# US 2010/0167530 A1 · Method for forming metal line of semiconductor device

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2010/0167530 A1
- Document ID: US20100167530A1
- Status: Published application
- Kind: A1
- Application number: 12/643,908
- Filed: 2009-12-21
- Published: 2010-07-01
- Earliest claimed: 2008-12-29
- Inventors: Chung-Kyung Jung
- Web page: https://patentgrep.com/patent/US20100167530A1

## CPC

- H10P 70/234: {the processing being the formation of vias or contact holes}
- H10W 20/081: {by forming openings in the dielectric parts}
- H10W 20/084: {for dual-damascene structures}
- H10P: GENERIC PROCESSES OR APPARATUS FOR THE MANUFACTURE OR TREATMENT OF DEVICES COVERED BY CLASS H10
- H10W: GENERIC PACKAGES, INTERCONNECTIONS, CONNECTORS OR OTHER CONSTRUCTIONAL DETAILS OF DEVICES COVERED BY CLASS H10

## Abstract

Disclosed is a method for forming a metal line of a semiconductor device. The method includes forming a first photoresist pattern on at least one interlayer dielectric provided on a semiconductor substrate, etching the interlayer dielectric using the first photoresist pattern to form a trench, removing the first photoresist pattern by ashing, and primarily removing residues left in the trench using a first cleaning solution comprising TMH, H2O2 and H2. Accordingly, copper metal lines with a great thickness of not less than 3 to 5 um can be formed, while preventing generation of voids in the process of forming the diffusion barrier and metal lines, thus advantageously improving yield and reliability of products.

## Claims

### Claim 1

A method comprising:
forming a first photoresist pattern over at least one interlayer dielectric provided over a semiconductor substrate;
etching the interlayer dielectric using the first photoresist pattern to form a trench;
removing the first photoresist pattern by performing an ashing process; and then
performing a primary cleaning process removing residues left in the trench using a first cleaning solution comprising TMH, H2O2 and H2.

### Claim 2 (depends on 1)

The method of claim 1, further comprising:
performing a secondary cleaning process removing residues left behind after performing the primary cleaning process using a second solution comprising an amine-based compound.

### Claim 3 (depends on 1)

The method of claim 1, wherein the ashing process is performed prior to performing the primary cleaning process.

### Claim 4 (depends on 1)

The method of claim 1, wherein the first cleaning solution has a ratio of TMH, H2O2 and H2O of 1:2 to 5:10 to 40.

### Claim 5 (depends on 4)

The method of claim 4, wherein performing the first cleaning process is carried out for 5 to 10 minutes.

### Claim 6 (depends on 1)

The method of claim 1, further comprising:
forming a second photoresist pattern over the interlayer dielectric including the trench;
etching the interlayer dielectric using the second photoresist pattern to form a via hole;
removing the second photoresist pattern;
forming a diffusion barrier over the trench and the via hole; and
embedding a metal layer in the trench and the via hole and over the diffusion barrier to form a metal line.

### Claim 7 (depends on 6)

The method of claim 6, wherein performing the first cleaning process is carried out prior to forming the via hole.

### Claim 8 (depends on 6)

The method of claim 6, further comprising:
performing a tertiary cleaning process prior to forming the diffusion barrier to remove residues left in the via hole using a third cleaning solution comprising an amine-based compound.

### Claim 9 (depends on 6)

The method of claim 6, wherein the metal line has a thickness not less than 3 μm to 5 μm.

### Claim 10 (depends on 1)

The method of claim 1, wherein polymer produced during formation of the trench is used for the formation of the trench.

### Claim 11 (depends on 1)

The method of claim 1, wherein the residues are removed in a batch manner using the first cleaning solution.

### Claim 12 (depends on 2)

The method of claim 2, wherein particles and polymer are removed from the residues using the first cleaning solution.

### Claim 13

A method comprising:
forming an interlayer dielectric over a semiconductor substrate
forming a trench in the interlayer dielectric layer by etching the interlayer dielectric;
performing a first cleaning process to remove residues in the trench after forming the trench; and then
performing a second cleaning process to remove residues in the trench after performing the first cleaning process.

### Claim 14 (depends on 13)

The method of claim 13, wherein the first cleaning process uses a first cleaning solution comprising TMH, H2O2 and H2.

### Claim 15 (depends on 14)

The method of claim 14, wherein the first cleaning solution has a ratio of TMH, H2O2 and H2O of 1:2 to 5:10 to 40.

### Claim 16 (depends on 13)

The method of claim 13, wherein the second cleaning process uses a second cleaning solution comprising an amine-based compound.

### Claim 17

A method comprising:
forming an interlayer dielectric over a semiconductor substrate
forming a trench in the interlayer dielectric layer by etching the interlayer dielectric;
performing a first cleaning process to remove residues in the trench after forming the trench;
performing a second cleaning process to remove residues in the trench after performing the first cleaning process;
forming a via hole by etching the interlayer dielectric using the second photoresist pattern;
performing a third cleaning process to remove residues in the via hole after forming the via hole;
forming a diffusion barrier over the trench and the via hole; and then
forming a metal line in the trench and the via hole and over the diffusion barrier.

### Claim 18 (depends on 17)

The method of claim 17, wherein the first cleaning process uses a first cleaning solution comprising TMH, H2O2 and H2.

### Claim 19 (depends on 17)

The method of claim 17, wherein the second cleaning process uses a second cleaning solution comprising an amine-based compound.

### Claim 20 (depends on 17)

The method of claim 17, wherein the third cleaning process uses a third cleaning solution comprising an amine-based compound.