# US 2010/0168298 A1 · Method for manufacturing hydrogenated block copolymer

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2010/0168298 A1
- Document ID: US20100168298A1
- Status: Published application
- Kind: A1
- Application number: 12/368,824
- Filed: 2009-02-10
- Published: 2010-07-01
- Earliest claimed: 2008-12-30
- Assignees: TSRC Corporation
- Inventors: Huan-Chun Kao; Sheng-Te Yang; Hung-Chieh Hou; Chung-Ming Tsai
- Web page: https://patentgrep.com/patent/US20100168298A1

## CPC

- C08F 6/10: Removal of volatile materials, e.g. solvents {(C08F6/001, C08F6/003, C08F6/005, C08F6/006, C08F6/008, C08F6/02, C08F6/04 take precedence)}
- C08F 6/003: {from polymer solutions, suspensions, dispersions or emulsions without recovery of the polymer therefrom}
- C08F 8/04: Reduction, e.g. hydrogenation
- C08F: MACROMOLECULAR COMPOUNDS OBTAINED BY REACTIONS ONLY INVOLVING CARBON-TO-CARBON UNSATURATED BONDS

## Abstract

The present invention relates to a method for manufacturing a substantially hydrogenated vinyl aromatic/conjugated diene block copolymer, which has a hydrogenation level of greater than 90 percent. The resulting substantially hydrogenated vinyl aromatic/conjugated diene block copolymer has advantageous physical properties suitable for use in discs, optical films, light guide plates, etc.

## Claims

### Claim 1

A method for manufacturing a substantially hydrogenated block copolymer, comprising:
hydrogenating a block copolymer of a vinyl aromatic polymer block and a conjugated diene polymer block by contacting with a hydrogenating agent in the presence of a hydrogenation catalyst to obtain a polymer solution including a hydrogenated block copolymer having a hydrogenation level of greater than 90 percent and a solvent;
removing said solvent from said polymer solution by a flash devolatilization at a temperature of 200 to 300° C. and a pressure of 1 to 10 Bar to obtain a concentrated polymer solution with a residual solvent in an amount of 1 to 50 weight percent based on the total weight of said concentrated polymer solution; and
removing said residual solvent from said concentrated polymer solution by a devolatilizer at a pressure below 100 torr to isolate said hydrogenated block copolymer.

### Claim 2 (depends on 1)

The method as recited in claim 1, wherein said vinyl aromatic polymer block is polymerized from styrene.

### Claim 3 (depends on 1)

The method as recited in claim 1, wherein said conjugated diene polymer block is polymerized from butadiene or isoprene.

### Claim 4 (depends on 1)

The method as recited in claim 1, wherein said block copolymer is a copolymer polymerized from at least a vinyl aromatic and at least a conjugated diene monomer.

### Claim 5 (depends on 1)

The method as recited in claim 1, wherein said block copolymer has a number average molecular weight of 40000 to 150000.

### Claim 6 (depends on 1)

The method as recited in claim 1, wherein a weight ratio of said vinyl aromatic polymer block to said conjugated diene polymer block in said block copolymer is from about 40:60 to about 90:10.

### Claim 7 (depends on 1)

The method as recited in claim 1, wherein said solvent comprises a non-polar solvent.

### Claim 8 (depends on 7)

The method as recited in claim 7, wherein said solvent comprises cyclohexane.

### Claim 9 (depends on 1)

The method as recited in claim 1, wherein said hydrogenation catalyst includes a Group VIII metal component and at least one component selected from a group consisting of a rhenium, molybdenum, tungsten, tantalum,niobium and platinum.

### Claim 10 (depends on 9)

The method as recited in claim 9, wherein said hydrogenation catalyst includes a silica support.

### Claim 11 (depends on 1)

The method as recited in claim 1, wherein said devolatilizer comprises a twin-screw extruder, a film evaporator, a double flash tank or an assembly of the above.

### Claim 12 (depends on 1)

The method as recited in claim 1, further comprising filtering said polymer solution before removing said solvent from said polymer solution.

### Claim 13 (depends on 12)

The method as recited in claim 12, further comprising adding an antioxidant into said polymer solution after filtering said polymer solution and before removing said solvent from said polymer solution.

### Claim 14 (depends on 13)

The method as recited in claim 13, wherein said antioxidant comprises a hindered phenolic antioxidant and/or a phosphate ester antioxidant, and a decomposition temperature of said antioxidant is more than 150° C.

### Claim 15 (depends on 1)

The method as recited in claim 1, wherein said hydrogenating agent comprises hydrogen gas, hydrazine or sodium borohydride.

### Claim 16 (depends on 1)

The method as recited in claim 1, wherein said block copolymer is formed by using a polymerization initiator, said polymerization initiator comprising an organolithium compound.

### Claim 17 (depends on 1)

The method as recited in claim 1, wherein said polymer solution is maintained at a pressure of 9 to 30 Bar before entering into a flask tank to remove said solvent from said polymer solution by said flash devolatilization.

### Claim 18 (depends on 17)

The method as recited in claim 17, wherein said polymer solution is preheated to be maintained at a temperature range of 200 to 300° C. before entering into said flask tank to remove said solvent from said polymer solution by said flash devolatilization.

### Claim 19 (depends on 1)

The method as recited in claim 1, wherein said step of removing said residual solvent from said concentrated polymer solution is performed by a twin-screw extruder at a temperature of 200 to 300° C.

### Claim 20 (depends on 1)

The method as recited in claim 1, wherein said hydrogenation level is greater than 95 percent.

### Claim 21 (depends on 1)

The method as recited in claim 1, wherein said step of removing said residual solvent from said concentrated polymer solution by said devolatilizer is performed at a pressure below 20 torr to isolate said hydrogenated block copolymer.