# US 2010/0165440 A1 · Electrochromic Device And Method For Making Electrochromic Device

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2010/0165440 A1
- Document ID: US20100165440A1
- Status: Published application
- Kind: A1
- Application number: 12/347,953
- Filed: 2008-12-31
- Published: 2010-07-01
- Earliest claimed: 2008-12-31
- Assignees: View, Inc.
- Inventors: Paul P. Nguyen; Shiwei Liu
- Web page: https://patentgrep.com/patent/US20100165440A1

## CPC

- G02F 1/155: Electrodes
- C23C 14/083: {of refractory metals or yttrium}
- C23C 14/086: {of zinc, germanium, cadmium, indium, tin, thallium or bismuth}
- C23C 14/18: on other inorganic substrates
- G02F 2001/1555: {Counter electrode}
- G02F: OPTICAL DEVICES OR ARRANGEMENTS FOR THE CONTROL OF LIGHT BY MODIFICATION OF THE OPTICAL PROPERTIES OF THE MEDIA OF THE ELEMENTS INVOLVED THEREIN; NON-LINEAR OPTICS; FREQUENCY-CHANGING OF LIGHT; OPTICAL LOGIC ELEMENTS; OPTICAL ANALOGUE/DIGITAL CONVERTERS
- C23C: COATING METALLIC MATERIAL; COATING MATERIAL WITH METALLIC MATERIAL; SURFACE TREATMENT OF METALLIC MATERIAL BY DIFFUSION INTO THE SURFACE, BY CHEMICAL CONVERSION OR SUBSTITUTION; COATING BY VACUUM EVAPORATION, BY SPUTTERING, BY ION IMPLANTATION OR BY CHEMICAL VAPOUR DEPOSITION, IN GENERAL (making metal-coated products by extrusion B21C23/22; covering with metal by connecting pre-existing layers to articles, see the relevant places, e.g. B21D39/00, B23K; metallising of glass C03C; metallising mortars, concrete, artificial stone, ceramics or natural stone C04B41/00; enamelling of, or applying a vitreous layer to, metals C23D; treating metal surfaces or coating of metals by electrolysis or electrophoresis C25D; single-crystal film growth C30B; by metallising textiles D06M11/83; decorating textiles by locally metallising D06Q1/04)

## Abstract

A method for lithiating an electrochromic device comprise forming a first transparent conductive layer on a substrate, forming an electrochromic structure on the first transparent conductive layer, forming a second transparent conductive layer on the electrochromic structure, and lithiating the electrochromic structure through the second transparent conductive layer. In one exemplary embodiment lithiating the electrochromic structure comprises lithiating the electrochromic structure at a temperature range of between about room temperature and about 500 C for the duration of the lithiation process. In another exemplary embodiment, lithiating the electrochromic structure further comprises lithiating the electrochromic structure by using at least one of sputtering, evaporation, laser ablation and exposure to a lithium salt. The electrochromic device can be configured in either a “forward” or a “reverse” stack configuration.

## Claims

### Claim 1

A method, comprising:
forming a first transparent conductive layer on a substrate;
forming an electrochromic structure on the first transparent conductive layer;
forming a second transparent conductive layer on the electrochromic structure; and
lithiating the electrochromic structure through the second transparent conductive layer.

### Claim 2 (depends on 1)

The method according to claim 1, wherein the electrochromic structure comprises a counter electrode (CE) on the first side and an electrochromic (EC) electrode on the second side, the first side of the electrochromic structure being formed on the first transparent conductive layer, and the second transparent conductive layer being formed on the second side of the electrochromic structure, and
wherein lithiating the electrochromic structure through the second transparent conductive layer comprises lithiating the electrochromic (EC) electrode of the electrochromic structure.

### Claim 3 (depends on 2)

The method according to claim 2, wherein the electrochromic structure further comprises an ion conductor (IC) layer between the counter electrode (CE) and the electrochromic (EC) electrode,
the method forming further comprising directly lithiating at least one of the counter electrode (CE) and the ion conductor (IC) layer.

