# US 2010/0167032 A1 · Front electrode for pdp

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2010/0167032 A1
- Document ID: US20100167032A1
- Status: Published application
- Kind: A1
- Application number: 12/638,248
- Filed: 2009-12-15
- Published: 2010-07-01
- Earliest claimed: 2008-12-29
- Assignees: E.I.Du Pont De Nemours and Company
- Inventors: Ji-Yeon Lee
- Web page: https://patentgrep.com/patent/US20100167032A1

## CPC

- H01J 11/24: Sustain electrodes or scan electrodes
- H01J 11/12: with main electrodes provided on both sides of the discharge space
- H01J 2211/225: Material of electrodes
- Y10T 428/24942: including components having same physical characteristic in differing degree
- H01J: ELECTRIC DISCHARGE TUBES OR DISCHARGE LAMPS (spark-gaps H01T; electric arc lamps H05B31/00; particle accelerators H05H)
- Y10T: TECHNICAL SUBJECTS COVERED BY FORMER US CLASSIFICATION

## Abstract

A PDP front electrode of this invention comprises a black layer which includes glass with a softening point not greater than 400° C.; and a white layer which includes glass with a softening point not greater than 500° C., and which is formed on the black layer.

## Claims

### Claim 1

A PDP front electrode, comprising:
a black layer which includes glass with a softening point not greater than 400° C.; and
a white layer which includes glass with a softening point not greater than 500° C., and which is formed on the black layer.

### Claim 2 (depends on 1)

The PDP front electrode according to claim 1, wherein the specific gravity of the glass included in the black layer and white layer is not less than 4.0.

### Claim 3 (depends on 1)

The PDP front electrode according to claim 1, wherein the black layer is formed through sintering of a black paste comprising a black powder, glass frit, and photopolymerizable monomer dispersed in a mixture of a resin, photopolymerization initiator, and solvent.

### Claim 4 (depends on 1)

The PDP front electrode according to claim 1, wherein the white layer is formed through sintering of a white paste comprising a conductive powder, glass frit, and photopolymerizable monomer dispersed in a mixture of a resin, photopolymerization initiator, and solvent.

### Claim 5 (depends on 1)

The PDP front electrode according to claim 1, wherein the PDP front electrode is formed on a glass substrate with no transparent electrode interposed.

### Claim 6

A method for forming a PDP front electrode, comprising:
a step of applying a black paste including a glass frit with a softening point not greater than 400° C. on a glass substrate to form a black layer;
a step of drying the black paste that has been applied;
a step of applying a white paste including a glass frit with a softening point not greater than 500° C. on the dried black paste to form a white layer;
a step of drying the white paste that has been applied; and
a step of exposing, developing, and sintering the black paste and white paste.

### Claim 7 (depends on 6)

The method for forming a PDP front electrode according to claim 6, wherein the black paste is a black paste in which a black powder, glass frit, and photopolymerizable monomer are dispersed in a mixture of a resin, photopolymerization initiator, and solvent.

### Claim 8 (depends on 6)

The method for forming a PDP front electrode according to claim 6, wherein the white paste is a white paste in which a conductive powder, glass frit, and photopolymerizable monomer are dispersed in a mixture of a resin, photopolymerization initiator, and solvent.

### Claim 9 (depends on 6)

The method for forming a PDP front electrode according to claim 6, wherein the specific gravity of the glass included in the black layer and white layer is not less than 4.0.

### Claim 10 (depends on 6)

The method for forming a PDP front electrode according to claim 6, wherein the black layer is formed on a glass substrate, with no transparent electrode.