# US 2010/0167514 A1 · Post metal gate vt adjust etch clean

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2010/0167514 A1
- Document ID: US20100167514A1
- Status: Published application
- Kind: A1
- Application number: 12/344,422
- Filed: 2008-12-26
- Published: 2010-07-01
- Earliest claimed: 2008-12-26
- Assignees: Texas Instruments Incorporated
- Inventors: BRIAN K. KIRKPATRICK; JINHAN CHOI; RANDALL W. PAK
- Web page: https://patentgrep.com/patent/US20100167514A1

## CPC

- H10P 70/273: {the processing being a delineation of conductive layers, e.g. by RIE}
- H10D 84/0181: {Manufacturing their gate insulating layers}
- H10D 84/038: {using silicon technology, e.g. SiGe}
- H10P 50/287: {by chemical means}
- H10D 64/01316: {the conductor comprising a layer of elemental metal contacting the insulator, e.g. Ta, W, Mo or Al}
- H10D 64/0132: {the conductor being a metallic silicide}
- Y10S 438/906: Cleaning of wafer as interim step
- H10P: GENERIC PROCESSES OR APPARATUS FOR THE MANUFACTURE OR TREATMENT OF DEVICES COVERED BY CLASS H10
- H10D: INORGANIC ELECTRIC SEMICONDUCTOR DEVICES
- Y10S: TECHNICAL SUBJECTS COVERED BY FORMER USPC CROSS-REFERENCE ART COLLECTIONS [XRACs] AND DIGESTS

## Abstract

A method for fabricating a CMOS integrated circuit (IC) includes providing a substrate having a semiconductor surface, wherein the semiconductor surface has PMOS regions for PMOS devices and NMOS regions for NMOS devices. A gate dielectric layer is formed on the semiconductor surface followed by forming at least a first metal including layer on the gate dielectric layer. A polysilicon or amorphous silicon layer is formed on the first metal including layer to form an intermediate gate electrode stack. A masking pattern is formed on the intermediate gate electrode stack. The polysilicon or amorphous silicon layer is dry etched using the masking pattern to define a patterned intermediate gate electrode stack over the NMOS or PMOS regions, wherein the dry etching stops on a portion of the first metal comprising layer. The masking pattern is removed using a first post etch clean for stripping the masking pattern. A multi-step solution cleaning sequence is used after the removing step and includes a first wet clean including sulfuric acid and a fluoride, and a second wet clean after the first wet clean including a fluoride. Fabrication of the IC is then completed.

## Claims

### Claim 1

A method for fabricating a CMOS integrated circuit (IC), comprising:
providing a substrate having a semiconductor surface, wherein the semiconductor surface has PMOS regions for PMOS devices and NMOS regions for NMOS devices;
forming a gate dielectric layer on said semiconductor surface;
forming at least a first metal comprising layer on said gate dielectric layer;
forming a polysilicon or amorphous silicon layer on said first metal comprising layer to form an intermediate gate electrode stack;
forming a masking pattern on said intermediate gate electrode stack;
dry etching said polysilicon or amorphous silicon layer using said masking pattern to define a patterned intermediate gate electrode stack over said NMOS or said PMOS regions, wherein said dry etching stops on a portion of said first metal comprising layer;
removing said masking pattern using a first post etch clean for stripping said masking pattern, and
a multi-step solution cleaning sequence after said removing, comprising:
a first wet clean comprising sulfuric acid and a fluoride, and
a second wet clean after said first wet clean comprising a fluoride, and
completing fabrication of said IC.

### Claim 2 (depends on 1)

The method of claim 1, wherein said masking pattern comprises a photoresist pattern and said removing comprises an ashing process.

### Claim 3 (depends on 2)

The method of claim 2, wherein said ashing process comprises a reducing ash process.

### Claim 4 (depends on 1)

The method of claim 1, wherein said multi-step solution cleaning sequence further comprises a third wet clean after said second wet clean, said third wet clean comprising a hydroxide and a peroxide.

### Claim 5 (depends on 4)

The method of claim 4, wherein said hydroxide comprises ammonium hydroxide and said peroxide comprises hydrogen peroxide, a volume ratio of said ammonium hydroxide to said hydrogen peroxide being in a range from 1:2 to 2:1 and a volume ratio of said ammonium hydroxide combined with said hydrogen peroxide to deionized (DI) water being from 1:250 to 1:1,500.

### Claim 6 (depends on 5)

The method of claim 5, wherein a temperature for said third wet clean is in a range from 20 to 50° C.

### Claim 7 (depends on 1)

The method of claim 1, wherein said first wet clean is performed at a temperature of at least 40° C.

