# US 2010/0167163 A1 · Proton-conducting membrane and the use of the same

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2010/0167163 A1
- Document ID: US20100167163A1
- Status: Published application
- Kind: A1
- Application number: 12/721,088
- Filed: 2010-03-10
- Published: 2010-07-01
- Earliest claimed: 2001-09-12
- Assignees: BASF Fuel Cell GmbH
- Inventors: Gordon Calundann; Michael J. Sansone; Oemer Uensal; Joachim Kiefer
- Web page: https://patentgrep.com/patent/US20100167163A1

## CPC

- B01D 67/0013: {Casting processes}
- B01D 71/62: Polycondensates having nitrogen-containing heterocyclic rings in the main chain
- C08J 5/2256: {based on macromolecular compounds obtained by reactions other than those involving carbon-to-carbon bonds, e.g. obtained by polycondensation}
- H01M 8/0293: Matrices for immobilising electrolyte solutions
- H01M 8/1027: having carbon, oxygen and other atoms, e.g. sulfonated polyethersulfones [S-PES]
- H01M 8/103: having nitrogen, e.g. sulfonated polybenzimidazoles [S-PBI], polybenzimidazoles with phosphoric acid, sulfonated polyamides [S-PA] or sulfonated polyphosphazenes [S-PPh]
- H01M 8/1032: having sulfur, e.g. sulfonated-polyethersulfones [S-PES]
- H01M 8/1048: Ion-conducting additives, e.g. ion-conducting particles, heteropolyacids, metal phosphate or polybenzimidazole with phosphoric acid
- H01M 8/1081: starting from solutions, dispersions or slurries exclusively of polymers
- H01M 8/1088: Chemical modification, e.g. sulfonation
- B01D 2323/081: Heating
- B01D 2323/26: Spraying processes
- C08J 2379/06: Polyhydrazides; Polytriazoles; Polyamino-triazoles; Polyoxadiazoles
- Y02E 60/50: Fuel cells
- Y02P 70/50: Manufacturing or production processes characterised by the final manufactured product
- B01D: SEPARATION (separating solids from solids by wet methods B03B, B03D; by pneumatic jigs or tables B03B; by other dry methods B07; magnetic or electrostatic separation of solid materials from solid materials or fluids, separation by high-voltage electric fields B03C; centrifuges, vortex apparatus B04; presses per se for squeezing-out liquid from liquid-containing material B30B9/02; treatment of water C02F, e.g. softening by ion-exchange C02F1/42; {arrangements of air intake cleaners in gas turbine plants F02C7/05} ; arrangements or mounting of filters in air-conditioning, air-humidification or ventilation F24F13/28)
- C08J: WORKING-UP; GENERAL PROCESSES OF COMPOUNDING; AFTER-TREATMENT NOT COVERED BY SUBCLASSES C08B, C08C, C08F, C08G or C08H (working, e.g. shaping, of plastics B29)
- H01M: PROCESSES OR MEANS, e.g. BATTERIES, FOR THE DIRECT CONVERSION OF CHEMICAL ENERGY INTO ELECTRICAL ENERGY
- Y02E: REDUCTION OF GREENHOUSE GAS [GHG] EMISSIONS, RELATED TO ENERGY GENERATION, TRANSMISSION OR DISTRIBUTION
- Y02P: CLIMATE CHANGE MITIGATION TECHNOLOGIES IN THE PRODUCTION OR PROCESSING OF GOODS

## Abstract

The invention relates to a novel proton-conducting polymer membrane based on polyazols. Said polymer membrane can be used in a variety of ways due to its outstanding chemical and thermal properties and is especially suitable as a polymer electrolyte membrane (PEM) for producing membrane electrode units for so-called PEM fuel cells.

## Claims

### Claim at position 1

1-23. (canceled)

### Claim 24

A process to produce proton-conducting polymer membrane based on polyazoles comprising the steps
A) dissolving a polyazole polymer in polyphosphoric acid to form a solution,
B) heating the solution obtained as described in step A) to temperatures of up to 400° C., under inert gas,
C) formulating a membrane on a support using the solution of the polyazole polymer from step B), and
D) treating the membrane formed in step C) in the presence of moisture at temperatures and for a time which are sufficient for the membrane to become self-supporting so that it can be detached from the support without damage.

### Claim 25 (depends on 24)

The process as claimed in claim 24, wherein the polyphosphoric acid used in step A) has an assay calculated as P2O5 (acidimetric) of at least 85%.

### Claim 26 (depends on 24)

The process as claimed in claim 24, wherein a dispersion/suspension instead of a solution of the polymer is produced in step A).

### Claim 27 (depends on 24)

The process as claimed in claim 24, wherein the polymer used in step A) comprises recurring azole units of the formula (I) and/or
where
Ar are identical or different and are each a tetravalent aromatic or heteroaromatic group which may have one or more rings,
Ar1 are identical or different and are each a divalent aromatic or heteroaromatic group which may have one or more rings,
Ar2 are identical or different and are each a divalent or trivalent aromatic or heteroaromatic group which may have one or more rings,
X are identical or different and are each oxygen, sulfur or an amino group bearing a hydrogen atom, a group having 1-20 carbon atoms, a branched or unbranched alkyl or alkoxy group, and an aryl group as further radical.

