# US 2010/0167036 A1 · Solid polymeric materials for detection, transfer, amplification and memory of chirality of optically active compounds

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2010/0167036 A1
- Document ID: US20100167036A1
- Status: Published application
- Kind: A1
- Application number: 12/293,710
- Filed: 2007-03-06
- Published: 2010-07-01
- Earliest claimed: 2006-03-21
- Assignees: Universita Degli Studi Di
- Inventors: Annamaria Buono; Gaetano Guerra; Paola Rizzo
- Web page: https://patentgrep.com/patent/US20100167036A1

## CPC

- G01N 21/19: Dichroism
- C08F 12/08: Styrene
- C08J 5/18: Manufacture of films or sheets
- G01N 21/77: by observing the effect on a chemical indicator
- C08J 2325/06: Polystyrene
- G01N: INVESTIGATING OR ANALYSING MATERIALS BY DETERMINING THEIR CHEMICAL OR PHYSICAL PROPERTIES (measuring or testing apparatus or processes other than immunoassay, involving enzymes or microorganisms C12M, C12Q)
- C08F: MACROMOLECULAR COMPOUNDS OBTAINED BY REACTIONS ONLY INVOLVING CARBON-TO-CARBON UNSATURATED BONDS
- C08J: WORKING-UP; GENERAL PROCESSES OF COMPOUNDING; AFTER-TREATMENT NOT COVERED BY SUBCLASSES C08B, C08C, C08F, C08G or C08H (working, e.g. shaping, of plastics B29)

## Abstract

Solid polymeric materials for detection, transfer, amplification and memory of chirality of optically active compounds are described. These materials not only are able to absorb also traces of volatile organic compounds (both chiral and achiral) prevailingly as guest of a nanoporous crystalline phase, but for the case of chiral guests are also able to transfer and amplify their chirality, producing intense phenomena of induced circular dichroism (ICD). This induced dichroism remains stable also after chiral guest removal, as well as after temperature increases at least up to 250° C. The solid polymeric materials of the present invention can find applications in sensorics of optically active molecules as well as in systems for storage of data.

## Claims

### Claim at position 1

1-12. (canceled)

### Claim 13

A process for the manufacture of solid polymeric materials based on syndiotactic polystyrene in its δ nanoporous crystalline form or on styrene copolymers with olefins CH2═CH—R, wherein R is an alkyl-aryl or a substituted aryl radical with 6-20 carbon atoms, or with other co-polymerizable ethylenically unsaturated monomers, said copolymers being syndiotactic and crystallizable in δ nanoporous crystalline form, wherein said crystalline form is characterized by elongated morphologies with shape-ratio higher than 5 and minor size in the range 10-0.01 μm, said process comprising:
(a) dissolution of syndiotactic polystyrene, syndiotactic styrene copolymers, or both with olefins CH2═CH—R, wherein R is an alkyl-aryl or a substituted aryl radical with 6-20 carbon atoms, or with other co-polymerizable ethylenically unsaturared monomers, in at least solvent selected from the group consisting of halogenated solvents, aromatic solvents, cyclic aliphatic solvents, and sulphur containing solvents, to obtain a solution of at least said polystyrene or said copolymers;
(b) flow-crystallization of said solution of said polystyrene, said copolymers, or both on a support to obtain a semicrystalline sample; and
(c) treatment of said semicrystalline sample with volatile guests of said polystyrene, said copolymers, or both, whereby said polystyrene, said copolymers, or both in said sample are obtained in δ nanoporous crystalline form.

### Claim 14 (depends on 13)

The process according to claim 13, wherein said flow-crystallization is obtained by spin-coating with spin-rate >100 rounds/min, preferably >300 rounds/min.

### Claim 15 (depends on 13)

The process according to claim 13, wherein said semicrystalline sample in step (b) is obtained as a film with thickness lower than 100 μm, preferably lower than 1 μm.

### Claim 16 (depends on 13)

The process according to claim 13, wherein said solvent is selected from the group consisting of chloroform, methylene chloride, carbon tetrachloride, dichloroethane, trichloroethylene, tetrachloroethylene, dibromoethane, methyliodide, benzene, styrene, cyclohexane, tetrahydrofurane, and carbon disulfide.

### Claim 17 (depends on 13)

The process according to claim 13, wherein said solvent is selected from the group consisting of chloroform and tetrahydrofurane.

### Claim 18 (depends on 13)

The process according to claim 13, wherein said treatment of said semicrystalline sample by a volatile guest of said polystyrene, said copolymers, or both comprises a treatment with carbon dioxide in supercritical conditions, said conditions comprising temperature in the range between room temperature and 100° C., preferably between 30 and 70° C., and pressure in the range between 60 and 800 bar, preferably between 70 and 150 bar.

### Claim 19 (depends on 13)

The process according to claim 13, wherein said treatment of said semicrystalline sample by a volatile guest of said polystyrene, said copolymers, or both comprises a treatment with acetone, acetonitrile, or both.

### Claim 20 (depends on 13)

A polymeric material obtainable according to claim 13.

### Claim 21 (depends on 14)

A polymeric material obtainable according to claim 14.

### Claim 22 (depends on 15)

A polymeric material obtainable according to claim 15.

### Claim 23 (depends on 22)

The polymeric material of claim 22, obtainable as a film with thickness lower than 100 μm, preferably lower than 1 μm.

### Claim 24 (depends on 20)

A process for the production of materials for detection, transfer, amplification and memory of chirality of optically active compounds comprising the use of a polymeric material of claim 20.

### Claim 25 (depends on 21)

A process for the production of materials for detection, transfer, amplification and memory of chirality of optically active compounds comprising the use of a polymeric material of claim 21.

### Claim 26 (depends on 22)

A process for the production of materials for detection, transfer, amplification and memory of chirality of optically active compounds comprising the use of a polymeric material of claim 22.

### Claim 27 (depends on 22)

A sensor for detection, transfer, amplification and memory of chirality of optically active compounds, containing a polymeric material of claim 22 as a sensing element.

### Claim 28 (depends on 23)

A sensor for detection, transfer, amplification and memory of chirality of optically active compounds, containing a polymeric material of claim 23 as a sensing element.

### Claim 29 (depends on 22)

A device for storage of data based on a polymeric material of claim 22.

### Claim 30 (depends on 23)

A device for storage of data based on a polymeric material of claim 23.