# US 2010/0167127 A1 · Lithium iron phosphate battery electrode and method for manufacturing the same

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2010/0167127 A1
- Document ID: US20100167127A1
- Status: Published application
- Kind: A1
- Application number: 12/641,278
- Filed: 2009-12-17
- Published: 2010-07-01
- Earliest claimed: 2008-12-30
- Assignees: Hengdian Group DMEGC Magnetic Limited Company, a Chinese Corporation
- Inventors: Dayang Cheng; Guoguang Wang; Daxin Bao; Shijin He
- Web page: https://patentgrep.com/patent/US20100167127A1

## CPC

- H01M 4/13: Electrodes for accumulators with non-aqueous electrolyte, e.g. for lithium-accumulators; Processes of manufacture thereof
- H01M 4/5825: {Oxygenated metallic salts or polyanionic structures, e.g. borates, phosphates, silicates, olivines}
- H01M 4/621: {Binders}
- H01M 10/0525: Rocking-chair batteries, i.e. batteries with lithium insertion or intercalation in both electrodes; Lithium-ion batteries
- Y02E 60/10: Energy storage using batteries
- Y02P 70/50: Manufacturing or production processes characterised by the final manufactured product
- H01M: PROCESSES OR MEANS, e.g. BATTERIES, FOR THE DIRECT CONVERSION OF CHEMICAL ENERGY INTO ELECTRICAL ENERGY
- Y02E: REDUCTION OF GREENHOUSE GAS [GHG] EMISSIONS, RELATED TO ENERGY GENERATION, TRANSMISSION OR DISTRIBUTION
- Y02P: CLIMATE CHANGE MITIGATION TECHNOLOGIES IN THE PRODUCTION OR PROCESSING OF GOODS

## Abstract

The present invention relates to an electrode for the lithium iron phosphate battery and the manufacturing method thereof, and more particularly, to a coated electrode for the lithium iron phosphate with a smooth surface and without de-powder phenomenon and the manufacturing method thereof. The electrode provided in the present invention uses an arabic gum modified by adding silicone-based gel into the arabic gum. The lithium iron phosphate active material and the conductive agent in a certain ratio are added into the aforesaid modified arabic gums, after the mixing process, a liquid slurry with a certain viscosity is formed. Then, the liquid slurry is coated uniformly onto a positive current collector of aluminum foil or mesh, and followed by the process like drying, calendaring, cutting and etc. to form positive electrode plate. The electrode in the present invention has the characteristics of smooth surface and no de-powder phenomenon. The difficult-to-coat problem in manufacturing lithium ion battery electrode with lithium iron phosphate in the prior art is overcome.

## Claims

### Claim 1

A lithium iron phosphate battery electrode, characterized in that, the electrode comprises a current collector and an active material layer coated on the current collector; the active material layer comprises an active material, a binder and a conductive agent, wherein the active material is lithium iron phosphate, and the binder is a modified arabic gum; preferably, the active material layer is composed of the active material, the binder and the conductive agent.

### Claim 2 (depends on 1)

The lithium iron phosphate battery electrode according to claim 1, characterized in that, the modified arabic gum is a mixture of silicone-based gel and arabic gum, preferably, the modified arabic gum is the mixture formed by adding silicone-based gel into water soluble arabic gum.

### Claim 3 (depends on 2)

The lithium iron phosphate battery electrode according to claim 2, characterized in that, the proportion of silicone-based gel and arabic gum in the modified arabic gum is (10-45) wt %:(90-55) wt % prefer (2-30) wt %:(88-70) wt %.

### Claim 4 (depends on 2)

The lithium iron phosphate battery electrode according to claim 2, characterized in that, the examples of the proportion of silicone-based gel and arabic gum in the modified arabic gum can be: 20 wt %:80 wt %, 16 wt %:84 wt %, 30 wt %:70 wt %, 12 wt %:88 wt %, 15 wt %:85 wt %, 20 wt %:80 wt %.

### Claim 5 (depends on 2)

The lithium iron phosphate battery electrode according to claim 2, characterized in that, on basis of the weight of the active material layer, the content of lithium iron phosphate is in the range of 85˜95 wt %, the content of the modified arabic gum is in the range of 2˜8 wt %, and the content of the conductive agent is in the range of 2˜8 wt %.

