# US 2010/0168274 A1 · Asphalt-rubber compositions and systems and methods for preparing same

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2010/0168274 A1
- Document ID: US20100168274A1
- Status: Published application
- Kind: A1
- Application number: 12/649,276
- Filed: 2009-12-29
- Published: 2010-07-01
- Earliest claimed: 2008-12-30
- Inventors: William B. Coe
- Web page: https://patentgrep.com/patent/US20100168274A1

## CPC

- C08L 95/005: {Aqueous compositions, e.g. emulsions}
- C09D 195/005: {Aqueous compositions, e.g. emulsions}
- C09J 195/005: {Aqueous compositions, e.g. emulsions}
- C08L 2555/60: Organic non-macromolecular ingredients, e.g. oil, fat, wax or natural dye
- C08L 2555/80: Macromolecular constituents
- C08L 2666/08: Homopolymers or copolymers according to C08L7/00 - C08L21/00; Derivatives thereof
- C08L: COMPOSITIONS OF MACROMOLECULAR COMPOUNDS (compositions based on polymerisable monomers C08F, C08G; artificial filaments or fibres D01F; textile treating compositions D06)
- C09D: COATING COMPOSITIONS, e.g. PAINTS, VARNISHES OR LACQUERS; FILLING PASTES; CHEMICAL PAINT OR INK REMOVERS; INKS; CORRECTING FLUIDS; WOODSTAINS; PASTES OR SOLIDS FOR COLOURING OR PRINTING; USE OF MATERIALS THEREFOR (cosmetics A61K; processes for applying liquids or other fluent materials to surfaces, in general, B05D; staining wood B27K5/02; glazes or vitreous enamels C03C; natural resins, French polish, drying-oils, driers, turpentine, per se, C09F; polishing compositions other than French polish, ski waxes C09G; adhesives or use of materials as adhesives C09J; materials for sealing or packing joints or covers C09K3/10; materials for stopping leaks C09K3/12; processes for the electrolytic or electrophoretic production of coatings C25D)
- C09J: ADHESIVES; NON-MECHANICAL ASPECTS OF ADHESIVE PROCESSES IN GENERAL; ADHESIVE PROCESSES NOT PROVIDED FOR ELSEWHERE; USE OF MATERIALS AS ADHESIVES (preparation of glue or gelatine C09H)

## Abstract

One embodiment provides a process for preparing an asphalt-coated crumb rubber composition that meets the specification set forth in ASTM D80-02 or deviations thereof which may be established by the specifying agency from time to time. The process generally comprises obtaining asphalt of different penetration grades, combining the asphalt of each grade with preselected chemicals to form separate premixed components, blending the premixed components together under predetermined conditions to form, upon curing, an asphalt-coated crumb rubber composition that meets certain physical requirements for asphalt-rubber binder (ARB), such as those set forth in ASTM D8-02. Advantageously, the resulting asphalt-coated crumb rubber composition not only meets the physical requirements of ARB used in road paving but also has improved dispersion of the rubber, such as dispersion of the rubber in an oil-in-water emulsion of an asphalt.

## Claims

### Claim 1

A method for preparing an emulsion of an asphalt-rubber binder comprising:
mixing a first asphalt with water and a first surfactant to form a first asphalt emulsion;
mixing a plurality of crumb rubber particles with an effective amount of a second asphalt to coat the particles to provide an asphalt-coated crumb rubber composition, and allowing the particles to swell; and
mixing the first asphalt emulsion with the asphalt-coated crumb rubber composition to provide an emulsion of an asphalt-rubber binder.

### Claim 2 (depends on 1)

The method of claim 1, wherein the first asphalt is harder than the second asphalt.

### Claim 3 (depends on 1)

The method of claim 1, wherein the first asphalt has a pen value in the range of about 0 dmm to about 100 dmm.

### Claim 4 (depends on 1)

The method of claim 1, wherein the first surfactant comprises an amine or an ammonium functional group.

### Claim 5 (depends on 4)

The method of claim 4, wherein the first surfactant is an amido amine surfactant, an ammonium salt thereof, or a combination thereof.

### Claim 6 (depends on 1)

The method of claim 1, wherein water is about 30% to about 50% of the weight of the first asphalt emulsion.

### Claim 7 (depends on 1)

The method of claim 1, wherein the second asphalt has a pen value in the range of about 100 dmm to about 200 dmm.

### Claim 8 (depends on 1)

The method of claim 1, wherein the second asphalt is above ambient temperature when mixed with the crumb rubber.

