# US 2010/0166975 A1 · Ink-jet printer ink

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2010/0166975 A1
- Document ID: US20100166975A1
- Status: Published application
- Kind: A1
- Application number: 12/649,734
- Filed: 2009-12-30
- Published: 2010-07-01
- Earliest claimed: 2008-12-30
- Assignees: M.G.I. USA, Inc.
- Inventors: Edmond ABERGEL
- Web page: https://patentgrep.com/patent/US20100166975A1

## CPC

- B41M 7/02: Dusting {, e.g. with an anti-offset powder for obtaining raised printing such as by thermogravure (B41M7/0027, B41M7/0036, B41M7/0045, B41M7/0054, B41M7/0072, B41M7/0081, B41M7/009 take precedence); Varnishing (devices for treating the surfaces of sheets, webs, or other articles in connection with printing B41F23/00, B41L23/00)}
- C09D 4/00: Coating compositions, e.g. paints, varnishes or lacquers, based on organic non-macromolecular compounds having at least one polymerisable carbon-to-carbon unsaturated bond {; Coating compositions, based on monomers of macromolecular compounds of groups C09D183/00 - C09D183/16}
- H05K 3/287: {Photosensitive compositions}
- H05K 2203/013: Inkjet printing, e.g. for printing insulating material or resist
- H05K 2203/161: Using chemical substances, e.g. colored or fluorescent, for facilitating optical or visual inspection
- B41M: PRINTING, DUPLICATING, MARKING, OR COPYING PROCESSES; COLOUR PRINTING, (correction of typographical errors B41J; processes for applying transfer pictures or the like B44C1/16; fluid media for correction of typographical errors by coating C09D10/00; printing textiles D06P)
- C09D: COATING COMPOSITIONS, e.g. PAINTS, VARNISHES OR LACQUERS; FILLING PASTES; CHEMICAL PAINT OR INK REMOVERS; INKS; CORRECTING FLUIDS; WOODSTAINS; PASTES OR SOLIDS FOR COLOURING OR PRINTING; USE OF MATERIALS THEREFOR (cosmetics A61K; processes for applying liquids or other fluent materials to surfaces, in general, B05D; staining wood B27K5/02; glazes or vitreous enamels C03C; natural resins, French polish, drying-oils, driers, turpentine, per se, C09F; polishing compositions other than French polish, ski waxes C09G; adhesives or use of materials as adhesives C09J; materials for sealing or packing joints or covers C09K3/10; materials for stopping leaks C09K3/12; processes for the electrolytic or electrophoretic production of coatings C25D)
- H05K: PRINTED CIRCUITS; CASINGS OR CONSTRUCTIONAL DETAILS OF ELECTRIC APPARATUS; MANUFACTURE OF ASSEMBLAGES OF ELECTRICAL COMPONENTS

## Abstract

Ink deposited on a substrate by an ink-jet arrangement to form a protective layer includes hardenable oligomer, hardenable monomer selected from a group including alkoxylated and/or poly-alkoxylated acrylic monomers comprising one or more di- or tri-acrylates, and a photoinitiator. The oligomer has a room temperature viscosity greater than 1 Pa·s. The oligomer to monomer weight ratio is between 1/6 and 1/25. The ink has a room temperature viscosity between 15 and 22 mPa·s and between 5 and 2 mPa·s at 60° C., and a room temperature surface tension between 15 and 28 mN/m. The photoinitiator is activated by a UV source having an appropriate wavelength and intensity.

## Claims

### Claim 1

An ink-jet ink comprising hardenable oligomer, hardenable monomer selected from a group including alkoxylated and/or poly-alkoxylated acrylic monomers having one or more di- or tri-acrylates, and a photoinitiator, the hardenable oligomer having a viscosity greater than 1 Pa·s at room temperature, the oligomer to monomer weight ratio being between 1/6 and 1/25, and the varnish component mixture having a viscosity between 15 and 22 mPa·s at room temperature and between 5 and 2 mPa·s at 60° C., and a surface tension between 15 and 28 mN/m at room temperature.

### Claim 2 (depends on 1)

The ink according to claim 1, wherein the hardenable oligomer is selected from a group having a viscosity greater than 1 Pa·s at room temperature, and wherein the oligomer to monomer weight ratio is between 1/7 and 1/21.

