# US 2010/0167527 A1 · Method of depositing tungsten film with reduced resistivity and improved surface morphology

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2010/0167527 A1
- Document ID: US20100167527A1
- Status: Published application
- Kind: A1
- Application number: 12/637,864
- Filed: 2009-12-15
- Published: 2010-07-01
- Earliest claimed: 2008-12-31
- Assignees: Applied Materials, Inc.
- Inventors: Kai Wu; Amit Khandelwal; Averinos V. Gelatos
- Web page: https://patentgrep.com/patent/US20100167527A1

## CPC

- H10W 20/045: {for deposition from the gaseous phase, e.g. for chemical vapour deposition [CVD]}
- C23C 16/02: Pretreatment of the material to be coated (C23C16/04 takes precedence)
- C23C 16/045: {Coating cavities or hollow spaces, e.g. interior of tubes; Infiltration of porous substrates}
- C23C 16/14: Deposition of only one other metal element
- C23C 16/45523: {Pulsed gas flow or change of composition over time}
- H10P 14/43: Chemical deposition, e.g. chemical vapour deposition [CVD]
- H10W 20/052: {by treatments not introducing additional elements therein}
- H10W 20/056: {by filling conductive material into holes, grooves or trenches}
- H10W: GENERIC PACKAGES, INTERCONNECTIONS, CONNECTORS OR OTHER CONSTRUCTIONAL DETAILS OF DEVICES COVERED BY CLASS H10
- C23C: COATING METALLIC MATERIAL; COATING MATERIAL WITH METALLIC MATERIAL; SURFACE TREATMENT OF METALLIC MATERIAL BY DIFFUSION INTO THE SURFACE, BY CHEMICAL CONVERSION OR SUBSTITUTION; COATING BY VACUUM EVAPORATION, BY SPUTTERING, BY ION IMPLANTATION OR BY CHEMICAL VAPOUR DEPOSITION, IN GENERAL (making metal-coated products by extrusion B21C23/22; covering with metal by connecting pre-existing layers to articles, see the relevant places, e.g. B21D39/00, B23K; metallising of glass C03C; metallising mortars, concrete, artificial stone, ceramics or natural stone C04B41/00; enamelling of, or applying a vitreous layer to, metals C23D; treating metal surfaces or coating of metals by electrolysis or electrophoresis C25D; single-crystal film growth C30B; by metallising textiles D06M11/83; decorating textiles by locally metallising D06Q1/04)
- H10P: GENERIC PROCESSES OR APPARATUS FOR THE MANUFACTURE OR TREATMENT OF DEVICES COVERED BY CLASS H10

## Abstract

A method of controlling the resistivity and morphology of a tungsten film is provided, comprising depositing a first film of a bulk tungsten layer on a substrate during a first deposition stage by (i) introducing a continuous flow of a reducing gas and a pulsed flow of a tungsten-containing compound to a process chamber to deposit tungsten on a surface of the substrate, (ii) flowing the reducing gas without flowing the tungsten-containing compound into the chamber to purge the chamber, and repeating steps (i) through (ii) until the first film fills vias in the substrate surface, increasing the pressure in the process chamber, and during a second deposition stage after the first deposition stage, depositing a second film of the bulk tungsten layer by providing a flow of reducing gas and tungsten-containing compound to the process chamber until a second desired thickness is deposited.

## Claims

### Claim 1

A method of controlling the resistivity and morphology of a tungsten film, comprising:
(a) positioning a substrate in a process chamber;
(b) during a first deposition stage, depositing a first film of a bulk tungsten layer by:
(i) introducing a continuous flow of a reducing gas and a pulsed flow of a tungsten-containing compound to the process chamber to deposit tungsten on a surface of the substrate,
(ii) flowing the reducing gas without flowing the tungsten-containing compound into the chamber to purge the chamber, and
(iii) repeating steps (i) through (ii) until the first film fills vias in the substrate surface;
(c) increasing the pressure in the process chamber; and
(d) during a second deposition stage after the first deposition stage, depositing a second film of the bulk tungsten layer by introducing a continuous flow of reducing gas and tungsten-containing compound to the process chamber until a second desired thickness is deposited.

### Claim 2 (depends on 1)

The method of claim 1, further comprising forming a nucleation layer on a surface of the substrate prior to step (b).

### Claim 3 (depends on 2)

The method of claim 2, further comprising forming a barrier layer on a surface of the substrate prior to forming the nucleation layer.

