# US 2010/0167455 A1 · Method for fabrication of cmos image sensor

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2010/0167455 A1
- Document ID: US20100167455A1
- Status: Published application
- Kind: A1
- Application number: 12/642,049
- Filed: 2009-12-18
- Published: 2010-07-01
- Earliest claimed: 2008-12-29
- Inventors: Chung-Kyung Jung
- Web page: https://patentgrep.com/patent/US20100167455A1

## CPC

- H10P 50/73: {using masks for insulating materials}
- H10F 39/024: {of coatings or optical elements}
- H10F 39/805: {Coatings}
- H10P 76/204: {of organic photoresist masks}
- H10P: GENERIC PROCESSES OR APPARATUS FOR THE MANUFACTURE OR TREATMENT OF DEVICES COVERED BY CLASS H10
- H10F: INORGANIC SEMICONDUCTOR DEVICES SENSITIVE TO INFRARED RADIATION, LIGHT, ELECTROMAGNETIC RADIATION OF SHORTER WAVELENGTH OR CORPUSCULAR RADIATION

## Abstract

Disclosed is a method for fabrication of a CMOS image sensor capable of improving adhesion between an interlayer insulating film and photoresist. According to embodiments in this disclosure, the CMOS image sensor fabrication method may include: forming a plurality of photodiodes over a semiconductor substrate at regular intervals; forming an interlayer insulating film over the semiconductor substrate including the plurality of photodiodes; applying photoresist over the entirety of the interlayer insulating film; hard-baking the photoresist; conducting exposure and development of the photoresist to expose a part of the interlayer insulating film corresponding to the photodiodes, thereby completing a photoresist pattern; and using the photoresist pattern as a mask to selectively etch the exposed part of the interlayer insulating film.

## Claims

### Claim 1

A method comprising:
forming a plurality of photodiodes over a semiconductor substrate at regular intervals;
forming an interlayer insulating film over the semiconductor substrate including the plurality of photodiodes;
applying photoresist over the entirety of the interlayer insulating film;
hard-baking the photoresist;
conducting exposure and development of the photoresist to expose a part of the interlayer insulating film corresponding to the photodiodes, thereby completing a photoresist pattern; and
using the photoresist pattern as a mask to selectively etch the exposed part of the interlayer insulating film.

### Claim 2 (depends on 1)

The method of claim 1, wherein the hard-baking is conducted at approximately 100° C. to 200° C.

### Claim 3 (depends on 1)

The method of claim 1, wherein the photoresist is a negative photoresist.

### Claim 4 (depends on 1)

The method of claim 1, wherein the selective etching process using the photoresist pattern as a mask to remove the exposed portion of the interlayer insulating film comprises a wet etching process using BHF.

### Claim 5 (depends on 1)

The method of claim 1, wherein the selective etching process using the photoresist pattern as a mask to remove the exposed portion of the interlayer insulating film comprises a wet etching process using DHF.

### Claim 6 (depends on 5)

The method of claim 5, wherein the DHF contains H2O and HF in a relative ratio of H2O:HF of between approximately 1:1 and 5:1.

### Claim 7 (depends on 1)

The method of claim 1, including placing a plurality of color filter layers over the interlayer insulating film at constant intervals corresponding to the plural photodiodes.

### Claim 8 (depends on 7)

The method of claim 7, including forming a micro-lens pattern over the color filter layer.

### Claim 9 (depends on 1)

The method of claim 1, wherein the selective etching process using the photoresist pattern as a mask to remove the exposed portion of the interlayer insulating film includes formation of a trench hole over the exposed interlayer insulating film portion.

### Claim 10 (depends on 9)

The method of claim 9, wherein a depth of the formed trench hole ranges from 0.5 to 1.5 μm.

### Claim 11

An apparatus configured to:
form a plurality of photodiodes over a semiconductor substrate at regular intervals;
form an interlayer insulating film over the semiconductor substrate including the plurality of photodiodes;
apply photoresist over the entirety of the interlayer insulating film;
hard-bake the photoresist;
conduct exposure and development of the photoresist to expose a part of the interlayer insulating film corresponding to the photodiodes, thereby completing a photoresist pattern; and
use the photoresist pattern as a mask to selectively etch the exposed part of the interlayer insulating film.

### Claim 12 (depends on 11)

The method of claim 11, configured to conduct the hard-baking at approximately 100° C. to 200° C.

### Claim 13 (depends on 11)

The method of claim 11, configured to apply a negative photoresist.

### Claim 14 (depends on 11)

The method of claim 11, configured to use a wet selective etching process using the photoresist pattern as a mask to remove the exposed portion of the interlayer insulating film using BHF.

### Claim 15 (depends on 11)

The method of claim 11, configured to use a wet selective etching process using the photoresist pattern as a mask to remove the exposed portion of the interlayer insulating film using DHF.

### Claim 16 (depends on 15)

The method of claim 15, configured with DHF which contains H2O and HF in a relative ratio of H2O:HF of between approximately 1:1 and 5:1.

### Claim 17 (depends on 11)

The method of claim 11, configured to place a plurality of color filter layers over the interlayer insulating film at constant intervals corresponding to the plural photodiodes.

### Claim 18 (depends on 17)

The method of claim 17, configured to form a micro-lens pattern over the color filter layer.

### Claim 19 (depends on 11)

The method of claim 11, configured to form a trench hole over the exposed interlayer insulating film portion in the selective etching process using the photoresist pattern as a mask to remove the exposed portion of the interlayer insulating film.

### Claim 20 (depends on 19)

The method of claim 19, configured to form a trench hole with a depth which ranges from 0.5 to 1.5 μm.