# US 2010/0167919 A1 · Hydrocarbon reforming catalyst, method of preparing the same and fuel cell including the hydrocarbon reforming catalyst

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2010/0167919 A1
- Document ID: US20100167919A1
- Status: Published application
- Kind: A1
- Application number: 12/641,599
- Filed: 2009-12-18
- Published: 2010-07-01
- Earliest claimed: 2008-12-30
- Assignees: Samsung Electronics Co., Ltd.; Samsung SDI Co., Ltd.
- Inventors: Hyun-chul LEE; Doo-hwan Lee; Eun-duck Park; Kang-hee Lee; Yun-ha Kim; Jae-hyun Park
- Web page: https://patentgrep.com/patent/US20100167919A1

## CPC

- H01M 8/0618: {Reforming processes, e.g. autothermal, partial oxidation or steam reforming}
- B01J 23/78: with alkali- or alkaline earth metals
- B01J 23/83: with rare earths or actinides
- B01J 23/835: with germanium, tin or lead
- B01J 23/8872: {Alkali or alkaline earth metals}
- B01J 23/888: Tungsten
- B01J 23/8892: {Manganese}
- B01J 23/8896: {Rhenium}
- B01J 37/0205: {in several steps}
- C01B 3/40: characterised by the catalyst
- C01B 3/48: followed by reaction of water vapour with carbon monoxide
- H01M 8/0625: {in a modular combined reactor/fuel cell structure}
- C01B 2203/0233: the reforming step being a steam reforming step
- C01B 2203/0283: containing a CO-shift step, i.e. a water gas shift step
- C01B 2203/066: with fuel cells
- C01B 2203/1041: Composition of the catalyst
- C01B 2203/1058: Nickel catalysts
- C01B 2203/1082: Composition of support materials
- C01B 2203/1235: Hydrocarbons
- Y02E 60/50: Fuel cells
- Y02P 20/52: using catalysts, e.g. selective catalysts
- Y02P 70/50: Manufacturing or production processes characterised by the final manufactured product
- H01M: PROCESSES OR MEANS, e.g. BATTERIES, FOR THE DIRECT CONVERSION OF CHEMICAL ENERGY INTO ELECTRICAL ENERGY
- B01J: CHEMICAL OR PHYSICAL PROCESSES, e.g. CATALYSIS OR COLLOID CHEMISTRY; THEIR RELEVANT APPARATUS
- C01B: NON-METALLIC ELEMENTS; COMPOUNDS THEREOF; {METALLOIDS OR COMPOUNDS THEREOF NOT COVERED BY SUBCLASS C01C}
- Y02E: REDUCTION OF GREENHOUSE GAS [GHG] EMISSIONS, RELATED TO ENERGY GENERATION, TRANSMISSION OR DISTRIBUTION
- Y02P: CLIMATE CHANGE MITIGATION TECHNOLOGIES IN THE PRODUCTION OR PROCESSING OF GOODS

## Abstract

A hydrocarbon reforming catalyst includes an oxide support as well as a nickel active catalyst layer, a metal oxide, an alkali metal supported by the oxide support.

## Claims

### Claim 1

A hydrocarbon reforming catalyst comprising:
an oxide support; and
a nickel, a metal oxide, and an alkali metal or alkali earth metal supported by the oxide support.

### Claim 2 (depends on 1)

The hydrocarbon reforming catalyst of claim 1, wherein the oxide support comprises at least one oxide selected from the group consisting of Al2O3, SiO2, ZrO2, TiO2 and yttria-stabilized zirconia (YSZ).

### Claim 3 (depends on 1)

The hydrocarbon reforming catalyst of claim 1, wherein the metal oxide comprises at least one oxide selected from the group consisting of manganese oxide, tin oxide, cerium oxide, rhenium oxide, molybdenum oxide and tungsten oxide.

### Claim 4 (depends on 1)

The hydrocarbon reforming catalyst of claim 1, wherein the alkali metal or alkali earth metal comprises at least one metal selected from the group consisting of lithium, sodium, potassium, magnesium, and calcium.

### Claim 5 (depends on 1)

The hydrocarbon reforming catalyst of claim 1, wherein the metal oxide is distributed on a layer including the nickel.

