# US 2010/0167213 A1 · Semiconductor device manufacturing method

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2010/0167213 A1
- Document ID: US20100167213A1
- Status: Published application
- Kind: A1
- Application number: 12/621,146
- Filed: 2009-11-18
- Published: 2010-07-01
- Earliest claimed: 2008-12-26
- Inventors: Yuriko SEINO; Tatsuhiko EMA
- Web page: https://patentgrep.com/patent/US20100167213A1

## CPC

- G03F 7/091: {characterised by antireflection means or light filtering or absorbing means, e.g. anti-halation, contrast enhancement}
- G03F 7/095: having more than one photosensitive layer (G03F7/075 takes precedence)
- H10P 76/2043: {using an anti-reflective coating}
- G03F: PHOTOMECHANICAL PRODUCTION OF TEXTURED OR PATTERNED SURFACES, e.g. FOR PRINTING, FOR PROCESSING OF SEMICONDUCTOR DEVICES; MATERIALS THEREFOR; ORIGINALS THEREFOR; APPARATUS SPECIALLY ADAPTED THEREFOR; (phototypographic composing devices B41B; photosensitive materials or processes for photographic purposes G03C; electrophotography, sensitive layers or processes therefor G03G)
- H10P: GENERIC PROCESSES OR APPARATUS FOR THE MANUFACTURE OR TREATMENT OF DEVICES COVERED BY CLASS H10

## Abstract

A semiconductor device manufacturing method includes: forming a first anti-reflective coating on a semiconductor wafer; forming a second anti-reflective coating on the first anti-reflective coating; forming a resist film on the second anti-reflective coating; selectively exposing the resist film to light; developing the resist film and the anti-reflective coatings after the light exposure; and processing the semiconductor wafer using as a mask a pattern of the resist film obtained by the development. The photosensitizer concentration of the first anti-reflective coating is higher than the photosensitizer concentration of the second anti-reflective coating.

## Claims

### Claim 1

A semiconductor device manufacturing method comprising:
forming an anti-reflective coating on a semiconductor wafer, the anti-reflective coating having varied photosensitizer concentration along its thickness;
forming a resist film on the anti-reflective coating;
selectively exposing the resist film to light;
developing the resist film and the anti-reflective coating after the light exposure; and
processing the semiconductor wafer using as a mask a pattern of the resist film obtained by the development.

### Claim 2 (depends on 1)

The method according to claim 1, wherein the anti-reflective coating has a heterogeneous multilayer structure.

### Claim 3 (depends on 1)

The method according to claim 1, wherein the photosensitizer concentration in the anti-reflective coating is lower in a portion in contact with the semiconductor wafer than in a portion in contact with the resist film.

### Claim 4 (depends on 3)

The method according to claim 3, wherein the forming the anti-reflective coating includes:
forming, on the semiconductor wafer, a first anti-reflective coating whose light-exposed portion and non-light-exposed portion are both soluble in a developer during the development; and
forming, on the first anti-reflective coating, a second anti-reflective coating whose light-exposed portion or non-light-exposed portion is soluble in the developer.

### Claim 5 (depends on 4)

The method according to claim 4, wherein in the second anti-reflective coating, the light-exposed portion is soluble in the developer.

### Claim 6 (depends on 4)

The method according to claim 4, wherein the second anti-reflective coating is thicker than the first anti-reflective coating.

### Claim 7 (depends on 3)

The method according to claim 3, wherein
the forming the anti-reflective coating includes supplying onto the semiconductor wafer a solution in which a photosensitive polymer and a non-photosensitive polymer are mixed, and
the photosensitive polymer is contained in an upper portion of the anti-reflective coating in a relatively high proportion, and the non-photosensitive polymer is contained in a lower portion of the anti-reflective coating in a relatively high proportion.

### Claim 8 (depends on 3)

The method according to claim 3, wherein in the forming the anti-reflective coating, a concentration gradient of the photosensitizer is produced along the thickness of the anti-reflective coating.

### Claim 9 (depends on 1)

The method according to claim 1, wherein in the anti-reflective coating, the photosensitizer concentration is higher in a portion in contact with the semiconductor wafer than in a portion in contact with the resist film.

### Claim 10 (depends on 9)

The method according to claim 9, wherein the forming the anti-reflective coating includes:
forming, on the semiconductor wafer, a first anti-reflective coating whose light-exposed portion or non-light-exposed portion is soluble in a developer during the development; and
forming, on the first anti-reflective coating, a second anti-reflective coating whose light-exposed portion and non-light-exposed portion are both soluble in the developer.

### Claim 11 (depends on 10)

The method according to claim 10, wherein in the first anti-reflective coating, the light-exposed portion is soluble in the developer.

### Claim 12 (depends on 10)

The method according to claim 10, wherein the first anti-reflective coating is thicker than the second anti-reflective coating.

### Claim 13 (depends on 9)

The method according to claim 9, wherein in the forming the anti-reflective coating, a concentration gradient of the photosensitizer is produced along the thickness of the anti-reflective coating.

### Claim 14 (depends on 9)

The method according to claim 9, wherein
the forming the anti-reflective coating includes supplying onto the semiconductor wafer a solution in which a photosensitive polymer and a non-photosensitive polymer are mixed, and
the photosensitive polymer is contained in a lower portion of the anti-reflective coating in a relatively high proportion, and the non-photosensitive polymer is contained in an upper portion of the anti-reflective coating in a relatively high proportion.

### Claim 15 (depends on 1)

The method according to claim 1, wherein the photosensitizer concentration in the anti-reflective coating is lower in a portion in contact with the semiconductor wafer and a portion in contact with the resist film than in an intermediate portion between these portions.

### Claim 16 (depends on 15)

The method according to claim 15, wherein the forming the anti-reflective coating includes:
forming, on the semiconductor wafer, a first anti-reflective coating whose light-exposed portion and non-light-exposed portion are both soluble in a developer during the development;
forming, on the first anti-reflective coating, a second anti-reflective coating whose light-exposed portion or non-light-exposed portion is soluble in the developer; and
forming, on the second anti-reflective coating, a third anti-reflective coating whose light-exposed portion and non-light-exposed portion are both soluble in a developer.

### Claim 17 (depends on 16)

The method according to claim 16, wherein in the second anti-reflective coating, the light-exposed portion is soluble in the developer.

### Claim 18 (depends on 16)

The method according to claim 16, wherein the second anti-reflective coating is thicker than the first anti-reflective coating and the third anti-reflective coating.

### Claim 19 (depends on 1)

The method according to claim 1, wherein in the anti-reflective coating, a portion with the photosensitizer concentration being low has a smaller thickness than a portion with the photosensitizer concentration being high.

### Claim 20 (depends on 1)

The method according to claim 1, wherein the photosensitizer is a photoacid generator that generates acid by an exposure light.