# US 2010/0166966 A1 · Sulfonated polyether ether ketone ketone, film utilizing the same, and method for manufacturing the same

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2010/0166966 A1
- Document ID: US20100166966A1
- Status: Published application
- Kind: A1
- Application number: 12/477,108
- Filed: 2009-06-02
- Published: 2010-07-01
- Earliest claimed: 2008-12-26
- Assignees: Industrial Technology Research Institute; National Central University
- Inventors: Chung-Liang Chang; Ming-Chou Chen; Ko-Lun Hsu; Hsing-Chieh Li; Chi-Han Hsieh; Peter Po-Jen Chu
- Web page: https://patentgrep.com/patent/US20100166966A1

## CPC

- H01M 8/1018: Polymeric electrolyte materials
- B01D 67/0006: {by chemical reactions (in-situ polymerisation, polycondensation, cross-linking or reaction for manufacturing composite membranes B01D69/125)}
- B01D 69/02: characterised by their properties
- B01D 71/5222: {Polyetherketone, polyetheretherketone, or polyaryletherketone}
- B01D 71/82: characterised by the presence of specified groups, e.g. introduced by chemical after-treatment
- C08G 65/4056: {(I) or (II) containing sulfur (as the sulfone group C08G75/23)}
- C08J 5/18: Manufacture of films or sheets
- H01M 8/1025: having only carbon and oxygen, e.g. polyethers, sulfonated polyetheretherketones [S-PEEK], sulfonated polysaccharides, sulfonated celluloses or sulfonated polyesters
- H01M 8/1081: starting from solutions, dispersions or slurries exclusively of polymers
- H01M 8/1088: Chemical modification, e.g. sulfonation
- B01D 2323/30: Cross-linking
- B01D 2323/34: Use of radiation
- B01D 2325/24: Mechanical properties, e.g. strength
- B01D 2325/30: Chemical resistance
- C08J 2371/10: from phenols
- H01M 8/1037: having silicon, e.g. sulfonated crosslinked polydimethylsiloxanes
- H01M 2300/0082: Organic polymers
- Y02E 60/50: Fuel cells
- Y02P 70/50: Manufacturing or production processes characterised by the final manufactured product
- H01M: PROCESSES OR MEANS, e.g. BATTERIES, FOR THE DIRECT CONVERSION OF CHEMICAL ENERGY INTO ELECTRICAL ENERGY
- B01D: SEPARATION (separating solids from solids by wet methods B03B, B03D; by pneumatic jigs or tables B03B; by other dry methods B07; magnetic or electrostatic separation of solid materials from solid materials or fluids, separation by high-voltage electric fields B03C; centrifuges, vortex apparatus B04; presses per se for squeezing-out liquid from liquid-containing material B30B9/02; treatment of water C02F, e.g. softening by ion-exchange C02F1/42; {arrangements of air intake cleaners in gas turbine plants F02C7/05} ; arrangements or mounting of filters in air-conditioning, air-humidification or ventilation F24F13/28)
- C08G: MACROMOLECULAR COMPOUNDS OBTAINED OTHERWISE THAN BY REACTIONS ONLY INVOLVING UNSATURATED CARBON-TO-CARBON BONDS
- C08J: WORKING-UP; GENERAL PROCESSES OF COMPOUNDING; AFTER-TREATMENT NOT COVERED BY SUBCLASSES C08B, C08C, C08F, C08G or C08H (working, e.g. shaping, of plastics B29)
- Y02E: REDUCTION OF GREENHOUSE GAS [GHG] EMISSIONS, RELATED TO ENERGY GENERATION, TRANSMISSION OR DISTRIBUTION
- Y02P: CLIMATE CHANGE MITIGATION TECHNOLOGIES IN THE PRODUCTION OR PROCESSING OF GOODS

## Abstract

A series of crosslinkable sulfonated poly(ether ketone)s containing cycloalkenyl groups were synthesized by aromatic nucleophilic substitution reaction. To decrease the swelling of fuel cell membranes, crosslinking of theses polymers by radical polymerization has been explored. These polymeric films exhibit good thermal and oxidative stability, and good dimensional stability in hot water. The proton conductivity of one example at room temperature is 7.52*10−2 S/cm. The results showed that these materials containing cycloalkenyl groups are possible inexpensive candidate materials for proton exchange membranes in fuel cell applications.

## Claims

### Claim 1

A sulfonated polyether ether ketone having a formula:
wherein R has a formula:
Ar is independently selected from phenyl, naphthyl, anthryl, or phenanthryl;
n is an integral of 0 to 2; and
a and b have a ratio of 95:5 to 70:30.

### Claim 2 (depends on 1)

The sulfonated polyether ether ketone as claimed in claim 1 has a formula:

### Claim 3 (depends on 1)

A film formula, comprising:
the sulfonated polyether ether ketone as claimed in claim 1, and
a radical initiator.

### Claim 4 (depends on 3)

The film formula as claimed in claim 3, wherein the radical initiator comprises a photo initiator or a thermal initiator.

### Claim 5 (depends on 3)

The film formula as claimed in claim 3, further comprising a double-bond compound and/or a triple-bond compound.

### Claim 6 (depends on 5)

The film formula as claimed in claim 5, wherein the double-bond compound comprises silane, divinyl benzene, or alkenyl oligomer.

### Claim 7 (depends on 3)

A method for manufacturing a film, comprising:
dissolving the film formula as claimed in claim 3 in a solvent to form a solution;
forming the solution on a substrate and providing an energy to radical crosslink the sulfonated polyether ether ketone; and
removing the solvent to form a film.

### Claim 8 (depends on 7)

The method as claimed in claim 7, wherein the energy comprises light or heat.

### Claim 9 (depends on 7)

The method as claimed in claim 7, further comprising a step of adding a double-bond compound and/or a triple-bond compound to the solution, wherein the sulfonated polyether ether ketone, the double-bond compound and/or the triple-bond compound are radical crosslinked by the energy.

### Claim 10 (depends on 1)

A film comprising the crosslinked polyether ether ketone as claimed in claim 1.

### Claim 11 (depends on 10)

The film as claimed in claim 10, further crosslinking a double-bond compound and/or a triple-bond compound.

### Claim 12 (depends on 11)

The film as claimed in claim 11, wherein the double-bond compound comprises silane, divinyl benzene, or alkenyl oligomer.