# US 2010/0168258 A1 · Preparation of Cobalt-Ruthenium/zeolite fischer-tropsch catalysts

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2010/0168258 A1
- Document ID: US20100168258A1
- Status: Published application
- Kind: A1
- Application number: 12/649,135
- Filed: 2009-12-29
- Published: 2010-07-01
- Earliest claimed: 2008-12-29
- Assignees: Chevron U.S.A. Inc.
- Inventors: Charles L. Kibby; Alfred Haas
- Web page: https://patentgrep.com/patent/US20100168258A1

## CPC

- B01J 29/072: Iron group metals or copper
- B01J 29/146: {Y-type faujasite}
- B01J 29/46: Iron group metals or copper
- B01J 29/7615: {Zeolite Beta}
- B01J 29/7669: {MTW-type, e.g. ZSM-12, NU-13, TPZ-12 or Theta-3}
- C10G 2/332: {of the iron-group}
- B01J 37/0045: {Drying a slurry, e.g. spray drying}
- B01J 37/32: Freeze drying, i.e. lyophilisation
- B01J 2229/186: not in framework positions
- C10G 2300/705: Passivation
- B01J: CHEMICAL OR PHYSICAL PROCESSES, e.g. CATALYSIS OR COLLOID CHEMISTRY; THEIR RELEVANT APPARATUS
- C10G: CRACKING HYDROCARBON OILS; PRODUCTION OF LIQUID HYDROCARBON MIXTURES, e.g. BY DESTRUCTIVE HYDROGENATION, OLIGOMERISATION, POLYMERISATION (cracking to hydrogen or synthesis gas C01B; cracking or pyrolysis of hydrocarbon gases to individual hydrocarbons or mixtures thereof of definite or specified constitution C07C; cracking to cokes C10B); RECOVERY OF HYDROCARBON OILS FROM OIL-SHALE, OIL-SAND, OR GASES; REFINING MIXTURES MAINLY CONSISTING OF HYDROCARBONS; REFORMING OF NAPHTHA; MINERAL WAXES

## Abstract

A method for forming a cobalt-containing Fischer-Tropsch catalyst involves precipitating a cobalt oxy-hydroxycarbonate species by turbulent mixing, during which a basic solution collides with an acidic solution comprising cobalt. The method further involves depositing the cobalt oxy-hydroxycarbonate species onto an acidic support to provide a catalyst comprising cobalt and the acidic support. The acidic support comprises a zeolite, a molecular sieve, or combinations thereof.

## Claims

### Claim 1

A method for forming a cobalt-containing Fischer-Tropsch catalyst, comprising:
precipitating a cobalt oxy-hydroxycarbonate species by turbulent mixing, wherein a basic solution is collided with an acidic solution comprising cobalt; and
depositing the cobalt oxy-hydroxycarbonate species onto an acidic support to provide a catalyst comprising cobalt and the acidic support, wherein the acidic support comprises a zeolite, a molecular sieve, or combinations thereof.

### Claim 2 (depends on 1)

The method of claim 1, wherein depositing the cobalt oxy-hydroxycarbonate species onto the acidic support comprises injecting the cobalt oxy-hydroxycarbonate species into an aqueous slurry of the acidic support.

### Claim 3 (depends on 1)

The method of claim 1, wherein depositing the cobalt oxy-hydroxycarbonate species onto the acidic support comprises mixing the acidic support with the basic solution such that the cobalt oxy-hydroxycarbonate species is precipitated onto the acidic support.

### Claim 4 (depends on 1)

The method of claim 1, further comprising multiple precipitation/deposition iterations with intervening decompositions.

### Claim 5 (depends on 1)

The method of claim 1, wherein the weight ratio of the zeolite, the molecular sieve, or combinations thereof to cobalt is at least about 10:1.

### Claim 6 (depends on 1)

The method of claim 1, wherein the acidic solution and a basic solution are heated.

### Claim 7 (depends on 6)

The method of claim 6, wherein the acidic solution and a basic solution are heated to a temperature of about 80° C.

### Claim 8 (depends on 1)

The method of claim 1, wherein the acidic solution comprises cobalt (II) nitrate.

### Claim 9 (depends on 1)

The method of claim 1, wherein the acidic solution further comprises one or more metals selected from the group consisting of Re, Ru, Pt, Pd, Ir, Rh, Os, Au, Ag, Cu, and Mn.

### Claim 10 (depends on 9)

The method of claim 9, wherein the acidic solution comprises Co(NO3)2*6H2O+Ru(NO)(NO3)3.

### Claim 11 (depends on 10)

The method of claim 10, wherein the acidic solution has a weight ratio of Co:Ru between about 20:1 and about 400:1.

### Claim 12 (depends on 1)

The method of claim 1, wherein the basic solution comprises (NH4)2CO3 and has a pH of about 7 to about 8.

### Claim 13 (depends on 1)

The method of claim 1, further comprising decomposing the oxy-hydroxycarbonate species from about 200° C. to about 250° C. in an oxidizing environment, inert gas or a reducing environment.

### Claim 14 (depends on 13)

The method of claim 13, further comprising calcining the catalyst comprising cobalt and the acidic support at a temperature of about 300° C. to about 400° C.

### Claim 15 (depends on 1)

The method of claim 1, further comprising reducing the catalyst comprising cobalt and the acidic support.

### Claim 16 (depends on 15)

The method of claim 15, further comprising re-oxidizing the catalyst comprising cobalt and the acidic support at ≦about 300° C.

### Claim 17 (depends on 16)

The method of claim 16, further comprising reducing the catalyst comprising cobalt and the acidic support for a second time.

### Claim 18 (depends on 17)

The method of claim 17, further comprising passivating the catalyst comprising cobalt and the acidic support between reducing and re-oxidizing and/or after reducing for a second time.

### Claim 19 (depends on 1)

A method of performing a Fischer-Tropsch synthesis reaction, comprising:
forming a cobalt-containing Fischer-Tropsch catalyst according to the method of claim 1; and
contacting the cobalt-containing Fischer-Tropsch catalyst with synthesis gas to provide Fischer-Tropsch products.

### Claim 20 (depends on 19)

The method of claim 19, wherein the Fischer-Tropsch products comprise between 0.00 wt % and about 0.02 wt % alcohols.