### Claim 4 (depends on 1)

The method of claim 1, further comprising flowing the reducing gas without flowing the tungsten-containing compound into the chamber during step (c).

### Claim 5 (depends on 1)

The method of claim 1, wherein a flow of a carrier gas is co-flowed with the reducing gas in steps (b)(i)-(b)(ii) and (d).

### Claim 6 (depends on 4)

The method of claim 4, wherein the carrier gas comprises argon.

### Claim 7 (depends on 1)

The method of claim 1, wherein the tungsten bulk layer is deposited by a chemical vapor deposition process.

### Claim 8 (depends on 1)

The method of claim 1, wherein the first deposition stage occurs at a pressure of 90 Torr and a temperature of 400° C. and the second deposition stage occurs at a pressure of 300 Torr and a temperature of 400° C.

### Claim 9 (depends on 1)

The method of claim 1, wherein the tungsten-containing compound comprises tungsten hexafluoride (WF6) and the reducing gas comprises hydrogen gas (H2).

### Claim 10 (depends on 1)

The method of claim 1, wherein the ratio of the flow of reducing gas to the tungsten-containing compound in step (b)(i) is between 25:1 and 50:1.

### Claim 11 (depends on 1)

The method of claim 1, wherein the ratio of the flow of reducing gas to the flow of tungsten-containing compound in step (b)(i) is 30:1.

### Claim 12

A method of controlling the resistivity and morphology of a tungsten film, comprising:
(a) positioning a substrate in a process chamber;
(b) during a first deposition stage, depositing a first film of a bulk tungsten layer by:
(i) introducing a continuous flow of a reducing gas and a pulsed flow of a tungsten-containing compound to the process chamber to deposit tungsten on a surface of the substrate,
(ii) flowing the reducing gas without flowing the tungsten-containing compound into the chamber to purge the chamber, and
(iii) repeating steps (i) through (ii) until the first film fills vias in the substrate surface;
(c) increasing the pressure in the process chamber; and
(d) during a second deposition stage after the first deposition stage, depositing a second film of the bulk tungsten layer by introducing a continuous flow of reducing gas and tungsten-containing compound to the process chamber at a lower ratio of reducing gas to tungsten-containing compound than in the first deposition stage until a second desired thickness is deposited.

### Claim 13 (depends on 12)

The method of claim 12, further comprising forming a nucleation layer on a surface of the substrate prior to step (b).

### Claim 14 (depends on 12)

The method of claim 12, further comprising forming a barrier layer on a surface of the substrate prior to forming the nucleation layer.

### Claim 15 (depends on 12)

The method of claim 12, wherein a flow of a carrier gas is co-flowed with the reducing gas in steps (b)(i)-(b)(ii) and (d).

### Claim 16 (depends on 15)

The method of claim 15, wherein the carrier gas comprises argon.

### Claim 17 (depends on 12)

The method of claim 12, further comprising exposing the substrate to a reducing gas during a soak process after forming the nucleation layer.

### Claim 18 (depends on 12)

The method of claim 12, wherein the first deposition stage occurs at a pressure of 90 Torr and a temperature of 400° C. and the second deposition stage occurs at a pressure of 300 Torr and a temperature of 400° C.

### Claim 19 (depends on 12)

The method of claim 12, wherein the ratio of the flow of reducing gas to the flow of tungsten-containing compound in the first deposition stage in step (b)(i) is between 25:1 and 50:1.

### Claim 20 (depends on 12)

The method of claim 12, wherein the ratio of the flow of reducing gas to the flow of tungsten-containing compound in the first deposition stage in step (b)(i) is 30:1.

### Claim 21 (depends on 12)

The method of claim 12, wherein the tungsten-containing compound comprises tungsten hexafluoride (WF6) and the reducing gas comprises hydrogen gas (H2).

### Claim 22 (depends on 14)

The method of claim 14, wherein the tungsten bulk layer is deposited by a chemical vapor deposition process.

### Claim 23

A method of controlling the resistivity and morphology of a tungsten film, comprising:
(a) positioning a substrate in a process chamber;
(b) introducing a continuous flow of a reducing gas and a pulsed flow of a tungsten-containing compound to the process chamber to deposit tungsten on a surface of the substrate, wherein the ratio of the flow of reducing gas to the flow of tungsten-containing compound is between 25:1 and 50:1;
(c) flowing the reducing gas without flowing the tungsten-containing compound into the chamber to purge the chamber; and
(d) repeating steps (b) through (c) until a tungsten bulk layer of desired thickness is deposited.