# US 2010/0165454 A1 · Method for Manufacturing Gradient-Index Optical Element Having Infrared Absorbing Ability

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2010/0165454 A1
- Document ID: US20100165454A1
- Status: Published application
- Kind: A1
- Application number: 11/990,005
- Filed: 2006-08-08
- Published: 2010-07-01
- Earliest claimed: 2005-08-08
- Assignees: Isuzu Glass Co., Ltd.; National Institute of Advanced Industrial Science and Technology
- Inventors: Tatsuya Suetsugu; Kazuhisa Kimura; Takeshi Ohtani; Naoko Kaga; Naoki Kikuchi; Naoto Yamashita; Yukiko Morizane; Toshihiko Einishi; Kohei Kadono
- Web page: https://patentgrep.com/patent/US20100165454A1

## CPC

- G02B 1/00: Optical elements characterised by the material of which they are made; Optical coatings for optical elements
- C03C 3/087: containing calcium oxide, e.g. common sheet or container glass
- C03C 3/17: containing aluminium or beryllium
- C03C 4/082: {for infrared absorbing glass}
- C03C 21/008: {in solid phase, e.g. using pastes, powders}
- G02B 3/0087: {with index gradient}
- G02B 5/226: {Glass filters}
- G02B: OPTICAL ELEMENTS, SYSTEMS OR APPARATUS
- C03C: CHEMICAL COMPOSITION OF GLASSES, GLAZES OR VITREOUS ENAMELS; SURFACE TREATMENT OF GLASS; SURFACE TREATMENT OF FIBRES OR FILAMENTS MADE FROM GLASS, MINERALS OR SLAGS; JOINING GLASS TO GLASS OR OTHER MATERIALS

## Abstract

A method of readily producing a gradient optical element having infrared absorbing ability by easily forming a refractive index distribution in a desired portion of a glass substrate having infrared absorbing ability without requiring a specific treatment atmosphere nor using a molten salt. More specifically, the present invention provides a method for producing a gradient-index optical element having infrared absorbing ability, the method comprising applying a paste containing an organic resin, an organic solvent, and at least one compound selected from the group consisting of lithium compounds, potassium compounds, rubidium compounds, cesium compounds, silver compounds, copper compounds, and thallium compounds onto a glass substrate containing an alkali metal component, at least one member selected from the group consisting of iron, copper, cobalt and vanadium, and over 3 wt. % of iron, when contained singly among iron, copper, cobalt and vanadium, on an Fe2O3 basis, taking the total weight of the glass as 100 wt. %, and heating the glass substrate at a temperature below the softening temperature of the glass substrate.

## Claims

### Claim 1

A method for producing a gradient-index optical element having infrared absorbing ability, the method comprising applying a paste containing an organic resin, an organic solvent, and at least one compound selected from the group consisting of lithium compounds, potassium compounds, rubidium compounds, cesium compounds, silver compounds, copper compounds, and thallium compounds onto a glass substrate containing an alkali metal component, at least one member selected from the group consisting of iron, copper, cobalt and vanadium, and over 3 wt. % of iron, when contained singly among iron, copper, cobalt and vanadium, on an Fe2O3 basis, taking the total weight of the glass as 100 wt. %, and heating the glass substrate at a temperature below the softening temperature of the glass substrate.

### Claim 2 (depends on 1)

The production method of claim 1, wherein the glass substrate has an infrared transmittance of 80% or lower at a thickness of 1 mm.

### Claim 3 (depends on 1)

The production method of claim 1, wherein the glass substrate is made of glass containing at least 2 wt. % of an alkali metal component on an oxide basis, the glass being a silicate glass, borosilicate glass, phosphate glass, or fluorophosphate glass.

### Claim 4 (depends on 1)

The production method of claim 1, wherein the glass substrate is made of a phosphate glass containing each component below as an oxide composition, taking the total glass weight as 100 wt. %,
(1) 51 to 60 wt. % of P2O5,
(2) 17 to 33 wt. % of ZnO,
(3) 1 to 6 wt. % of Al2O3,
(4) 0 to 5 wt. % of Li2O, 0 to 10 wt. % of Na2O and 0 to 15 wt. % of K2O, with the total weight of Li2O, Na2O and K2O being 5 to 17 wt. %,
(5) 0 to 7 wt. % of MgO, and 0 to 7 wt. % of CaO, with the total weight of MgO and CaO being 1 to 12 wt. %,
(6) 0 to 5 wt. % of B2O3,
(7) 0 to 10 wt. % of at least one member selected from the group consisting of Y2O3, La2O3, Ta2O5 and WO3, and
(8) 0.2 to 8 wt. % of CuO.

### Claim 5 (depends on 1)

The production method of claim 1, wherein the glass substrate is made of a phosphate glass containing each component below as an oxide composition, taking the total glass weight as 100 wt. %,
(1) 60 to 80 wt. % of P2O5,
(2) 5 to 12 wt. % of ZnO,
(3) 5 to 10 wt. % of Al2O3,
(4) 0 to 5 wt. % of Li2O, 0 to 8 wt. % of Na2O, 7 to 15 wt. % of K2O and 0 to 8 wt. % of Cs2O, with the total weight of Li2O, Na2O, K2O and Cs2O being 7 to 15 wt. %,
(5) 0 to 10 wt. % of MgO and 0 to 10 wt. % of CaO, the total weight of MgO and CaO being 3 to 10 wt. %,
(6) 0 to 1.5 wt. % of B2O3 and 0 to 1.5 wt. % of SiO2, with the total weight of B2O3 and SiO2 being 0.5 to 2 wt. %, and
(7) 0.2 to 10 wt. % of CuO.

### Claim 6 (depends on 1)

The production method of claim 1, wherein the glass substrate further contains 0 to 5 wt. % of at least one member selected from the group consisting of BaO, SrO, Y2O3, La2O3, ZrO2, Ta2O5, Nb2O5, TiO2 and Gd2O3

### Claim 7 (depends on 1)

A gradient-index optical element having infrared absorbing ability produced by the production method of claim 1.

### Claim 8 (depends on 7)

The gradient-index optical element of claim 7, wherein the element is a lens or lens array.

### Claim 9 (depends on 7)

The gradient-index optical element of claim 7, wherein the element is a camera lens or camera lens array.