# US 2010/0167496 A1 · Method for forming device isolation layer of semiconductor device and non-volatile memory device

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2010/0167496 A1
- Document ID: US20100167496A1
- Status: Published application
- Kind: A1
- Application number: 12/473,307
- Filed: 2009-05-28
- Published: 2010-07-01
- Earliest claimed: 2008-12-26
- Assignees: Hynix Semiconductor Inc.
- Inventors: Jae-Hyoung Koo; Jin-Woong Kim; Mi-Ri Lee; Chi-Ho Kim; Jin-Ho Bin
- Web page: https://patentgrep.com/patent/US20100167496A1

## CPC

- H10W 10/17: formed using trench refilling with dielectric materials, e.g. shallow trench isolations
- H10B 41/30: characterised by the memory core region
- H10B 43/30: characterised by the memory core region
- H10W 10/0145: {of trenches having shapes other than rectangular or V-shape (H10W10/0143 takes precedence)}
- H10W: GENERIC PACKAGES, INTERCONNECTIONS, CONNECTORS OR OTHER CONSTRUCTIONAL DETAILS OF DEVICES COVERED BY CLASS H10
- H10B: ELECTRONIC MEMORY DEVICES

## Abstract

A method for forming a device isolation layer of a semiconductor device or a non-volatile memory device is provided. A method for forming a device isolation layer of a semiconductor device includes: forming trenches having a first predetermined depth by etching a substrate; forming a first insulation layer having a second predetermined depth inside the trenches; forming a liner oxide layer having a predetermined thickness on internal walls of the trenches with the first insulation layer formed therein; and forming a second insulation layer for forming a device isolation layer over the substrate with the liner oxide layer formed therein, wherein the second insulation layer has a lower etch rate than that of the first insulation layer.

## Claims

### Claim 1

A method for forming a device isolation layer of a semiconductor device, comprising:
forming trenches having a first depth by etching a substrate;
forming a first insulation layer having a second depth inside the trenches;
forming a liner oxide layer having a predetermined thickness on internal walls of the trenches with the first insulation layer; and
forming a second insulation layer over the substrate with the liner oxide layer to fill the trenches,
wherein the second insulation layer has a lower etch rate than that of the first insulation layer.

### Claim 2 (depends on 1)

The method of claim 1, wherein the forming of the first insulation layer includes:
forming a flowable oxide layer over the substrate with the trenches;
forming the first insulation layer by performing a thermal treatment;
planarizing the first insulation layer until a surface of the substrate is exposed; and
removing the first insulation layer while leaving the first insulation layer in the second depth inside the trenches.

### Claim 3 (depends on 1)

The method of claim 1, wherein the forming a liner oxide layer includes:
oxidizing internal walls of the trenches with the first insulation layer to form the liner oxide layer.

### Claim 4 (depends on 1)

The method of claim 1, wherein a surface of the first insulation layer is lower than a surface of the substrate.

### Claim 5 (depends on 1)

The method of claim 1, wherein the predetermined thickness of the liner oxide layer is a thickness ranging from approximately 20 Å to approximately 150 Å.

### Claim 6 (depends on 1)

The method of claim 1, wherein the first insulation layer includes an SOD layer formed of PSZ, and the second insulation layer includes formed of HDP oxide.

### Claim 7

A method for forming a device isolation layer of a non-volatile memory device, comprising:
forming a tunnel insulation layer, a charge storage layer, and a hard mask layer over a substrate;
forming trenches having a first depth by etching the hard mask layer, the charge storage layer, the tunnel insulation layer, and the substrate;
forming a first insulation layer having a second depth inside the trenches; and
forming a liner oxide layer having a predetermined thickness on internal walls of the trenches with the first insulation layer; and
forming a second insulation layer over the hard mask layer with the liner oxide layer,
wherein the second insulation layer has a lower etch rate than that of the first insulation layer.

### Claim 8 (depends on 7)

The method of claim 7, wherein the forming of the first insulation layer includes:
forming a flowable oxide layer over the hard mask layer with the trenches;
forming the first insulation layer by performing a thermal treatment;
planarizing the first insulation layer until a surface of the hard mask layer is exposed; and
removing the first insulation layer while leaving the first insulation layer in the second depth inside the trenches.

### Claim 9 (depends on 7)

The method of claim 7, wherein the forming of the liner oxide layer includes:
oxidizing internal walls of the trenches with the first insulation layer to form the liner oxide layer.

### Claim 10 (depends on 7)

The method of claim 7, wherein a surface of the first insulation layer is lower than a surface of the hard mask layer.

### Claim 11 (depends on 7)

The method of claim 7, wherein the predetermined thickness of the liner oxide layer is a thickness ranging from approximately 20 Å to approximately 150 Å.

### Claim 12 (depends on 7)

The method of claim 7, wherein the first insulation layer is an SOD layer formed of PSZ, and the second insulation layer is formed of HDP oxide.

### Claim 13 (depends on 7)

The method of claim 7, further comprising:
planarizing the second insulation layer until a surface of the hard mask layer is exposed after the forming of the second insulation layer; and
removing the hard mask layer.