# US 2010/0167085 A1 · Electroplating Method and Electroplated Product

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2010/0167085 A1
- Document ID: US20100167085A1
- Status: Published application
- Kind: A1
- Application number: 12/623,727
- Filed: 2009-11-23
- Published: 2010-07-01
- Earliest claimed: 2008-12-26
- Assignees: BYD Company Limited
- Inventors: Jipeng Sun; Aihua Li; Zaichun Li; Bo Peng
- Web page: https://patentgrep.com/patent/US20100167085A1

## CPC

- C23C 28/023: {only coatings of metal elements only}
- C23C 28/021: {including at least one metal alloy layer}
- C23C 28/025: {with at least one zinc-based layer}
- C25D 3/06: from solutions of trivalent chromium
- C25D 3/38: of copper
- C25D 3/58: containing more than 50% by weight of copper
- C25D 5/12: at least one layer being of nickel or chromium
- C25D 5/611: {Smooth layers}
- C25D 5/627: {Electroplating characterised by the visual appearance of the layers, e.g. colour, brightness or mat appearance}
- Y10T 428/12736: Al-base component
- C23C: COATING METALLIC MATERIAL; COATING MATERIAL WITH METALLIC MATERIAL; SURFACE TREATMENT OF METALLIC MATERIAL BY DIFFUSION INTO THE SURFACE, BY CHEMICAL CONVERSION OR SUBSTITUTION; COATING BY VACUUM EVAPORATION, BY SPUTTERING, BY ION IMPLANTATION OR BY CHEMICAL VAPOUR DEPOSITION, IN GENERAL (making metal-coated products by extrusion B21C23/22; covering with metal by connecting pre-existing layers to articles, see the relevant places, e.g. B21D39/00, B23K; metallising of glass C03C; metallising mortars, concrete, artificial stone, ceramics or natural stone C04B41/00; enamelling of, or applying a vitreous layer to, metals C23D; treating metal surfaces or coating of metals by electrolysis or electrophoresis C25D; single-crystal film growth C30B; by metallising textiles D06M11/83; decorating textiles by locally metallising D06Q1/04)
- C25D: PROCESSES FOR THE ELECTROLYTIC OR ELECTROPHORETIC PRODUCTION OF COATINGS; ELECTROFORMING; APPARATUS THEREFOR
- Y10T: TECHNICAL SUBJECTS COVERED BY FORMER US CLASSIFICATION

## Abstract

A method for electroplating a substrate having an aluminum alloy surface comprises: applying a zinc layer onto the aluminum alloy surface; electroplating a first copper layer onto the zinc layer from an alkaline copper electroplating solution; electroplating a second copper layer onto the first copper layer from an acid copper electroplating solution; electroplating a Cu—Sn alloy layer onto the second copper layer from a Cu—Sn electroplating solution; and electroplating a chromium layer onto the Cu—Sn alloy layer from a trivalent chromium solution. The alkaline copper electroplating solution is substantially free of cyanide ion.

## Claims

### Claim 1

A method for electroplating a substrate having an aluminum alloy surface comprising:
applying a zinc layer onto the aluminum alloy surface;
electroplating a first copper layer onto the zinc layer from an alkaline copper electroplating solution, wherein the alkaline copper solution is substantially free of cyanide ion;
electroplating a second copper layer onto the first copper layer from an acid copper electroplating solution;
electroplating a Cu—Sn alloy layer onto the second copper layer from a Cu—Sn electroplating solution; and
electroplating a chromium layer onto the Cu—Sn alloy layer from a trivalent chromium solution.

### Claim 2 (depends on 1)

The method of claim 1, wherein the zinc layer is formed by placing the aluminum alloy in a zinc-containing solution;
wherein the zinc-containing solution comprises zinc oxide, sodium hydroxide, potassium sodium tartrate, ferric chloride, sodium nitrite, and water; and
wherein the concentration of zinc oxide is between about 20 and about 60 g/L, the concentration of sodium hydroxide is between about 100 and about 130 g/L, the concentration of potassium sodium tartrate is between about 40 and about 60 g/L, the concentration of ferric chloride is between about 0.5 and about 2.5 g/L, and the concentration of sodium nitrite is between about 0.5 and about 4 g/L.

### Claim 3 (depends on 2)

The method of claim 2, wherein the temperature of the zinc-containing solution is between about 20 and about 28° C.; and the aluminum alloy is placed in the zinc-containing solution for between about 40 seconds and about 2 minutes.

### Claim 4 (depends on 1)

The method of claim 1, wherein the alkaline copper electroplating solution comprises potassium pyrophosphate, copper pyrophosphate, a stabilizing agent, a brightening agent, and water; and
wherein the concentration of potassium pyrophosphate is between about 350 and about 420 g/L, the concentration of copper pyrophosphate is between about 15 and about 25 g/L, the concentration of the stabilizing agent is between about 65 and about 85 ml/L, and the concentration of the brightening agent is between about 15 and about 25 ml/L.

### Claim 5 (depends on 1)

The method of claim 1, wherein the temperature of the alkaline copper electroplating solution is between about 35 and about 60° C.; the pH of the alkaline copper electroplating solution is between about 9.2 and about 10.0; the electroplating cathodic current density of the first copper layer is between about 0.5 and about 2.5 A/dm2; and the electroplating time for the first copper layer is between about 5 minutes and about 20 minutes.

