# US 2010/0167177 A1 · Carbon nanofiber with skin-core structure, method of producing the same, and products comprising the same

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2010/0167177 A1
- Document ID: US20100167177A1
- Status: Published application
- Kind: A1
- Application number: 12/385,439
- Filed: 2009-04-08
- Published: 2010-07-01
- Earliest claimed: 2008-11-06
- Assignees: Industry Foundation of Chonnam National University; Board of Regents, The University of Texas System
- Inventors: Kap Seung Yang; Bo-Hye Hye Kim; John P. Ferraris; Marilou dela Cruz
- Web page: https://patentgrep.com/patent/US20100167177A1

## CPC

- D01F 8/08: with at least one polyacrylonitrile as constituent
- D01D 5/003: {the material being a polymer solution or dispersion (D01D5/0053 takes precedence)}
- D01F 8/18: from other substances
- D01F 9/145: from pitch or distillation residues
- D01F 9/22: from polyacrylonitriles
- Y10T 428/2918: including free carbon or carbide or therewith [not as steel]
- D01F: CHEMICAL FEATURES IN THE MANUFACTURE OF ARTIFICIAL FILAMENTS, THREADS, FIBRES, BRISTLES OR RIBBONS; APPARATUS SPECIALLY ADAPTED FOR THE MANUFACTURE OF CARBON FILAMENTS
- D01D: MECHANICAL METHODS OR APPARATUS IN THE MANUFACTURE OF ARTIFICIAL FILAMENTS, THREADS, FIBRES, BRISTLES OR RIBBONS
- Y10T: TECHNICAL SUBJECTS COVERED BY FORMER US CLASSIFICATION

## Abstract

This invention relates to carbon nanofiber having a skin-core structure containing pitch and polyacrylonitrile, to a method of producing the carbon nanofiber, and to a product including the carbon nanofiber. The carbon nanofiber includes polyacrylonitrile and pitch having different properties respectively constituting a skin layer and/or a core layer, with a diameter of 1 μm or less, and thus functions of the carbon nanofiber vary depending on change in composition thereof.

## Claims

### Claim 1

A carbon nanofiber obtained by electrospinning a solution of polyacrylonitrile and pitch, the carbon nanofiber comprising:
a core comprising the pitch; and
a skin formed around the core and comprising a polyacrylonitrile homopolymer or copolymer.

### Claim 2

A carbon nanofiber obtained by electrospinning a solution of polyacrylonitrile and pitch, the carbon nanofiber comprising:
a core comprising a polyacrylonitrile homopolymer or copolymer; and
a skin formed around the core and comprising the pitch.

### Claim 3 (depends on 1)

The carbon nanofiber as set forth in claim 1, wherein the solution of polyacrylonitrile and pitch is prepared by dissolving the polyacrylonitrile and the pitch in solvents having different boiling points.

### Claim 4 (depends on 1)

The carbon nanofiber as set forth in claim 1, wherein the pitch is a dimethylformamide insoluble fraction obtained by fractionating the pitch using dimethylformamide.

### Claim 5 (depends on 1)

The carbon nanofiber as set forth in claim 1, wherein the pitch has a weight average molecular weight of 700˜5000 g/mol and solubility of 95% or more in a tetrahydrofuran solvent.

### Claim 6 (depends on 1)

The carbon nanofiber as set forth in claim 1, wherein a diameter of the carbon nanofiber including the core and the skin is 1 μm or less.

### Claim 7 (depends on 1)

The carbon nanofiber as set forth in claim 1, wherein a composition of the skin and the core varies depending on amounts of the polyacrylonitrile and the pitch.

### Claim 8 (depends on 1)

The carbon nanofiber as set forth in claim 1, wherein the skin comprises a plurality of pores having a size and a distribution that is controlled depending on changes in a heating rate, a kind of solvent for dissolving the pitch, or a concentration of the solvent.

### Claim 9

A method of producing a carbon nanofiber, the method comprising:
dissolving polyacrylonitrile in a first solvent, thus preparing a first spinning solution;
dissolving in a second solvent pitch having a molecular weight such that phase separation ensues upon blending with the polyacrylonitrile, thus preparing a second spinning solution;
blending the first spinning solution with the second spinning solution, thus preparing a third spinning solution;
electrospinning the third spinning solution, thus preparing a carbon nanofiber precursor; and
stabilizing the carbon nanofiber precursor, thus obtaining a flame-resistant fiber.

### Claim 10 (depends on 9)

The method as set forth in claim 9, wherein the second solvent has a boiling point lower than that of the first solvent.

### Claim 11 (depends on 10)

The method as set forth in claim 10, wherein the first solvent and the second solvent are each one or more members selected from the group consisting of tetrahydrofuran, dimethylformamide, dimethylacetamide, pyridine, and quinoline.

### Claim 12 (depends on 9)

The method as set forth in claim 9, further comprising subjecting the flame-resistant fiber to heat treatment at 900° C. or higher after stabilizing the carbon nanofiber precursor, thus obtaining the carbon nanofiber having a skin-core structure having different properties with a BET specific surface area of 300 m2/g or more.

### Claim 13 (depends on 1)

An electric double layer capacitor, comprising an electrode comprising the carbon nanofiber of claim 1.

### Claim 14 (depends on 1)

A fuel cell, comprising a catalyst support comprising the carbon nanofiber of claim 1.

### Claim 15 (depends on 14)

The fuel cell as set forth in claim 14, wherein the carbon nanofiber comprises a skin comprising pitch and a core comprising polyacrylonitrile.

### Claim 16 (depends on 9)

An electric double layer capacitor, comprising an electrode comprising the carbon nanofiber produced by the method set forth in claim 9.

### Claim 17 (depends on 9)

A fuel cell, comprising a catalyst support comprising the carbon nanofiber produced by the method as set forth in claim 9.

### Claim 18 (depends on 17)

The fuel cell as set forth in claim 17, wherein the carbon nanofiber comprises a skin comprising pitch and a core comprising polyacrylonitrile.