### Claim 6 (depends on 3)

The lithium iron phosphate battery electrode according to claim 3, characterized in that, on basis of the weight of the active material layer, the content of lithium iron phosphate is in the range of 85˜95 wt %, the content of the modified arabic gum is in the range of 2˜8 wt %, and the content of the conductive agent is in the range of 2˜8 wt %.

### Claim 7 (depends on 2)

The lithium iron phosphate battery electrode according to claim 2, characterized in that, the compacted density of the electrode is in the range of 2.0˜2.3 g/cm3.

### Claim 8 (depends on 2)

A lithium ion battery, comprising a positive electrode, a negative electrode, an electrolyte solution and a separator, in which, the lithium iron phosphate battery electrode as set forth in claim 2 is used.

### Claim 9 (depends on 3)

A lithium ion battery, comprising a positive electrode, a negative electrode, an electrolyte solution and a separator, in which, the lithium iron phosphate battery electrode as set forth in claim 3 is used.

### Claim 10 (depends on 4)

A lithium ion battery, comprising a positive electrode, a negative electrode, an electrolyte solution and a separator, in which, the lithium iron phosphate battery electrode as set forth in claim 4 is used.

### Claim 11 (depends on 5)

A lithium ion battery, comprising a positive electrode, a negative electrode, an electrolyte solution and a separator, in which, the lithium iron phosphate battery electrode as set forth in claim 5 is used.

### Claim 12

A method for improving the surface smoothness of the lithium iron phosphate battery electrode or decreasing de-powder phenomenon of the said electrode, in which, the modified arabic gum as binder is used to manufacture lithium iron phosphate battery electrode.

### Claim 13 (depends on 1)

A method for manufacturing lithium iron phosphate battery electrode according to claim 1, comprising the following steps:
A. mixing the modified arabic gum, the conductive agent and lithium iron phosphate, and stirring uniformly to form the mixture;
B. coating the aforesaid mixture to form the electrode, then drying the electrode.

### Claim 14 (depends on 13)

The method for manufacturing lithium iron phosphate battery electrode according to claim 13, comprising the following steps:
A. on basis of the dry weight of the mixture, mixing 2˜8 wt % of the modified arabic gum, 2˜8 wt % of the conductive agent and 85˜95 wt % of lithium iron phosphate, stirring uniformly to form the slurry, and adjusting the viscosity of the slurry to 3500±500 mPa·s;
B. coating the mixture on the electrode, and drying the electrode at the temperature of 60˜130° C.;
C. drying the coated electrode in vacuum oven at 100˜120° C. for 8˜10 hours; calendaring the dried electrode to the compacted density of 2.0˜2.3 g/cm3.

### Claim 15 (depends on 13)

The method for manufacturing lithium iron phosphate battery electrode according to claim 13, wherein in step A, the mixing is adding lithium iron phosphate and the conductive agent into the modified arabic gum solution successively.

### Claim 16 (depends on 13)

The method for manufacturing lithium iron phosphate battery electrode according to claim 13, wherein in step B, the coating is one-side coating or two-side coating.

### Claim 17 (depends on 13)

The method for manufacturing lithium iron phosphate battery electrode according to claim 13, wherein in step B, when the coating is one-side coating, the drying temperature is in the range of 60˜100° C.

### Claim 18 (depends on 16)

The method for manufacturing lithium iron phosphate battery electrode according to claim 16, wherein in step B, when the coating in step B is two-side coating, drying the electrode at lower temperature after the first side is coated, and then drying the electrode at higher temperature, preferably at 100˜130° C., after the second side is coated.

### Claim 19 (depends on 13)

The method for manufacturing lithium iron phosphate battery electrode according to claim 13, wherein in step B, the area density for single side is 125˜200 g/m2.

### Claim 20 (depends on 13)

The method for manufacturing lithium iron phosphate battery electrode according to claim 13, characterized in that, the modified arabic gum is prepared to 5 wt % of the modified arabic gum solution when being used in step A, and the added amount of the modified arabic gum when mixing is calculated based on the amount of the solid modified arabic gum.

### Claim 21 (depends on 15)

The method for manufacturing lithium iron phosphate battery electrode according to claim 15, characterized in that, the modified arabic gum is prepared to 5 wt % of the modified arabic gum solution when being used in step A, and the added amount of the modified arabic gum when mixing is calculated based on the amount of the solid modified arabic gum.