# US 2010/0167180 A1 · Photosensitive Film for Holographic Recording and Production Method Thereof

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2010/0167180 A1
- Document ID: US20100167180A1
- Status: Published application
- Kind: A1
- Application number: 12/594,870
- Filed: 2008-03-19
- Published: 2010-07-01
- Earliest claimed: 2007-04-06
- Inventors: Liangheng Xu; Yun Gao; Yang Shen; Renshun You
- Web page: https://patentgrep.com/patent/US20100167180A1

## CPC

- G03H 1/02: Details {of features involved during the holographic process; Replication of holograms without interference recording}
- G03H 1/0252: {Laminate comprising a hologram layer}
- G03H 2001/0264: {Organic recording material}
- G03H 2001/0417: {for recording single beam Lippmann hologram wherein the object is illuminated by reference beam passing through the recording material}
- G03H 2001/2615: {in physical contact, i.e. layered holograms}
- G03H 2250/39: Protective layer
- G03H 2260/12: Photopolymer
- G03H: HOLOGRAPHIC PROCESSES OR APPARATUS (holograms, e.g. point holograms, used as ordinary optical elements G02B5/32; producing stereoscopic or other three-dimensional effects G02B30/00; diffraction-grating systems G02B27/44; systems using moiré fringes G02B27/60; optical logic elements G02F3/00; stereo-photography G03B35/00; photosensitive materials or processes for photographic purposes G03C; {stereo-photographic or similar processes G03C9/00}; apparatus for processing exposed photographic materials G03D; analogue computers performing mathematical operations with the aid of optical elements G06E3/00; authentication by radiation, of concealed information carried by holograms or diffraction gratings G06K19/16; holographic storage G11B7/0065, G11C13/04; {stereoscopic or other three dimensional effects in television systems H04N13/00})

## Abstract

A photosensitive film for holographic recording and its production method thereof are disclosed. The film comprises a base film, a buffer layer coated on one side of the base film, a photosensitive polymer coating layer formed by applying a photosensitive coating on the other side of the buffer layer, and a surface protective film covering the surface of the photosensitive polymer coating layer. Interference fringe patterns of a holographic image or an amphichronic graph are recorded in the photosensitive polymer coating layer. The film according to the present invention is a photosensitive material composed of two polymers of different refractive indexes, when coherent light beams intersect in its recording medium and produce an interference fringe pattern in the medium, monomers therein are excited accordingly and undergo free radical polymerization, thereby forming a hologram.

## Claims

### Claim 1

A photosensitive coating A comprising a photosensitive polymer coating and a solvent, wherein the photosensitive polymer coating contains the following ingredients in weight percents based on the total weight of the photosensitive polymer coating:
film former 20%-80%
monomers 10%-70%
photoinitiator 0.5%-7%
chain transfer agent 0.3%-5%
photosensitizer 0.05-2%
wherein the film former is selected from the group consisting of poly(methyl methacrylate), poly(butyl cellulose acetate), a butyl cellulose acetate-ethyl vinyl ether copolymer, a blend of polyvinyl butyral and cellulose acetate, a vinyl acetate-butyl acrylate-acrylic acid terpolymer, polystyrene-acrylonitrile, and a mixture of the polymers above and a fluoropolymer;
the monomers are two or more monomers selected from ethylenically unsaturated monomers; and
the photoinitiator is 2,4,6-triphenyl imidazolyl dimer, and;
the photosensitizer is selected from the group consisting of erythrosin B, diethylamino-benzylidene cyclopenpanone, michler's ketone, and 1,3,3-trimethyl-2-[5-(1,3,3-trimethyl-2-indolylidene)-1,3-pentadiene]indole iodide; and
the chain transfer agent is selected from the group consisting of 2-mercaptobenzoxazole, dodecanethiol and mercaptobenzothiazole.

### Claim 2 (depends on 1)

The photosensitive coating A according to claim 1, wherein the solid content of the photosensitive coating A is 5%-50% by weight.

### Claim 3 (depends on 1)

The photosensitive coating A according to claim 1, wherein the weight percents of ingredients are preferably as follows:
film former 30%-70%
monomers 23.0%-60.0%
photoinitiator 2.0%-7.0%
chain transfer agent 1.0%-3.0%
photosensitizer 0.5%-2.0%

### Claim 4 (depends on 1)

The photosensitive coating A according to claim 1, further comprising 0.5%-3% of a plasticizer based on the total weight of the photosensitive polymer coating, the plasticizer being selected from the group consisting of phthalate, alkyl diester, polyethylene glycol carboxylate and diethyl sebacate.

### Claim 5 (depends on 4)

The photosensitive coating A according to claim 4, further comprising 0.1% -1% of a UV absorber based on the total weight of the photosensitive polymer coating, the UV absorber based on the total wight of the photosensitive polymer coating, the UV absorber being selected from the group consisting of 2-hydroxyl-4-methoxybenzophenone and 2-(2H-Benzotriazole-2-yl)-4,6-bis(1-methyl-1-phenylethyl)phenol.