### Claim 28 (depends on 27)

The process as claimed in claim 27, wherein
X are identical or different and a branched or unbranched alkyl or alkoxy group.

### Claim 29 (depends on 24)

The process as claimed in claim 24, wherein a polymer selected from the group consisting of polybenzimidazole, poly(pyridines), poly(pyrimidines), polyimidazoles, polybenzothiazoles, polybenzoxazoles, polyoxadiazoles, polyquinoxalines, polythiadiazoles and poly(tetrazapyrenes) is used in step A).

### Claim 30 (depends on 24)

The process as claimed in claim 24, wherein the polymer used in step A) comprises one or more recurring benzimidazole units of the formula
where n and m are each an integer greater than or equal to 10.

### Claim 31 (depends on 30)

The process as claimed in claim 30, wherein n and m are each an integer greater than or equal to 100.

### Claim 32 (depends on 24)

The process as claimed in claim 24, wherein the viscosity is adjusted by addition of phosphoric acid after step B) and before step C).

### Claim 33 (depends on 24)

The process as claimed in claim 24, wherein the membrane produced in step C) is treated in the presence of moisture at temperatures and for a time until the membrane is self-supporting and can be detached from the support without damage.

### Claim 34 (depends on 24)

The process as claimed in claim 24, wherein the treatment of the membrane in step D) is carried out at temperatures of from >0° C. to 150° C. in the presence of moisture or water, dilute phosphoric acid and/or water vapor.

### Claim 35 (depends on 34)

The process as claimed in claim 34, wherein the treatment of the membrane in step D) is carried out at temperatures of from 10° C. to 120° C.

### Claim 36 (depends on 35)

The process as claimed in claim 35, wherein the treatment of the membrane in step D) is carried out at temperatures of from room temperature (20° C.) to 90° C.

### Claim 37 (depends on 24)

The process as claimed in claim 24, wherein the treatment of the membrane in step D) is carried out for from 10 second to 300 hours.

### Claim 38 (depends on 37)

The process as claimed in claim 37, wherein the treatment of the membrane in step D) is carried out for from 1 minute to 200 hours.

### Claim 39 (depends on 24)

The process as claimed in claim 24, wherein subsequent to the treatment in step D) the membrane is crosslinked by action of IR or NIR.

### Claim 40 (depends on 24)

The process as claimed in claim 24, wherein an electrode is chosen as the support in step C).

### Claim 41 (depends on 24)

The process as claimed in claim 24, wherein the membrane formed in step C) has a thickness of from 20 to 2000 μm.

### Claim 42 (depends on 41)

The process as claimed in claim 41, wherein the membrane formed in step C) has a thickness of from 30 to 1500 μm.

### Claim 43 (depends on 42)

The process as claimed in claim 42, wherein the membrane formed in step C) has a thickness of from 50 to 1200 μm.

### Claim 44 (depends on 24)

The process as claimed in claim 24, wherein the membrane formed in step D) has a thickness of from 15 to 400 μm and is self-supporting.

### Claim 45 (depends on 44)

The process as claimed in claim 44, wherein the membrane formed in step D) has a thickness of from 20 to 200 μm.

### Claim 46 (depends on 45)

The process as claimed in claim 45, wherein the membrane formed in step D) has a thickness of from 20 to 150 μm.

### Claim 47 (depends on 24)

The process as claimed in claim 24, wherein the membrane has a layer comprising a catalytically active component.

### Claim 48

An electrode provided with a proton-conducting polymer coating based on polyazoles which has a concentration of phosphoric acid expressed as mol of acid per mol of recurring unit of the polymer of from 12 to 20 which membrane is obtained by a process comprising the steps
A) dissolving a polyazole polymer in polyphosphoric acid to form a solution,
B) heating the solution obtained as described in step A) to temperatures of up to 400° C., under inert gas,
C) applying a layer to an electrode using the solution of the polyazole polymer from step B), and.
D) treating the layer formed in step C) at temperatures of from 0° C. to 150° C. in the presence of moisture.

### Claim 49

A membrane-electrode unit comprising:
at least one electrode provided with a proton-conducting polymer coating based on polyazoles which has a concentration of phosphoric acid expressed as mol of acid per mol of recurring unit of the polymer of from 12 to 20 which membrane is obtained by a process comprising the steps
i) dissolving a polyazole polymer in polyphosphoric acid to form a solution,
ii) heating the solution obtained as described in step i) to temperatures of up to 400° C., under inert gas,
iii) applying a layer to an electrode using the solution of the polyazole polymer from step ii), and
iv) treating the layer formed in step iii) at temperatures of from 0° C. to 150° C. in the presence of moisture; and
at least one proton-conducting polymer membrane based on polyazoles which has a concentration of phosphoric acid expressed as mol of acid per mol of recurring unit of the polymer of from 12 to 20 and is obtained by a process comprising the steps
A) dissolving a polyazole polymer in polyphosphoric acid to form a solution,
B) heating the solution obtained as described in step A) to temperatures of up to 400° C., under inert gas,
C) formulating a membrane on a support using the solution of the polyazole polymer from step B), and
D) treating of the membrane formed in step C) in the presence of moisture at temperatures and for a time which are sufficient for the membrane to become self-supporting so that it can be detached from the support without damage.

### Claim 50 (depends on 49)

A fuel cell comprising the membrane-electrode membrane as claimed in claim 49.