- Web page: https://patentgrep.com/patent/US20100167059A1

## CPC

- C03C 21/00: Treatment of glass, not in the form of fibres or filaments, by diffusing ions or metals in the surface
- C03B 17/064: {by the overflow downdraw fusion process; Isopipes therefor}
- C03C 3/062: with less than 40% silica by weight
- C03C 15/00: Surface treatment of glass, not in the form of fibres or filaments, by etching (etching or surface-brightening compositions, in general C09K13/00)
- C03C 21/002: {to perform ion-exchange between alkali ions (C03C21/005 takes precedence)}
- C03C 2203/10: Melting processes
- C03C 2203/50: After-treatment
- Y10T 428/315: Surface modified glass [e.g., tempered, strengthened, etc.]
- C03C: CHEMICAL COMPOSITION OF GLASSES, GLAZES OR VITREOUS ENAMELS; SURFACE TREATMENT OF GLASS; SURFACE TREATMENT OF FIBRES OR FILAMENTS MADE FROM GLASS, MINERALS OR SLAGS; JOINING GLASS TO GLASS OR OTHER MATERIALS
- C03B: MANUFACTURE, SHAPING, OR SUPPLEMENTARY PROCESSES
- Y10T: TECHNICAL SUBJECTS COVERED BY FORMER US CLASSIFICATION

## Abstract

A glass substrate chemically strengthened, includes a primary surface that has a compressive stress layer formed in an uppermost surface layer thereof. The compressive stress layer is configured to enhance strength of the glass substrate due to a compressive stress generated in the compressive stress layer. The compressive layer consists of a layer of a potassium ion concentration equal to or less than 5000 parts per million (ppm).

## Claims

### Claim 1

A glass substrate chemically strengthened, comprising a primary surface that has a compressive stress layer formed in an uppermost surface layer thereof, the compressive stress layer being configured to enhance strength of the glass substrate due to a compressive stress generated in the compressive stress layer,
wherein the compressive layer consists of a layer of a potassium ion concentration equal to or less than 5000 parts per million (ppm).

### Claim 2 (depends on 1)

The glass substrate according to claim 1,
wherein the compressive stress layer is configured with an ion exchange layer of a potassium ion concentration more than 5000 ppm being completely removed therefrom.

### Claim 3 (depends on 1)

The glass substrate according to claim 1, formed from molten glass by a down-draw method.

### Claim 4 (depends on 1)

The glass substrate according to claim 1, configured with aluminosilicate glass that contains at least one of SiO2, Al2O3, Li2O, and Na2O.

### Claim 5 (depends on 4)

The glass substrate according to claim 4, configured by chemically strengthening a glass substrate that contains substantially no potassium ion.

### Claim 6 (depends on 1)

The glass substrate according to claim 1, configured to be used for a cover glass for protecting a display screen of a mobile terminal device.

### Claim 7

A method for manufacturing a glass substrate, comprising the steps of:
chemically strengthening the glass substrate by immersing the glass substrate in heated molten salt such that ions of the glass substrate are ion-exchanged for ions of the molten salt; and
removing an ion exchange layer formed in an uppermost surface layer of a primary surface of the glass substrate in the step of chemically strengthening the glass substrate.

### Claim 8 (depends on 7)

The method according to claim 7,
wherein, in the step of removing the ion exchange layer, the ion exchange layer is removed by etching.

### Claim 9 (depends on 8)

The method according to claim 8,
wherein the etching is implemented in a wet manner using etching solution that contains at least one of hydrofluoric acid, hexafluorosilicic acid, and buffered hydrofluoric acid.

### Claim 10 (depends on 7)

The method according to claim 7,
wherein, in the step of chemically strengthening the glass substrate, the glass substrate is chemically strengthened using at least one of molten salt of potassium nitrate and molten salt of sodium nitrate at a temperature equal to or less than a glass transition point of the glass substrate.

### Claim 11 (depends on 7)

The method according to claim 7,
wherein the ion exchange layer has a potassium ion concentration more than 5000 ppm.