### Claim 6 (depends on 1)

The method of claim 1, wherein the acid copper electroplating solution comprises CuSO4, H2SO4, chloride ion, an auxiliary agent, a smoothing agent, a brightening agent, and water; and
wherein the concentration of CuSO4 is between about 180 and about 250 g/L, the concentration of H2SO4 is between about 50 and about 70 g/L, the concentration of chloride ion is between about 40 and about 100 mg/L, the concentration of the auxiliary agent is between about 8 and about 10 ml/L, the concentration of the smoothing agent is between about 0.4 and about 0.6 ml/L, and the concentration of the brightening agent of about 0.4 and about 0.6 ml/L.

### Claim 7 (depends on 1)

The method of claim 1, wherein the temperature of the acid copper electroplating solution is between about 20 and about 30° C., and the cathodic current density of the second copper layer is between about 3 and about 5 A/dm2; the electroplating time for the second copper layer is between about 15 minutes and about 40 minutes; and
wherein an anode is made of copper containing phosphorus in about 0.03 to 0.06% by weight.

### Claim 8 (depends on 1)

The method of claim 1, wherein the electroplating of the second copper layer further comprises steps of:
stirring the copper solution; and
filtering the copper solution.

### Claim 9 (depends on 1)

The method of claim 1, wherein the Cu—Sn electroplating solution comprises potassium pyrophosphate, copper pyrophosphate, stannous pyrophosphate, a complexing agent, a stabilizing agent, and a brightening agent;
wherein the concentration of potassium pyrophosphate is between about 250 and about 350 g/L, the concentration of copper pyrophosphate is between about 5 and about 12 g/L, the concentration of stannous pyrophosphate is between about 15 and about 35 g/L, the concentration of the complexing agent is between about 80 and about 120 ml/L, the concentration of the stabilizing agent is between about 10 and about 30 ml/L, and the concentration of the brightening agent is between about 10 and about 20 ml/L.

### Claim 10 (depends on 1)

The method of claim 1, wherein the temperature of the Cu—Sn alloy electroplating solution is between about 15 and about 30° C.; the pH of the Cu—Sn alloy electroplating solution is between about 8.0 and about 8.8; the electroplating cathodic current density of the Cu—Sn alloy layer is between about 0.5 and about 1 A/dm2; and the electroplating time for the Cu—Sn alloy layer is between about 5 minutes and about 15 minutes.

### Claim 11 (depends on 1)

The method of claim 1, wherein the trivalent chromium electroplating solution comprises an auxiliary agent, a stabilizing agent, a wetting agent, a complexing agent and a trivalent chromium compound; and
wherein the auxiliary agent is between about 400 and about 450 ml/L, the stabilizing agent is between about 55 and about 75 ml/L, the wetting agent is between about 2 and about 5 ml/L, the complexing agent is between about 1 and about 3 ml/L, and trivalent chromium is between about 20 and about 25 g/L.

### Claim 12 (depends on 1)

The method of claim 1, wherein the temperature of the chromium electroplating solution is between about 28 and about 35° C.; the pH of the chromium electroplating solution is between about 2.5 and about 3.0; the electroplating current density of the chromium layer is between about 8 and about 30 A/dm2; and the electroplating time for the chromium layer is between about 1 minutes and about 5 minutes.

### Claim 13 (depends on 1)

The method of claim 1, wherein the electroplating of the chromium layer further comprises steps of:
stirring the chromium solution; and
filtering the chromium solution.

### Claim 14 (depends on 1)

The method of claim 1, further comprising a step of treating the aluminum alloy surface.

### Claim 15 (depends on 1)

The method of claim 1, further comprising a step of washing with water after at least one step of electroplating.

### Claim 16

A method for electroplating a substrate having an aluminum alloy surface comprising:
applying a zinc layer onto the aluminum alloy surface;
electroplating a first copper layer onto the zinc layer from an alkaline copper electroplating solution, wherein the alkaline copper solution is substantially free of cyanide ion;
electroplating a second copper layer onto the first copper layer from an acid copper electroplating solution;
applying an activating solution onto the second copper layer;
electroplating a Cu—Sn alloy layer onto the second copper layer from a Cu—Sn electroplating solution; and
electroplating a chromium layer onto the Cu—Sn alloy layer from a trivalent chromium solution.

### Claim 17 (depends on 16)

The method of claim 16, wherein the activating solution is an acid.

### Claim 18 (depends on 17)

The method of claim 17, wherein the acid is a H2SO4 solution.

### Claim 19 (depends on 16)

The method of claim 16, further comprising a step of applying a solution onto the Cu—Sn alloy layer.

### Claim 20

An electroplated product comprising:
a substrate having an aluminum alloy surface;
a zinc layer on the aluminum alloy surface;
a copper layer on the zinc layer, wherein the copper layer is formed by electroplating from an alkaline copper electroplating solution, and wherein the alkaline copper electroplating solution is substantially free of cyanide ion;
a Cu—Sn alloy layer on the copper layer; and
a chromium layer on Cu—Sn alloy layer;
wherein the electroplated layers are substantially free of nickel.