### Claim 3 (depends on 1)

The ink of claim 1, further including a viscosity reducer for facilitating adhesion of the ink to a printed substrate, and/or, an inhibiter of free radicals.

### Claim 4 (depends on 1)

The ink of claim 1, wherein the ink has an electrical conductivity less than 1.5 μSm/cm.

### Claim 5 (depends on 1)

The ink of claim 1, wherein the photoinitiator includes 2-methyl-1-4-methylthiophenyl-2-4-morpholinyl-propanone.

### Claim 6 (depends on 5)

The ink of claim 5, wherein the photoinitiator includes 2-isopropyl-thioxanthone.

### Claim 7 (depends on 1)

The ink of claim 1, wherein the photoinitiator includes 2-isopropyl-thioxanthone.

### Claim 8 (depends on 1)

The ink of claim 1, further including N-vinylcaprolactam to provide adhesion of the ink on the surface of a printed substrate.

### Claim 9 (depends on 1)

The ink of claim 1, wherein the hardenable oligomer having a viscosity greater than 1 Pa·s at room temperature includes aliphatic urethane di-acrylate.

### Claim 10 (depends on 1)

The ink of claim 1, wherein the hardenable oligomer having a viscosity greater than 1 Pa·s at room temperature includes hexa-functional urethane acrylate.

### Claim 11 (depends on 1)

The ink of claim 1, wherein the hardenable oligomer having a viscosity greater than 1 Pa·s at room temperature includes bisphenol A epoxy di-acrylate.

### Claim 12 (depends on 1)

The ink of claim 1 further including an additive with a granulometry less than 50 μm, this additive including at least one of the following:
a flatting agent for obtaining a mat or satin varnish, and/or, flakes for obtaining a flaked varnish,
pigments and/or colorants for obtaining a colored varnish, pigments and/or fluorescent colors for obtaining a fluorescent varnish,
pigments sensitive to black light for obtaining a varnish for optical purposes, and
colorants sensitive to black light for obtaining a varnish for optical purposes.

### Claim 13 (depends on 1)

The ink of claim 1, wherein the ink has a granulometry suited for passing through a nozzle when ink is deposited by an ink-jet on a printed substrate.

### Claim 14 (depends on 3)

A method of producing the ink of claim 3, the method comprising:
mixing the viscosity reducer with the inhibiter of free radicals, and the photoinitiator at a temperature between 150 and 300° C.,
cooling the resulting mixture to room temperature,
adding under agitation at least one hardenable oligomer according to the ink composition, and at least one hardenable monomer according to the ink composition.

### Claim 15 (depends on 14)

The method of claim 14, further including filtering the mixture resulting from the cooling and adding under agitation according to a granulometry so the mixture resulting from the cooling and adding under agitation can pass through a nozzle during deposition by the ink-jet nozzle on the printed substrate.

### Claim 16 (depends on 1)

The ink of claim 1 wherein the room temperature is in the range of 23-25° C.

### Claim 17 (depends on 1)

A method of depositing a protective layer on a substrate comprising projecting the ink-jet ink of claim 1 through a non-impact ink-jet nozzle arrangement onto the substrate and then irradiating the ink on the substrate with ultraviolet energy to which the photoinitiator is responsive.

### Claim 18 (depends on 17)

The method of claim 17 wherein the nozzle is vibrated by a piezoelectric actuator.

### Claim 19 (depends on 1)

Apparatus for depositing a protective layer on a substrate comprising an ink-jet printer having a nonimpact ink-jet nozzle arrangement, a supply of the ink-jet ink of claim 1, a fluid flow arrangement for supplying the ink-jet ink to the ink-jet nozzle arrangement for enabling the ink-jet ink to be projected onto the substrate, and a UV source positioned to irradiate the ink projected onto the substrate, the UV source being arranged to emit UV radiation having a wavelength and intensity to activate the photoinitiator.

### Claim 20 (depends on 19)

The apparatus of claim 19 wherein the nozzle is arranged to be vibrated by a piezoelectric actuator.

### Claim 21 (depends on 1)

The ink of claim 1 wherein the room temperature is 25° C.