# US 2010/0167206 A1 · Photoresist composition and method for manufacturing a display substrate using the photoresist composition

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2010/0167206 A1
- Document ID: US20100167206A1
- Status: Published application
- Kind: A1
- Application number: 12/557,215
- Filed: 2009-09-10
- Published: 2010-07-01
- Earliest claimed: 2008-12-29
- Assignees: Samsung Electronics Co., Ltd.; AZ Electronic Materials (Japan) K.K.
- Inventors: Woo-Seok JEON; Sang-Hyun YUN; Hi-Kuk LEE; Deok-Man KANG; Sae-Tae OH
- Web page: https://patentgrep.com/patent/US20100167206A1

## CPC

- G02F 1/13439: {characterised by their electrical, optical, physical properties; materials therefor; method of making}
- G03F 7/0007: {Filters, e.g. additive colour filters; Components for display devices}
- G03F 7/0226: {characterised by the non-macromolecular additives}
- H10D 86/0231: {using masks, e.g. half-tone masks}
- G02F: OPTICAL DEVICES OR ARRANGEMENTS FOR THE CONTROL OF LIGHT BY MODIFICATION OF THE OPTICAL PROPERTIES OF THE MEDIA OF THE ELEMENTS INVOLVED THEREIN; NON-LINEAR OPTICS; FREQUENCY-CHANGING OF LIGHT; OPTICAL LOGIC ELEMENTS; OPTICAL ANALOGUE/DIGITAL CONVERTERS
- G03F: PHOTOMECHANICAL PRODUCTION OF TEXTURED OR PATTERNED SURFACES, e.g. FOR PRINTING, FOR PROCESSING OF SEMICONDUCTOR DEVICES; MATERIALS THEREFOR; ORIGINALS THEREFOR; APPARATUS SPECIALLY ADAPTED THEREFOR; (phototypographic composing devices B41B; photosensitive materials or processes for photographic purposes G03C; electrophotography, sensitive layers or processes therefor G03G)
- H10D: INORGANIC ELECTRIC SEMICONDUCTOR DEVICES

## Abstract

A photoresist composition includes a novolac resin, a benzophenone photosensitizer and an ethylidyne tris phenol photosensitizer, and an organic solvent. Thus, a micropattern having a higher resolution than the resolution of an exposure apparatus is formed to decrease an amount of exposure and/or exposure time, thereby improving manufacturing reliability and productivity.

## Claims

### Claim 1

A photoresist composition, comprising:
a novolac resin;
a benzophenone photosensitizer and an ethylidyne tris phenol photosensitizer in a weight ratio of the benzophenone photosensitizer to the ethylidyne tris phenol photosensitizer in a range from about 20:80 to about 80:20 based on a total weight of the benzophenone photosensitizer and the ethylidyne tris phenol photosensitizer; and
an organic solvent.

### Claim 2 (depends on 1)

The photoresist composition of claim 1, wherein the benzophenone photosensitizer comprises a resultant of a benzophenone compound and a quinone diazide compound reaction.

### Claim 3 (depends on 1)

The photoresist composition of claim 1, wherein the benzophenone photosensitizer comprises a resultant of 2,3,4,4′-tetrahydroxybenzophenone and a quinone diazide compound reaction.

### Claim 4 (depends on 1)

The photoresist composition of claim 1, wherein the ethylidyne tris phenol photosensitizer comprises a resultant of an ethylidyne tris phenol compound and a quinone diazide compound reaction.

### Claim 5 (depends on 1)

The photoresist composition of claim 1, wherein the ethylidyne tris phenol photosensitizer comprises a resultant of 4,4′,4″-ethylidyne tris phenol and a quinone diazide compound reaction.

### Claim 6 (depends on 1)

The photoresist composition of claim 1, wherein the weight ratio of the benzophenone photosensitizer to the ethylidyne tris phenol photosensitizer is about 40:60.

### Claim 7 (depends on 1)

The photoresist composition of claim 1, wherein the novolac resin comprises a phenol compound including an m-cresol and a p-cresol in a weight ratio of the m-cresol to the p-cresol in a range from about 40:60 to about 60:40.

### Claim 8 (depends on 1)

The photoresist composition of claim 1, wherein the novolac resin comprises a phenol compound including an m-cresol and a p-cresol in a weight ratio of the m-cresol to the p-cresol of about 50:50.

### Claim 9 (depends on 1)

The photoresist composition of claim 1, wherein the novolac resin has a weight average molecular weight in a range from about 3,000 to about 15,000.

### Claim 10 (depends on 1)

The photoresist composition of claim 1, wherein a content of the novolac resin is in a range from about 5 percent by weight to about 20 percent by weight, a content of the photosensitizers is in a range from about 2 percent by weight to about 10 percent by weight, and a content of the organic solvent is in a range from about 75 percent by weight to about 90 percent by weight of the composition.

### Claim 11

A method of manufacturing a display substrate, the method comprising:
forming a switching element connected to a gate line and a data line;
forming a transparent electrode layer on a substrate having the switching element;
forming a photoresist pattern using a photoresist composition comprising: a) a novolac resin, b) a benzophenone photosensitizer and an ethylidyne tris phenol photosensitizer in a weight ratio of the benzophenone photosensitizer to the ethylidyne tris phenol photosensitizer in a range from about 20:80 to about 80:20 based on a total weight of the benzophenone photosensitizer and the ethylidyne tris phenol photosensitizer, and c) an organic solvent, the photoresist pattern formed on the transparent electrode layer; and
patterning the transparent electrode layer using the photoresist pattern as an etching mask to form a pixel electrode comprising a plurality of microelectrodes.

### Claim 12 (depends on 11)

The method of claim 11, wherein each of the microelectrodes has a width in a range from about 2.0 μm to about 2.8 μm.

### Claim 13 (depends on 11)

The method of claim 11, wherein a distance between the microelectrodes adjacent to each other is in a range from about 2.0 μm to about 2.8 μm.

### Claim 14 (depends on 11)

The method of claim 11, further comprising preparing the benzophenone photosensitizer by reacting a benzophenone compound with a quinone diazide compound.

### Claim 15 (depends on 11)

The method of claim 11, further comprising preparing the ethylidyne tris phenol photosensitizer by reacting an ethylidyne tris phenol compound with a quinone diazide compound.

### Claim 16 (depends on 11)

The method of claim 11, further comprising forming the novolac resin using a phenol compound including an m-cresol and a p-cresol in a weight ratio of the m-cresol to the p-cresol in a range from about 40:60 to about 60:40.

### Claim 17 (depends on 11)

The method of claim 11, wherein the novolac resin has a weight average molecular weight in a range from about 3,000 to about 15,000.

### Claim 18 (depends on 11)

The method of claim 11, wherein a content of the novolac resin is in a range from about 5 percent by weight to about 20 percent by weight, a content of the photosensitizer is in a range from about 2 percent by weight to about 10 percent by weight, and a content of the organic solvent is in a range from about 75 percent by weight to about 90 percent by weight.