# US 2010/0167841 A1 · Golf ball and process for preparing the same

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2010/0167841 A1
- Document ID: US20100167841A1
- Status: Published application
- Kind: A1
- Application number: 12/647,122
- Filed: 2009-12-24
- Published: 2010-07-01
- Earliest claimed: 2008-12-26
- Assignees: Dunlop Sports Co. Ltd.
- Inventors: Satoko OKABE; Keiji Ohama; Takahiro Shigemitsu
- Web page: https://patentgrep.com/patent/US20100167841A1

## CPC

- A63B 37/0003: {Golf balls}
- A63B 37/0039: {characterised by the material}
- A63B 37/004: {Physical properties}
- A63B 37/0075: {Three piece balls, i.e. cover, intermediate layer and core}
- A63B 45/00: Apparatus or methods for manufacturing balls (working of plastics or substances in a plastic state B29)
- A63B: APPARATUS FOR PHYSICAL TRAINING, GYMNASTICS, SWIMMING, CLIMBING, OR FENCING; BALL GAMES; TRAINING EQUIPMENT (apparatus for passive exercising, massage A61H)

## Abstract

An object of the present invention is to provide a golf ball providing a great distance. Another object of the present invention is to provide a golf ball striking a balance between a flight distance on a driver shot and an approach performance on an approach shot while providing an excellent shot feeling. The present invention provides a golf ball comprising: a center, a cover and at least one intermediate layer disposed between the center and the cover, wherein at least one piece or one layer of the intermediate layer is formed from a high fluidity intermediate layer composition that contains (A) a polyamide resin composition having a flexural modulus in a range from 700 MPa to 4,000 MPa; (B) at least one member selected from the group consisting of an ethylene-(meth)acrylic acid binary copolymer, a metal-neutralized product of the binary copolymer, an ethylene-(meth)acrylic acid-(meth)acrylic acid ester ternary copolymer, and a metal-neutralized product of the ternary copolymer, and (C) a fluidity improving agent.

## Claims

### Claim 1

A golf ball comprising:
a center, a cover and at least one intermediate layer disposed between the center and the cover,
wherein at least one piece or one layer of the intermediate layer is formed from a high fluidity intermediate layer composition that contains
(A) a polyamide resin composition having a flexural modulus in a range from 700 MPa to 4,000 MPa;
(B) at least one member selected from the group consisting of an ethylene-(meth)acrylic acid binary copolymer, a metal-neutralized product of the binary copolymer, an ethylene-(meth)acrylic acid-(meth)acrylic acid ester ternary copolymer, and a metal-neutralized product of the ternary copolymer, and
(C) a fluidity improving agent.

### Claim 2 (depends on 1)

The golf ball according to claim 1, further comprising a surrounding layer between the center and the intermediate layer.

### Claim 3

A golf ball comprising:
a core having a center and at least one intermediate layer covering the center; and
a cover covering the core,
wherein at least one piece or one layer of the intermediate layer is formed from a high fluidity intermediate layer composition that contains
(A) a polyamide resin composition having a flexural modulus in a range from 700 MPa to 4,000 MPa and a melt flow rate (240° C., 2.16 kg) of 5.0 g/10 min or more, and containing (a-1) a polyimide resin and (a-2) a resin having at least one functional group selected from the group consisting of a hydroxyl group, a carboxyl group, an anhydride group, a sulfonic acid group, and an epoxy group (including a glycidyl group);
(B) at least one member selected from the group consisting of an ethylene-(meth)acrylic acid binary copolymer, a metal-neutralized product of the binary copolymer, an ethylene-(meth)acrylic acid-(meth)acrylic acid ester ternary copolymer, and a metal-neutralized product of the ternary copolymer; and
(C) a fluidity improving agent.

### Claim 4 (depends on 3)

The golf ball according to claim 3, wherein the high fluidity intermediate layer composition has a melt flow rate (240° C., 2.16 kg) in a range from 5.0 g/10 min to 50.0 g/10 min.

### Claim 5 (depends on 3)

The golf ball according to claim 3, wherein the high fluidity intermediate layer composition has a flexural modulus in a range from 350 MPa to 1,000 MP, and a slab hardness in a range from 65 to 75 in Shore D hardness.

### Claim 6 (depends on 3)

The golf ball according to claim 3, wherein a content ratio ((A)/(B)) of (A) component to (B) component (a total is 100 mass %) in the high fluidity intermediate layer composition is 20 mass % to 80 mass %/80 mass % to 20 mass %, and a blending amount of (C) the fluidity improving agent in the high fluidity intermediate layer composition is from 1 part to 30 parts by mass with respect to 100 parts by mass of a sum of (A) component and (B) component.

### Claim 7 (depends on 3)

The golf ball according to claim 3, wherein (a-1) the polyamide resin is at least one selected from the group consisting of polyamide 6, polyamide 11, polyamide 12, polyamide 66, polyamide 610, polyamide 6T, polyamide 6I, polyamide 9T, polyamide M5T, polyamide 612 and a polyetherblock amide copolymer.

### Claim 8 (depends on 3)

The golf ball according to claim 3, wherein (a-2) the resin having at least one functional group selected from the group consisting of a hydroxyl group, a carboxyl group, an anhydride group, a sulfonic acid group, and an epoxy group (including a glycidyl group) is a thermoplastic elastomer having at least one functional group selected from the group consisting of a hydroxyl group, a carboxyl group, an anhydride group, a sulfonic acid group, and an epoxy group (including a glycidyl group).

