# US 2010/0167446 A1 · Method for Manufacturing a Junction

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2010/0167446 A1
- Document ID: US20100167446A1
- Status: Published application
- Kind: A1
- Application number: 12/647,773
- Filed: 2009-12-28
- Published: 2010-07-01
- Earliest claimed: 2008-12-29
- Assignees: Imec
- Inventors: Ngoc Duy Nguyen; Roger Loo; Matty Caymax
- Web page: https://patentgrep.com/patent/US20100167446A1

## CPC

- H10P 14/3411: {Silicon, silicon germanium or germanium}
- H10D 10/021: {of heterojunction BJTs [HBT]}
- H10D 62/822: comprising only Group IV materials heterojunctions, e.g. Si/Ge heterojunctions
- H10P 14/3441: {Conductivity type}
- H10P: GENERIC PROCESSES OR APPARATUS FOR THE MANUFACTURE OR TREATMENT OF DEVICES COVERED BY CLASS H10
- H10D: INORGANIC ELECTRIC SEMICONDUCTOR DEVICES

## Abstract

The present invention relates to a semiconductor device comprising a homojunction or a heterojunction with a controlled dopant (concentration) profile and a method of making the same. Accordingly, one aspect of the invention is a method for manufacturing a junction comprising forming a first semiconductor material comprising a first dopant having a first concentration and thereupon; forming a second semiconductor material comprising a second dopant, having a second concentration thereby forming a junction, and depositing by Atomic Layer Epitaxy or Vapor Phase Doping at least a fraction of a monolayer of a precursor suitable to form the second dopant on the first semiconductor material, prior to forming the second semiconductor material, thereby increasing the second concentration of the second dopant at the junction.

## Claims

### Claim 1

A method for manufacturing a junction with a controlled dopant profile comprising:
forming a first semiconductor material comprising a first dopant having a first concentration and thereupon
forming a second semiconductor material comprising a second dopant, having a second concentration thereby forming a junction, and
depositing by Atomic Layer Epitaxy or Vapor Phase Doping at least a fraction of a monolayer of a precursor suitable to form the second dopant on the first semiconductor material, prior to forming the second semiconductor material, thereby increasing the second concentration of the second dopant at the junction.

### Claim 2 (depends on 1)

The method according to claim 1, wherein the first semiconductor material and the second semiconductor material have the same composition, thereby forming a homojunction.

### Claim 3 (depends on 1)

The method according to claim 1, wherein the first semiconductor material and the second semiconductor material have different compositions, thereby forming a heterojunction.

### Claim 4 (depends on 1)

The method according to claim 1, wherein forming the second semiconductor material comprises
performing a sequence consisting of
epitaxially growing a layer of a second semiconductor material and thereupon
depositing by Atomic Layer Epitaxy a monolayer of a precursor suitable to form the second dopant, and
repeating the sequence at least twice, thereby incorporating the second dopant in substitutional sites in the second semiconductor material.

### Claim 5 (depends on 1)

The method according to claim 1, wherein the second concentration of the second dopant in the second semiconductor material is higher or equal to 1×1020 atoms/cm3.

### Claim 6 (depends on 1)

The method according to any of claims 1, wherein the second dopant is a n-type dopant.

### Claim 7 (depends on 6)

The method according to claim 6, wherein the n-type dopant is arsenic (As) or phosphorus (P).

### Claim 8 (depends on 7)

The method according to claim 7, wherein the precursors suitable to form the n-type dopant are arsine (AsH3) or phosphine (PH3).

### Claim 9 (depends on 1)

The method according to claim 1, wherein the first dopant is a p-type dopant.

### Claim 10 (depends on 9)

The method according to claim 9, wherein the p-type dopant is boron.

### Claim 11 (depends on 1)

The method according to claim 1, wherein the second semiconductor material comprises Si, Ge or combinations thereof.

### Claim 12 (depends on 1)

The method according to claim 1, wherein the second semiconductor material is an emitter region of a bipolar transistor.

### Claim 13 (depends on 1)

The method according to claim 1, wherein the first semiconductor material comprises Si, Ge or combinations thereof.

### Claim 14 (depends on 1)

The method according to claim 1, wherein the first semiconductor material is a base region of a bipolar transistor.

### Claim 15 (depends on 1)

The method according to claim 1, further comprising a rapid thermal treatment.

### Claim 16 (depends on 15)

The method according to claim 15, wherein the rapid thermal treatment is a typical HDD activation anneal used in CMOS technology.

### Claim 17 (depends on 15)

The method according to claim 15, wherein upon the rapid thermal treatment an in-diffusion depth of As into the first semiconductor material is lower or equal to 15 nm.

### Claim 18 (depends on 1)

Use of the method according to claim 1 for the manufacture of a bipolar CMOS (BiCMOS) device.

### Claim 19 (depends on 1)

Use of the method according to claim 1 for the manufacture of a photovoltaic device.