### Claim 9 (depends on 1)

The method of claim 1, wherein at least a portion of mixing a plurality of crumb rubber particles with a second asphalt occurs in the presence of oleic acid.

### Claim 10 (depends on 8)

The method of claim 8, wherein at least a portion of mixing a plurality of crumb rubber particles with a second asphalt occurs in the presence of oleic acid, and a fatty amine surfactant, an ammonium salt thereof, or a combination thereof.

### Claim 11 (depends on 1)

The method of claim 1, wherein the crumb rubber particles are about 60% to about 90% the total weight of all non-volatile components of the asphalt-coated crumb rubber composition.

### Claim 12 (depends on 1)

The method of claim 1, wherein at least a portion of mixing a plurality of crumb rubber particles with a second asphalt occurs in the presence of wood rosin, naphtha, a second surfactant, or a combination thereof.

### Claim 13 (depends on 12)

The method of claim 12, wherein at least a portion of mixing a plurality of crumb rubber particles with a second asphalt occurs in the presence of wood rosin, naphtha, a second surfactant, or a combination thereof, and a third surfactant comprising an amine functional group, an ammonium salt thereof, or a combination thereof.

### Claim 14 (depends on 1)

The method of claim 1, wherein the crumb rubber particles are about 20% to about 40% of the total weight of all non-volatile components of the asphalt-coated crumb rubber composition.

### Claim 15 (depends on 1)

The method of claim 1, further comprising:
mixing a third asphalt with a polymer to provide a polymer modified asphalt;
mixing the polymer modified asphalt with water and a fourth surfactant to provide a second asphalt emulsion; and
mixing the second asphalt emulsion with at least one of the first asphalt emulsion, the asphalt-coated crumb rubber composition, and the emulsion of the asphalt-rubber binder.

### Claim 16 (depends on 15)

The method of claim 15, wherein the third asphalt is softer than the first asphalt.

### Claim 17 (depends on 1)

An emulsion of an asphalt-rubber binder prepared by the process of claim 1.

### Claim 18 (depends on 17)

The emulsion of an asphalt-rubber binder of claim 17, comprising about 15% to about 30% crumb rubber based upon the total weight of all non-volatile components of the emulsion.

### Claim 19

An emulsion of an asphalt-rubber binder comprising:
an asphalt;
crumb rubber, representing about 30% to about 50% of the total weight of all non-volatile components of the emulsion, which has swollen in the presence of the asphalt;
a cationic surfactant;
and water;
wherein the emulsion is stable at a pH below about 7.

### Claim 20

An asphalt emulsion comprising:
an asphalt having a pen value of from about 0 dmm to about 30 dmm;
an amido amine surfactant, an ammonium salt thereof, or a combination thereof; and
water, representing about 30% to about 50% of the weight of the emulsion.

### Claim 21

An asphalt-coated rubber composition comprising:
an asphalt;
crumb rubber; and
an amount of a cationic surfactant which is effective to increase the hydrophilicity of the composition as compared to a composition which is identical except that it has no added cationic surfactant.

### Claim 22 (depends on 20)

The asphalt-coated rubber composition of claim 20, which has less than about 2% by weight of water.

### Claim 23 (depends on 20)

The asphalt-coated rubber composition of claim 20, wherein the crumb rubber is about 60% to about 80% of the weight of all non-volatile components of the asphalt-coated rubber composition.

### Claim 24 (depends on 20)

The asphalt-coated rubber composition of claim 20, wherein the crumb rubber is about 20% to about 40% of the weight of all non-volatile components of the asphalt-coated rubber composition.

### Claim 25

A method for preparing an emulsion of an asphalt-rubber binder comprising:
mixing a first asphalt emulsion with an asphalt-coated crumb rubber composition to provide an emulsion of an asphalt-rubber binder;
wherein the first asphalt emulsion is a product of mixing a first asphalt with water and a surfactant to form a first asphalt emulsion; and
wherein the asphalt-coated crumb rubber composition is a product of mixing a plurality of crumb rubber particles with an effective amount of a second asphalt to coat the particles, and wherein the second asphalt has caused the particles to swell.

### Claim 26

A method for preparing an emulsion of an asphalt-rubber binder comprising:
immersing finely ground rubber in a waterless, polymer modified asphalt;
reacting the finely ground rubber in the waterless, polymer modified asphalt to form a hot rubber adhesive; and
mixing the hot rubber adhesive with an asphalt emulsion to form an asphalt-rubber binder emulsion that can be cured at about 40° F.