### Claim 6 (depends on 1)

The hydrocarbon reforming catalyst of claim 1, wherein the metal oxide is distributed in a layer including the nickel.

### Claim 7 (depends on 1)

The hydrocarbon reforming catalyst of claim 1, wherein the amount of nickel is in a range of about 1.0 to about 40 parts by weight based on 100 parts by weight of the hydrocarbon reforming catalyst.

### Claim 8 (depends on 1)

The hydrocarbon reforming catalyst of claim 1, wherein the amount of metal in the metal oxide is in a range of about 0.5 to about 20 parts by weight based on 1 part by weight of nickel.

### Claim 9 (depends on 1)

The hydrocarbon reforming catalyst of claim 1, wherein the amount of alkali metal or alkali earth metal is in a range of about 0.1 to about 20 parts by weight based on 100 parts by weight of the hydrocarbon reforming catalyst.

### Claim 10 (depends on 1)

The hydrocarbon reforming catalyst of claim 1, wherein the metal oxide is manganese oxide and the alkali metal is potassium.

### Claim 11 (depends on 1)

The hydrocarbon reforming catalyst of claim 1, wherein a carbon deposition rate of the hydrocarbon reforming catalyst is less than 10%.

### Claim 12 (depends on 11)

The hydrocarbon reforming catalyst of claim 11, wherein the carbon deposition rate is less than 5%.

### Claim 13

A method of manufacturing a hydrocarbon reforming catalyst, the method comprising:
loading nickel onto an oxide support, thereby obtaining a first resultant structure;
loading a metal oxide onto the first resultant structure; and
loading alkali metal or alkali earth metal,
wherein the alkali metal or alkali earth metal is loaded at least one time selected from before the nickel is loaded, after the nickel is loaded and before the metal oxide is loaded, and after the metal oxide is loaded.

### Claim 14 (depends on 13)

The method of claim 13, wherein the loading of the nickel, the loading of the metal oxide, and the loading of the alkali metal or alkali earth metal are each performed independently by deposition precipitation, co-precipitation, wet impregnation, sputtering, gas-phase grafting, liquid-phase grafting or incipient-wetness impregnation.

### Claim 15 (depends on 13)

The method of claim 13, wherein each of the loading of the nickel, the loading of the metal oxide, and the loading of the alkali metal or alkali earth metal further comprises performing a heat-treatment process at a temperature in a range of about 500 to about 750° C. for about 2 to about 5 hours.

### Claim 16 (depends on 13)

The method of claim 13, wherein the metal oxide comprises at least one oxide selected from the group consisting of manganese oxide, tin oxide, cerium oxide, rhenium oxide, molybdenum oxide and tungsten oxide.

### Claim 17 (depends on 13)

The method of claim 13, wherein the oxide support comprises at least one oxide selected from the group consisting of Al2O3, SiO2, ZrO2, TiO2 and YSZ.

### Claim 18 (depends on 13)

The method of claim 13, wherein the alkali metal or alkali earth metal comprises at least one metal selected from the group consisting of lithium, sodium, potassium, magnesium and potassium.

### Claim 19

A method of manufacturing a hydrocarbon reforming catalyst, the method comprising:
loading a metal oxide onto an oxide support, thereby obtaining a first resultant structure;
loading nickel onto the first resultant structure; and
loading an alkali metal or alkali earth metal,
wherein the alkali metal or alkali earth metal is loaded at at least one time selected from before the metal oxide is loaded, after the metal oxide is loaded and before the nickel is loaded, and after the nickel is loaded.

### Claim 20

A method of manufacturing a hydrocarbon reforming catalyst, the method comprising:
simultaneously loading a metal oxide and nickel onto an oxide support; and
loading a alkali metal or alkali earth metal,
wherein the alkali metal or alkali earth metal is loaded before or after the metal oxide and nickel are simultaneously loaded.

### Claim 21

A method of manufacturing a hydrocarbon reforming catalyst, the method comprising simultaneously loading nickel, a metal oxide, and an alkali metal or alkali earth metal onto an oxide support.

### Claim 22 (depends on 1)

A fuel cell comprising the hydrocarbon reforming catalyst of claim 1.