# US 2010/0166961 A1 · Production of high porosity open-cell membranes

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2010/0166961 A1
- Document ID: US20100166961A1
- Status: Published application
- Kind: A1
- Application number: 12/537,218
- Filed: 2009-08-06
- Published: 2010-07-01
- Earliest claimed: 2004-01-20
- Inventors: Kirby W. Beard
- Web page: https://patentgrep.com/patent/US20100166961A1

## CPC

- B01D 69/02: characterised by their properties
- B01D 67/00091: {by evaporation}
- B01D 71/301: {Polyvinylchloride}
- B01D 71/34: Polyvinylidene fluoride
- H01M 50/414: Synthetic resins, e.g. thermoplastics or thermosetting resins
- B01D 2323/081: Heating
- B01D 2325/20: Specific permeability or cut-off range
- B01D 2325/26: Electrical properties
- H01M 50/491: Porosity
- H01M 50/494: Tensile strength
- Y02E 60/10: Energy storage using batteries
- B01D: SEPARATION (separating solids from solids by wet methods B03B, B03D; by pneumatic jigs or tables B03B; by other dry methods B07; magnetic or electrostatic separation of solid materials from solid materials or fluids, separation by high-voltage electric fields B03C; centrifuges, vortex apparatus B04; presses per se for squeezing-out liquid from liquid-containing material B30B9/02; treatment of water C02F, e.g. softening by ion-exchange C02F1/42; {arrangements of air intake cleaners in gas turbine plants F02C7/05} ; arrangements or mounting of filters in air-conditioning, air-humidification or ventilation F24F13/28)
- H01M: PROCESSES OR MEANS, e.g. BATTERIES, FOR THE DIRECT CONVERSION OF CHEMICAL ENERGY INTO ELECTRICAL ENERGY
- Y02E: REDUCTION OF GREENHOUSE GAS [GHG] EMISSIONS, RELATED TO ENERGY GENERATION, TRANSMISSION OR DISTRIBUTION

## Abstract

A method for forming an open celled membrane. A gelled polymer is formed of a polymer having a known polymer interfacial tension and a known polymer melting point. A first liquid into which the polymer is soluble, the first liquid being selected to have a first liquid interfacial tension to be 95% or less than the polymer interfacial tension is mixed with a second liquid that is miscible in the first liquid to form a mixture. The second liquid is selected to have a second liquid interfacial tension to be 105% or greater than the polymer interfacial tension. The polymer is dissolved into the mixture to form a saturated solution. The saturated solution reaches a solution forming temperature which is less than the polymer melting point. The saturated solution is spread on a substrate. The first liquid from the saturated solution to form the gelled polymer.

## Claims

### Claim 1

A method for forming a gelled polymer, the method comprising:
providing a polymer having a known polymer interfacial tension and a known polymer melting point;
providing a first liquid into which the polymer is soluble, the first liquid being selected to have a first liquid interfacial tension to be 95% or less than the polymer interfacial tension;
mixing a second liquid that is miscible in the first liquid to form a mixture, the second liquid being selected to have a second liquid interfacial tension to be 105% or greater than the polymer interfacial tension;
dissolving the polymer into the mixture to form a saturated solution;
causing the saturated solution to reach a solution forming temperature less than the polymer melting point;
forming the saturated solution on a substrate; and
selectively removing the first liquid from the saturated solution to form the gelled polymer.

### Claim 2 (depends on 1)

The method of claim 1, wherein:
the polymer is PVDF, having an interfacial tension of about 35 dynes/cm;
the first liquid is selected from a group consisting of methyl formate at about 24.4 dynes/cm, acetone (2-propanone) at about 23.5 dynes/cm, methyl acetate at about 24.7 dynes/cm, tetrahydrofuran at about 26.4 dynes/cm, ethyl acetate at about 23.4 dynes/cm, methyl ethyl ketone (2-butanone) at about 24 dynes/cm, acetonitrile at about 29 dynes/cm, dimethyl carbonate at about 31.9 dynes/cm, 1,2-dioxane at about 32 dynes/cm, toluene at about 28.4 dynes/cm, and methyl isobutyl ketone at about 23.4 dynes/cm;
the second liquid is liquid miscible with the first liquid and selected from a group consisting of nitromethane at about 37 dynes/cm, bromobenzene at about 37 dynes/cm, formic acid at about 38 dynes/cm, pyridine at about 38 dynes/cm, ethylene bromide at about 38 dynes/cm, 3-furaldehyde at about 40 dynes/cm, bromine at about 42 dynes/cm, tribromomethane at about 42 dynes/cm, quinoline at about 43 dynes/cm, nitric acid (69%) at about 43 dynes/cm, and water at about 72.5 dynes/cm;
wherein the solution forming temperature is between 20 and 90° C.; and
and the film forming temperature is selected to be less than 177° C.

### Claim 3 (depends on 1)

The method of claim 1 wherein the selectively removing the first liquid includes reducing an ambient pressure around the saturated solution sufficiently to shift a first liquid boiling point.

### Claim 4 (depends on 1)

The method of claim 1 wherein the selective removing the first liquid includes heating the saturated solution to reach a removal temperature distinct from the solution forming temperature and less than 177° C.

### Claim 5 (depends on 1)

The method of claim 1, wherein the saturated solution is a stable saturated solution.

### Claim 6 (depends on 1)

The method of claim 1, wherein the removing the first liquid shifts the saturated solution to a supersaturated solution.

### Claim 7 (depends on 1)

The method of claim 1 further including the causing the saturated solution to reach a film forming temperature that is less than the second temperature whereby the polymer gel is formed.

### Claim 8 (depends on 1)

The method of claim 1, wherein the removal of the first liquid includes transitioning the saturated solution into a supersaturated solution.

### Claim 9 (depends on 1)

The method of claim 1 wherein the removal of the first liquid occurs by one of a group consisting of cooling, forced air drying, extended dwell time, first liquid evaporation, vibration, and ultrasonics.

### Claim 10 (depends on 1)

The method of claim 1 further including the removal of the second liquid from the gelled polymer to form a porous membrane, the removal occurring at a second liquid removal temperature less than 100°

### Claim 11 (depends on 10)

The method of claim 10, wherein the second liquid removal temperature is less than 80° C.

### Claim 12 (depends on 1)

The method of claim 1, wherein the polymer is selected from a group consisting of polyvinylidene fluoride, polyvinylidene fluoridehexafluoropropylene copolymer, polyvinyl chloride, polyvinylidene chloride, chlorinated polyvinyl chloride, polymethyl methacrylate, and mixtures of two or more of these semi-crystalline polymers.