# US 2010/0167493 A1 · Method of manufacturing semiconductor device

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2010/0167493 A1
- Document ID: US20100167493A1
- Status: Published application
- Kind: A1
- Application number: 12/548,471
- Filed: 2009-08-27
- Published: 2010-07-01
- Earliest claimed: 2008-12-25
- Assignees: NEC Electronics Corporation
- Inventors: Keiji SAKAMOTO; Takashi OGURA; Masashige MORITOKI
- Web page: https://patentgrep.com/patent/US20100167493A1

## CPC

- H10W 10/17: formed using trench refilling with dielectric materials, e.g. shallow trench isolations
- H10W 10/0145: {of trenches having shapes other than rectangular or V-shape (H10W10/0143 takes precedence)}
- H10W: GENERIC PACKAGES, INTERCONNECTIONS, CONNECTORS OR OTHER CONSTRUCTIONAL DETAILS OF DEVICES COVERED BY CLASS H10

## Abstract

A method of manufacturing a semiconductor device includes a process of forming a STI trench in a substrate, a process of forming a thermal oxide film on a sidewall and a bottom surface of the STI trench, a process of performing a plasma treatment on a surface of the thermal oxide film that is located at a bottom portion of the STI trench, and a process of forming an insulating film in the STI trench using a CVD method

## Claims

### Claim 1

A method of manufacturing a semiconductor device, comprising:
forming a shallow trench isolation (STI) trench in a substrate;
forming a thermal oxide film on a sidewall and a bottom surface of the STI trench;
performing a plasma treatment on the thermal oxide film that is located at a bottom portion of the STI trench; and
forming an insulating film in the STI trench using a chemical vapor deposition (CVD) method,
wherein, in the performing of the plasma treatment, an arrival density of active specifies that are generated by plasma is larger at the bottom portion than at the sidewall.

### Claim 2 (depends on 1)

The method according to claim 1, wherein, during the plasma treatment, power equal to or more than 0.1 W/cm2 and equal to or less than 10 W/cm2 per area of the substrate is applied to excite the plasma.

### Claim 3 (depends on 1)

The method according to claim 1, wherein, during the plasma treatment, bias power is applied to the substrate.

### Claim 4 (depends on 3)

The method according to claim 3, wherein the bias power equal to or more than 0.1 W/cm2 and equal to or less than 1.0 W/cm2 per area of the substrate is applied.

### Claim 5 (depends on 1)

The method according to claim 1, wherein, during the plasma treatment, gas that is selected from the group consisting of oxygen, argon, helium, and nitrogen is used as treatment gas.

### Claim 6 (depends on 1)

The method according to claim 1, wherein the plasma treatment is performed under a pressure that is equal to or higher than 40 Pa and equal to or lower than 134 Pa.

### Claim 7 (depends on 1)

The method according to claim 1, wherein the insulating film is formed using the CVD method using tetraethoxysilane.

### Claim 8 (depends on 1)

The method according to claim 1, wherein an opening width of the STI trench is equal to or less than 100 nm.