# US 2010/0167917 A1 · Method for producing a hydrogen storage material

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2010/0167917 A1
- Document ID: US20100167917A1
- Status: Published application
- Kind: A1
- Application number: 12/063,496
- Filed: 2006-07-27
- Published: 2010-07-01
- Earliest claimed: 2005-08-10
- Assignees: Forschungszentrum Karlsruhe GmbH
- Inventors: Maximilian Fichtner; Christoph Frommen
- Web page: https://patentgrep.com/patent/US20100167917A1

## CPC

- C01B 3/0078: Composite solid storage media, e.g. mixtures of polymers and metal hydrides, coated solid compounds or structurally heterogeneous solid compounds
- C01B 3/001: characterised by the uptaking media; Treatment thereof
- Y02E 60/32: Hydrogen storage
- C01B: NON-METALLIC ELEMENTS; COMPOUNDS THEREOF; {METALLOIDS OR COMPOUNDS THEREOF NOT COVERED BY SUBCLASS C01C}
- Y02E: REDUCTION OF GREENHOUSE GAS [GHG] EMISSIONS, RELATED TO ENERGY GENERATION, TRANSMISSION OR DISTRIBUTION

## Abstract

Method for producing a hydrogen storage material that includes a metal hydride and a non-hydrogenated material and that is doped with a metal as a catalyst, includes; mixing a catalyst precursor, which includes the metal, with the non-hydrogenated material so as to provide a first mixture; agitating the first mixture; thermally treating the first mixture so as to form a composite of the non-hydrogenated material and the metal; mixing the composite with the metal hydride so as to provide a second mixture; and grinding the second mixture so as to provide the hydrogen storage material.

## Claims

### Claim at position 1

1-12. (canceled)

### Claim 13

A method for producing a hydrogen storage material that includes a metal hydride and a non-hydrogenated material and that is doped with a metal as a catalyst, comprising:
a) mixing a catalyst precursor, which includes the metal, with the non-hydrogenated material so as to provide a first mixture;
b) agitating the first mixture;
c) thermally treating the first mixture so as to form a composite of the non-hydrogenated material and the metal;
d) mixing the composite with the metal hydride so as to provide a second mixture; and
e) grinding the second mixture so as to provide the hydrogen storage material.

### Claim 14 (depends on 13)

The method as recited in claim 13, wherein the metal of the catalyst precursor includes at least one of a rare earth metal and a transition metal from the group 3 through 11 of the periodic system.

### Claim 15 (depends on 14)

The method as recited in claim 14, wherein the metal of the catalyst precursor includes at least one of titanium, zirconium, iron, cobalt, nickel, cerium, a mixture thereof and an alloy thereof.

### Claim 16 (depends on 13)

The method as recited in claim 13, wherein the catalyst precursor is present in the form of at least one of a halogenide, a hydride, a carbide, a nitride, oxide and an alcoholate.

### Claim 17 (depends on 16)

The method as recited in claim 16, wherein the catalyst precursor is present in the form of a chloride.

### Claim 18 (depends on 13)

The method as recited in claim 13, wherein the non-hydrogenated material of the hydrogen storage material includes an element of the 3rd main group of the periodic system.

### Claim 19 (depends on 18)

The method as recited in claim 18, wherein the non-hydrogenated material of the hydrogen storage material includes at least one of aluminum and boron.

### Claim 20 (depends on 13)

The method as recited in claim 13, wherein the metal hydride includes at least one of LiH, NaH, KH and a mixture thereof.

### Claim 21 (depends on 13)

The method as recited in claim 13, wherein the mixing the catalyst precursor with the non-hydrogenated material includes adding an organic solvent with the non-hydrogenated material.

### Claim 22 (depends on 21)

The method as recited in claim 21, wherein the organic solvent includes at least one of tetrahydrofuran and diethyl ether.

### Claim 23 (depends on 13)

The method as recited in claim 13, wherein the thermally treating the first mixture is carried out below the melting point of the non-hydrogenated material and at a temperature of between 250° C. and 900° C.

### Claim 24 (depends on 23)

The method as recited in claim 23, wherein the thermally treating the mixture is carried out at a temperature of between 350° C. and 600° C.