# US 2010/0167425 A1 · Method of producing bonded silicon wafer

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2010/0167425 A1
- Document ID: US20100167425A1
- Status: Published application
- Kind: A1
- Application number: 12/644,312
- Filed: 2009-12-22
- Published: 2010-07-01
- Earliest claimed: 2008-12-25
- Assignees: Sumco Corporation
- Inventors: Takashi Sakai
- Web page: https://patentgrep.com/patent/US20100167425A1

## CPC

- H10P 74/203: {Structural properties, e.g. testing or measuring thicknesses, line widths, warpage, bond strengths or physical defects}
- H10P 74/238: {comprising acting in response to an ongoing measurement without interruption of processing, e.g. endpoint detection or in-situ thickness measurement}
- H10P 90/1908: {using silicon implanted buried insulating layers, e.g. oxide layers [SIMOX]}
- H10W 10/181: {Semiconductor-on-insulator [SOI] isolation regions, e.g. buried oxide regions of SOI wafers}
- H10P: GENERIC PROCESSES OR APPARATUS FOR THE MANUFACTURE OR TREATMENT OF DEVICES COVERED BY CLASS H10
- H10W: GENERIC PACKAGES, INTERCONNECTIONS, CONNECTORS OR OTHER CONSTRUCTIONAL DETAILS OF DEVICES COVERED BY CLASS H10

## Abstract

A bonded silicon wafer is produced by a method comprising a step of implanting oxygen ions from one surface of a silicon wafer for active layer to form an oxygen ion implanted layer, a step of bonding the one surface of the silicon wafer for active layer to one surface of a silicon wafer for support layer and then conducting a heat treatment for strengthening the bonding to form a silicon wafer composite, a step of polishing a silicon portion at a side of the silicon wafer for active layer in the silicon wafer composite on a rotating platen having a polishing means and stopping the polishing at a time of detecting change of physical properties on the rotating platen resulting from the exposure of at least a part of the oxygen ion implanted layer and a step of removing the oxygen ion implanted layer.

## Claims

### Claim 1

A method of producing a bonded silicon wafer comprising:
a step of implanting oxygen ions from one surface of a silicon wafer for active layer to form an oxygen ion implanted layer at a given depth area from the one surface of the silicon wafer for active layer;
a step of bonding the one surface of the silicon wafer for active layer to one surface of a silicon wafer for support layer with or without an insulating layer and then conducting a heat treatment for strengthening the bonding to form a silicon wafer composite;
a step of polishing a silicon portion at a side of the silicon wafer for active layer in the silicon wafer composite on a rotating platen having a polishing means and stopping the polishing at a time of detecting change of physical properties on the rotating platen resulting from the exposure of at least a part of the oxygen ion implanted layer; and
a step of removing the oxygen ion implanted layer.

### Claim 2 (depends on 1)

The method according to claim 1, wherein the change of physical properties is a change of friction resistance produced between the polishing means and a polished surface of the silicon wafer composite.

### Claim 3 (depends on 2)

The method according to claim 2, wherein the friction resistance is measured by a rotation torque applied to the rotating platen.

### Claim 4 (depends on 1)

The method according to claim 1, wherein the silicon wafer composite is polished by making rotation number of the rotating platen different before and after the polishing stop.

### Claim 5 (depends on 1)

The method according to claim 1, wherein the polishing means comprises a polishing cloth substantially containing no abrasives and a polishing solution containing abrasives.

### Claim 6 (depends on 1)

The method according to claim 1, wherein the polishing means comprises a polishing cloth fixed with given abrasives and a polishing solution substantially containing no abrasives.

### Claim 7 (depends on 5)

The method according to claim 5, wherein the polishing solution is a solution containing abrasives and has a different abrasive concentration before and after the polishing stop for polishing the silicon wafer composite.

### Claim 8 (depends on 1)

The method according to claim 1, wherein an amount of the silicon wafer composite polished is 0.1 to 50 μm in total before and after the polishing stop.

### Claim 9 (depends on 5, 6)

The method according to claim 5 or 6, wherein the polishing cloth is a urethane or a urethane-containing nonwoven cloth, and the polishing solution is a caustic solution.

### Claim 10 (depends on 1)

The method according to claim 1, wherein the bonded silicon wafer is composed of a silicon single crystal or of a silicon single crystal and a silicon oxide.