### Claim 6 (depends on 5)

The photosensitive coating A according to claim 5, further comprising 0.1%-1% of a non-ionic surfactant based on the total wight of the photosensitive polymer coaing, the non-ionic surfactant being selected from the group consisting of polyethylene glycol, methoxy polyethylene glycol, and Fluroad® FC-4430 (CAS No. 108-88-3).

### Claim 7 (depends on 1)

The photosensitive coating A according to claim 1, wherein the solvent is mixed solvent of butanone, dichloromethane, and methanol in a weight ration of 4-6:0.5-1.5:0.5-1.5.

### Claim 8 (depends on 7)

The photosensitive coating A according to claim 7, wherein the solvent is a mixed solvent of butanone, dichloromethane, and methanol in a weight ration of 5:1:1.

### Claim 9 (depends on 1)

The photosensitive coating material A according to claim 1, wherein the weight ratio of the two monomers is in the range of 0.5-1.8.

### Claim 10 (depends on 1)

The photosensitive coating material A according to claim 1, wherein the monomers are selected from the group consisting of monofunctional acrylates, N-vinylcarbazoles, ethoxylated bisphenol A diacrylate, 9-(4-phenyl-2-acrylethoxy)bifluorene and tricyclodecane dimethanol diacrylate.

### Claim 11 (depends on 1)

A photosensitive polymer film material C, comprising: a base film, a buffer layer coated on one side of the base film, a photosensitive polymer coating layer formed by applying the photosensitive polymer coating as recited in claim 1 on the other side of the buffer layer, and a surface protective film covering the surface of the photosensitive polymer coating layer.

### Claim 12 (depends on 11)

The photosensitive polymer film material C according to claim 11, wherein the photosensitive polymer coating, when dried, has a thickness of 3-50 μm.

### Claim 13 (depends on 11)

The photosensitive polymer film material C according to claim 11, wherein the buffer layer comprises a copolymer of vinyl acetate and acrylates, a vinylidene choloride-styrene-vinyl acetate copolymer, or a light-cured coating layer, and having a thickness of 1-2 μm.

### Claim 14 (depends on 11)

The photosensitive polymer film material C according to claim 11, wherein the surface protective film is selected from a group consisting of a PET film, a BOPP film, and a PE PVC film, each of which having a release coating layer, and the base film is selected from a group consisting of a PVC film, a PET film, and a BOPP film, and having a thickness of 20-100 μm.

### Claim 15 (depends on 1)

A reflection holographic film D, comprising a base film, a buffer layer coated on one side of the base film, and a photosensitive polymer coating layer formed by applying the photosensitive polymer coating as recited in claim 1 on the other side of the buffer layer, wherein interference fringe patterns of a holographic image or amphichronic graph are recorded onto the photosensitive polymer coating layer.

### Claim 16 (depends on 15)

The reflection holographic film D according to claim 15, wherein the recording layer has a thickness of 3-50 μm.

### Claim 17 (depends on 15)

The reflection holographic film D according to claim 15, wherein the base film is selected from a group consisting of a PVC film, a PET film, and a BOPP film.

### Claim 18 (depends on 15)

A method for producing the holographic photosensitive film D according to claim 15, comprising the steps of:
1) preparation of the coating material, wherein a film former, monomers, an initiator, a photosensitizer, a plasticizer and a surfactant are added to a solvent in a proportion under a light-proof condition or red light, dissolved by stirring to obtain the photosensitive coating A;
2) preparation of the film, wherein a layer with a thickness of 1-2 μm, composed of a copolymer of vinyl acetate and acrylates, or a vinylidene chloride-stryrene-vinyl acetate copolymer, is coated on the base film as a buffer layer; and the photosensitive coating A obtained from the previous step is applied onto the base film having the buffer layer under a light-proof condition or red light; and
the base film with a thickness of 20-100 μm is dried at 65-75° C. for 1-5 minutes to obtain a 20-50 μm thick photosensitive holographic material; and
the photosensitive holographic material is then dried and covered with a protective film, thereby obtaining the photosensitive polymer film material C;
3) preparation of the reflection holographic film D:
The protective film is removed from the product obtained from the previous step, and a hologram is recorded onto the photosensitive polymer film material C by a reflection holographic recording process;
the film is exposed to UV and visible light for a completed exposure on a UV curing machine and is heated at 120° C. for 2-50 minutes, thereby obtaining the reflection holographic film D.

### Claim 19 (depends on 18)

The method according to claim 18, wherein the wavelength of red light should be greater than 600 nm.

### Claim 20 (depends on 18)

The method according to claim 18, wherein a laser source has a wavelength of 514.5 nm or 532 nm, a light intensity of 60-110 mw/cm2, and the exposure time is 0.1-1.0 s.

### Claim 21 (depends on 18)

The method according to claim 18, wherein the laser source is generated by an argon ion laser or a semiconductor solid laser.