymerization reactor is maintained at a temperature of about 110 to about 140° C.

### Claim 19

The method of 16, further comprising delivering a polymer from the final polymerization reactor to a devolatizer apparatus and removing volatile components of the polymer.

### Claim 20

The method of 19, wherein the polymer delivered from the final polymerization reactor to the devolatizer at a temperature of about 140 to about 160° C.

### Claim 21

The method of 19, wherein said devolatizer apparatus is operated under the conditions of a temperature of about 230 to about 260° C. and a pressure of about 100 torr or less.

### Claim 22

The method of 16, wherein the number of the plurality of reactors is about 2 to about 5.

### Claim 23

The method of 16, wherein the first reactant and the second reactant are fed into the same reactor and polymerized.

### Claim 24

The method of 16, wherein the first reactant is fed into a first reactor and polymerization thereof is initiated in the first reactor to form a polymer, the second reactant is fed into a downstream reactor, the polymer from the first reactor is directed into the downstream reactor, and the second reactant participates in additional polymerization of the polymer in the downstream reactor.

### Claim 25

The method of 16, wherein said first reactant further comprises an organic solvent.