# US 2010/0167444 A1 · Fabrication method for thermoelectric device

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2010/0167444 A1
- Document ID: US20100167444A1
- Status: Published application
- Kind: A1
- Application number: 12/644,712
- Filed: 2009-12-22
- Published: 2010-07-01
- Earliest claimed: 2008-12-26
- Assignees: Corning Incorporated; Shanghai Institute of Ceramics
- Inventors: Lidong Chen; Monika Backhaus-Ricoult; Lin He; Xiaoya Li; Xugui Xia; Degang Zhao
- Web page: https://patentgrep.com/patent/US20100167444A1

## CPC

- H10N 10/17: characterised by the structure or configuration of the cell or thermocouple forming the device
- H10N 10/01: Manufacture or treatment
- H10N: ELECTRIC SOLID-STATE DEVICES NOT OTHERWISE PROVIDED FOR

## Abstract

A method for fabricating thermoelectric device is provided. The method comprises placing a first electrode in a die, forming a first interlayer on an upper surface of the first electrode; positioning a separating plate on an upper surface of the first interlayer to divide an inner space of the die into a plurality of cells, and depositing a first thermoelectric material on the first interlayer within a first fraction of the cells, and depositing a second thermoelectric material on the first interlayer within a second fraction of the cells, sintering the die contents, and removing the separating plate after sintering to obtain a π shaped thermoelectric device.

## Claims

### Claim 1

A method for fabricating a thermoelectric device, comprising:
placing a first electrode in a die;
forming a first interlayer on an upper surface of the first electrode;
positioning a separating plate on an upper surface of the first interlayer to divide an inner space of the die into a plurality of cells, and depositing a first thermoelectric material on the first interlayer within a first fraction of the cells, and depositing a second thermoelectric material on the first interlayer within a second fraction of the cells;
sintering the die contents; and
removing the separating plate after sintering to obtain a π shaped thermoelectric device.

### Claim 2 (depends on 1)

The method of claim 1, wherein after the π shaped thermoelectric device is obtained, welding a plurality of π shaped thermoelectric devices to a copper-coated ceramic plate to form an entire body.

### Claim 3 (depends on 2)

The method of claim 2, wherein the step of welding a plurality of π shaped thermoelectric devices to the copper-coated ceramic plate further comprises providing a second interlayer and a tin soldering layer sequentially on one side of the plurality of π shaped thermoelectric devices, which are then welded with the copper-coated ceramic plate.

### Claim 4 (depends on 1)

The method of claim 1, wherein the first interlayer comprises:
a joint enhancement layer in contact with the first electrode; and
a barrier layer in contact with the joint enhancement layer.

### Claim 5 (depends on 1)

The method of claim 1, wherein the step of sintering comprises:
sintering the die contents with electricity in a spark plasma apparatus.

### Claim 6 (depends on 1)

The method of claim 1, wherein the step of sintering is performed under a pressure of 30-60 MPa and a sintering temperature of 550-680° C.

### Claim 7 (depends on 1)

The method of claim 1, wherein the separating plate comprises one or more of ZrO2, Al2O3, AlN, SiO2, glass, graphite, Ni, Cu, Fe, and stainless steel.

### Claim 8 (depends on 1)

The method of claim 1, wherein the first electrode comprises binary or ternary alloys or composite material that include a first metal selected from Cu, Ag, Al or Au, and a second metal selected from Mo, W, Zr, Ta, Cr, Nb, V or Ti.

### Claim 9 (depends on 1)

The method of claim 1, wherein the first electrode comprises metal alloys or composite material selected from molybdenum-copper alloys with a general formula MoxCu1-x, in which x (weight %) is 20≦x≦80, or tungsten-copper alloys with a general formula WxCu1-x, in which x (weight %) is 50≦x≦90.

### Claim 10 (depends on 1)

The method of claim 1, wherein the first thermoelectric material comprises n-type thermoelectric material selected from n-CoSb3, n-PbTe and n-Zn4Sb3, and the second thermoelectric material comprises p-type thermoelectric material selected from p-CoSb3, p-PbTe and p-Zn4Sb3.

### Claim 11 (depends on 1)

The method of claim 1, wherein ((characterized in that, between step (c-1) and step (d-1), further comprising steps of:
forming a second interlayer on the first thermoelectric material and the second thermoelectric material;
forming a second electrode on the second interlayer.

### Claim 12 (depends on 11)

The method of claim 11, wherein the second electrode comprises metal alloys or composite material selected from molybdenum-copper alloys with a general formula MoxCu1-x, in which x (weight %) is 20≦x≦80, or tungsten-copper alloys with a general formula WxCu1-x, in which x (weight %) is 50≦x≦90.

### Claim 13 (depends on 11)

The method of claim 11, wherein the step of forming the first layer or the step of forming the second layer is performed by plasma spraying, flame spraying, arc spraying or electroplating.

### Claim 14 (depends on 11)

The method of claim 11, wherein after the m shaped thermoelectric device is obtained, welding a plurality of π shaped thermoelectric devices to a copper-coated ceramic plate to form an entire body.

### Claim 15 (depends on 11)

The method of claim 11, wherein coefficients of thermal expansion of the first electrode and the second electrode are substantially equal to those of the first thermoelectric material and second thermoelectric material.