### Claim 4 (depends on 1)

The method according to claim 1, wherein the electrochromic structure comprises an electrochromic (EC) electrode on the first side and a counter electrode (CE) on the second side, the first side of the electrochromic structure being formed on the first transparent conductive layer, and the second transparent conductive layer being formed on the second side of the electrochromic structure, and
wherein lithiating the electrochromic structure through the second transparent conductive layer comprises lithiating the counter electrode (CE) of the electrochromic structure.

### Claim 5 (depends on 4)

The method according to claim 4, wherein the electrochromic structure further comprises an ion conductor (IC) layer between the electrochromic layer (EC) and the counter electrode (CE),
the method further comprising directly lithiating at least one of the electrochromic (EC) electrode and the ion conductor (IC) layer.

### Claim 6 (depends on 1)

The method according to claim 1, wherein lithiating the electrochromic structure comprises lithiating the electrochromic structure at a temperature range of between about room temperature and about 500 C for the duration of the lithiation process.

### Claim 7 (depends on 6)

The method according to claim 6, wherein lithiating the electrochromic structure further comprises lithiating the electrochromic structure by using at least one of sputtering, evaporation, laser ablation and exposure to a lithium salt.

### Claim 8

An electrochromic device formed by a method comprising:
forming a first transparent conductive layer on a substrate;
forming an electrochromic structure on the first transparent conductive layer;
forming a second transparent conductive layer on the electrochromic structure; and
lithiating the electrochromic structure through the second transparent conductive layer.

### Claim 9 (depends on 8)

The electrochromic device according to claim 8, wherein the electrochromic structure comprises a counter electrode (CE) on the first side and an electrochromic (EC) electrode on the second side, the first side of the electrochromic structure being formed on the first transparent conductive layer, and the second transparent conductive layer being formed on the second side of the electrochromic structure, and
wherein lithiating the electrochromic structure through the second transparent conductive layer comprises lithiating the electrochromic (EC) electrode of the electrochromic structure.

### Claim 10 (depends on 9)

The electrochromic device according to claim 9, wherein the electrochromic structure further comprises an ion conductor (IC) layer between the counter electrode (CE) and the electrochromic (EC) electrode,
the method forming the electrochromic device further comprising directly lithiating at least one of the counter electrode (CE) and the ion conductor (IC) layer.

### Claim 11 (depends on 10)

The electrochromic device according to claim 10, wherein the electrochromic structure comprises an electrochromic (EC) electrode on the first side and a counter electrode (CE) on the second side, the first side of the electrochromic structure being formed on the first transparent conductive layer, and the second transparent conductive layer being formed on the second side of the electrochromic structure, and
wherein lithiating the electrochromic structure through the second transparent conductive layer comprises lithiating the counter electrode (CE) of the electrochromic structure.

### Claim 12 (depends on 11)

The electrochromic device according to claim 11, wherein the electrochromic structure further comprises an ion conductor (IC) layer between the electrochromic layer (EC) and the counter electrode (CE),
the method forming the electrochromic device further comprising directly lithiating at least one of the electrochromic (EC) electrode and the ion conductor (IC) layer.

### Claim 13 (depends on 8)

The electrochromic device according to claim 8, wherein lithiating the electrochromic structure comprises lithiating the electrochromic structure at a temperature range of between about room temperature and about 500 C for the duration of the lithiation process.

### Claim 14 (depends on 13)

The electrochromic device according to claim 13, wherein lithiating the electrochromic structure further comprises lithiating the electrochromic structure by using at least one of sputtering, evaporation, laser ablation and exposure to a lithium salt.

### Claim 15 (depends on 8)

The electrochromic device according to claim 8, wherein the electrochromic device is part of an Insulated Glass Unit (IGU), and wherein a percentage transmission of the electrochromic device in a bleached state is greater than or equal to about 65% at a wavelength of about 600 nm.

### Claim 16 (depends on 8)

The electrochromic device according to claim 8, wherein a percentage transmission of the electrochromic device in a colored state is less than or equal to about 5% over a wavelength range of about 380 nm to about 1050 nm.