### Claim 8 (depends on 7)

The method of claim 7, wherein said temperature for said first wet clean is between 60 and 120° C.

### Claim 9 (depends on 1)

The method of claim 1, wherein said first metal comprising layer comprises a refractory metal.

### Claim 10 (depends on 9)

The method of claim 9, wherein said refractory metal comprises W.

### Claim 11 (depends on 1)

The method of claim 1, wherein said fluoride for said first wet clean and said fluoride for said second wet clean are independently selectable from the group consisting of hydrogen fluoride, ammonium fluoride, tetramethylammonium fluoride, ammonium hydrogen fluoride, fluorboric acid and tetramethylammonium tetrafluoroborate.

### Claim 12 (depends on 1)

The method of claim 1, further comprising a first DI water rinse between said first wet clean and said second wet clean and a second DI water rinse after said second wet clean, wherein said first DI water rinse and said second DI water rinse comprise megasonic agitation for at least a portion of their respective times.

### Claim 13 (depends on 1)

The method of claim 1, wherein said gate dielectric layer comprises a high-k dielectric material.

### Claim 14 (depends on 13)

The method of claim 13, wherein said high-k dielectric material comprises hafnium oxide, hafnium silicon oxide, hafnium silicon oxynitride, lanthanum oxide, zirconium oxide, zirconium oxide, zirconium silicon oxide, tantalum oxide, titanium oxide, barium strontium titanium oxide, barium titanium oxide, strontium titanium oxide, yttrium oxide, aluminum oxide, lead scandium tantalum oxide, or lead zinc niobate.

### Claim 15 (depends on 1)

The method of claim 1, wherein said fluoride in said first wet clean comprises HF and said first wet clean further comprises DI water, wherein a ratio of said sulfuric acid, DI water and said HF is A:B:1 wherein A is between 200 and 800, B is between 2 and 50.

### Claim 16 (depends on 1)

The method of claim 1, wherein said fluoride in said second wet clean comprises HF, wherein said second clean comprises said HF diluted from 50 to 150:1 with DI water, at a temperature of 20 to 30° C.

### Claim 17

A method for fabricating a CMOS integrated circuit (IC), comprising:
providing a substrate having a silicon comprising surface, wherein the silicon comprising surface has PMOS regions for PMOS devices and NMOS regions for NMOS devices;
forming a high-k gate dielectric layer on said silicon comprising surface;
forming at least one refractory metal comprising layer on said high-k gate dielectric layer;
forming a polysilicon or amorphous silicon layer on said refractory metal comprising layer to form an intermediate gate electrode stack;
forming a photoresist masking pattern on said intermediate gate electrode stack;
dry etching said polysilicon or amorphous silicon layer using said masking pattern to define a patterned intermediate gate electrode stack over said NMOS regions, wherein said dry etching stops on a portion of said refractory metal comprising layer;
a reducing ash process to remove said photoresist masking pattern,
a multi-step wet cleaning sequence after said removing, comprising:
a first wet clean consisting essentially of sulfuric acid and a fluoride at a temperature between 60 and 120 C;
a second wet clean after said first clean comprising a fluoride, and
a third wet clean after said second wet clean, said third wet clean comprising a hydroxide and a peroxide, wherein a volume ratio of said hydroxide to said peroxide is in a range from 1:2 to 2:1 and a volume ratio of said hydroxide combined with said peroxide to deionized (DI) water to is from 1:250 to 1:1,000, and
completing fabrication of said IC.

### Claim 18 (depends on 17)

The method of claim 17, wherein said completing fabrication of said IC comprises selectively forming a silicide from said patterned intermediate gate electrode stack over said NMOS regions.

### Claim 19 (depends on 17)

The method of claim 17, wherein said hydroxide comprises ammonium hydroxide and said peroxide comprises hydrogen peroxide.

### Claim 20 (depends on 17)

The method of claim 17, further comprising a DI water rinse after said third wet clean, wherein said DI water rinse comprises megasonic agitation.

### Claim 21 (depends on 17)

The method of claim 17, wherein said refractory metal comprises W.

### Claim 22

A multi-step wet cleaning sequence for cleaning a semiconductor wafer surface, comprising:
a first wet clean consisting essentially of sulfuric acid and a fluoride at a temperature between 60 and 120° C.;
a second wet clean after said first clean comprising a fluoride, and
a third wet clean after said second wet clean, said third wet clean comprising a hydroxide and a peroxide, wherein a volume ratio of said hydroxide to said peroxide is in a range from 1:2 to 2:1 and a volume ratio of said hydroxide combined with said peroxide to deionized (DI) water is from 1:250 to 1:1,000.