### Claim 9 (depends on 8)

The golf ball according to claim 8, wherein the thermoplastic elastomer contains at least one member selected from the group consisting of a thermoplastic polyolefin elastomer, a thermoplastic polyester elastomer, a thermoplastic polyamide elastomer, a thermoplastic polyurethane elastomer, and a thermoplastic polystyrene elastomer.

### Claim 10 (depends on 8)

The golf ball according to claim 8, wherein the thermoplastic elastomer is a thermoplastic polystyrene elastomer.

### Claim 11 (depends on 3)

The golf ball according to claim 3, wherein (B) component is the metal-neutralized product of the ethylene-(meth)acrylic acid binary copolymer, and/or the metal-neutralized product of the ethylene-(meth)acrylic acid-(meth)acrylic acid ester ternary copolymer, and is neutralized with at least one metal selected from the group consisting of Li, Na, Ca, Zn, Mg and Cu.

### Claim 12 (depends on 3)

The golf ball according to claim 3, wherein (C) the fluidity improving agent includes at least one selected from the group consisting of a fatty acid, a metal salt thereof, a nonionic thermoplastic resin having a melt viscosity (190° C.) ranging from 5 Pa·s to 1,000 Pa·s measured by a flow tester, and an ionomer resin having a melt viscosity (190° C.) ranging from 1 Pa·s to 10 Pa·s measured by a brookfield viscometer.

### Claim 13 (depends on 3)

The golf ball according to claim 3, wherein the intermediate layer has a thickness in a range from 0.5 mm to 2.0 mm.

### Claim 14

A process for producing a golf ball having a core having a center and at least one intermediate layer covering the center and a cover covering the core, comprising,
dry blending (A) a polyamide resin composition having a flexural modulus in a range from 700 MPa to 4,000 MPa and a melt flow rate (240° C., 2.16 kg) of 5.0 g/10 min or more, and containing (a-1) a polyamide resin and (a-2) a resin having at least one functional group selected from the group consisting of a hydroxyl group, a carboxyl group, an anhydride group, a sulfonic acid group, and an epoxy group (including a glycidyl group) with (B) at least one member selected from the group consisting of an ethylene-(meth)acrylic acid binary copolymer, a metal-neutralized product of the binary copolymer, an ethylene-(meth)acrylic acid-(meth)acrylic acid ester ternary copolymer, and a metal-neutralized product of the ternary copolymer;
mixing a melt of (C) a fluidity improving agent to an obtained mixture of (A) component and (B) component, while adding (C) the fluidity improving agent in a liquid state to prepare a high fluidity intermediate layer composition by extrusion,
forming an intermediate layer from the obtained high fluidity intermediate layer composition; and
forming a cover from a cover composition on the intermediate layer.

### Claim 15

A golf ball comprising:
an inner core consisting of a center and a surrounding layer covering the center,
at least one intermediate layer covering the inner core, and
a cover covering the intermediate layer,
wherein at least one piece or one layer of the intermediate layer is formed from a high fluidity intermediate layer composition that has a melt flow rate (240° C., 2.16 kg) of 5.0 g/10 min or more and contains;
(A) a polyamide resin composition having a flexural modulus in a range from 700 MPa to 4,000 MPa;
(B) at least one member selected from the group consisting of an ethylene-(meth)acrylic acid binary copolymer, a metal-neutralized product of the binary copolymer, an ethylene-(meth)acrylic acid-(meth)acrylic acid ester ternary copolymer, and a metal-neutralized product of the ternary copolymer; and
(C) a fluidity improving agent,
wherein a surface hardness (H6) of the intermediate layer and a surface hardness (H4) of the inner core satisfy the equation: H6≧H4, and the cover has a slab hardness (H7) of 45 or less in Shore D hardness.

### Claim 16 (depends on 15)

The golf ball according to claim 15, wherein (A) the polyamide resin composition contains (a-2) a resin having at least one functional group selected from the group consisting of a hydroxyl group, a carboxyl group, an anhydride group, a sulfonic acid group, and an epoxy group (including a glycidyl group) and has a melt flow rate (240° C., 2.16 kg) of 5.0 g/10 min or more.

### Claim 17 (depends on 15)

The golf ball according to claim 15, wherein the inner core has a surface hardness (H4) from 45 to 65 in Shore D hardness.

### Claim 18 (depends on 15)

The golf ball according to claim 15, wherein the high fluidity intermediate layer composition has a flexural modulus in a range from 400 MPa to 1,000 MP, and a slab hardness in range from 65 to 75 in Shore D hardness.

### Claim 19 (depends on 15)

The golf ball according to claim 15, wherein (A) the polyamide resin composition contains at least one selected from the group consisting of polyamide 6, polyamide 11, polyamide 12, polyamide 66, polyamide 610, polyamide 6T, polyamide 6I, polyamide 9T, polyamide M5T, polyamide 612 and a polyetherblock amide copolymer.

### Claim 20 (depends on 15)

The golf ball according to claim 15, wherein (C) the fluidity improving agent includes at least one selected from the group consisting of a fatty acid, a metal salt thereof, a nonionic thermoplastic resin having a melt viscosity (190° C.) ranging from 5 Pa·s to 1,000 Pa·s measured by a flow tester, and an ionomer resin having a melt viscosity (190° C.) ranging from 1 Pa·s to 10 Pa·s measured by a brookfield viscometer.

### Claim 21 (depends on 15)

The golf ball according to claim 15, wherein the cover has a thickness of 0.8 mm or less.