# US 2010/0164663 A1 · Permanent magnet and a manufacturing method thereof

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2010/0164663 A1
- Document ID: US20100164663A1
- Status: Published application
- Kind: A1
- Application number: 12/438,057
- Filed: 2007-08-22
- Published: 2010-07-01
- Earliest claimed: 2006-08-23
- Assignees: Ulvac, Inc.
- Inventors: Hiroshi Nagata; Yoshinori Shingaki
- Web page: https://patentgrep.com/patent/US20100164663A1

## CPC

- C22C 38/005: {containing rare earths, i.e. Sc, Y, Lanthanides}
- C22C 38/06: containing aluminium
- C22C 38/12: containing tungsten, tantalum, molybdenum, vanadium, or niobium
- C22C 38/14: containing titanium or zirconium
- H01F 1/0577: {sintered}
- H01F 41/0293: {diffusion of rare earth elements, e.g. Tb, Dy or Ho, into permanent magnets}
- C22C: ALLOYS (treatment of alloys C21D, C22F)
- H01F: MAGNETS; INDUCTANCES; TRANSFORMERS; SELECTION OF MATERIALS FOR THEIR MAGNETIC PROPERTIES

## Abstract

[Object] One object of the present invention is to provide a method for manufacturing a permanent magnet which can effectively improving the magnetizing properties and coercive force with efficiently diffusing Dy into grain boundary phases without deteriorating a surface of sintered magnet of Nd—Fe—B family and does not require any subsequent working process. [Means for achieving the object] Sintered magnet S of Nd—Fe—B family and Dy are arranged in a processing chamber 20 apart from each other. Then Dy is evaporated by heating the processing chamber 20 under a reduced pressure condition to evaporate Dy with elevating the temperature of sintered magnet S to a predetermined temperature and to supply and deposit evaporated Dy atoms onto the surface of sintered magnet S. During which the supplying amount of Dy atoms onto the sintered magnet S is controlled so as to diffuse and homogeneously penetrate them into the grain boundary phases of sintered magnet before Dy layer is formed on the surface of sintered magnet.

## Claims

### Claim 1

Method for manufacturing a permanent magnet comprising steps of heating a sintered magnet of Fe—B-rare earth elements family arranged in a processing chamber to a predetermined temperature and evaporating metal evaporating material including at least one of Dy and Tb arranged in said processing chamber of another processing chamber; depositing evaporated metal atoms onto a surface of the sintered magnet with controlling a supplying amount of the metal atoms into grain boundary phases of the sintered magnet before formation of thin film of the metal evaporating material on the surface of the sintered magnet.

### Claim 2 (depends on 1)

Method for manufacturing a permanent magnet of claim 1 wherein said processing chamber is heated to a temperature in a range of 800° C.˜1050° C. under a vacuum condition when the sintered magnet of Fe—B-rare earth elements family and the metal evaporating material having a primary component of Dy are arranged in the processing chamber.

### Claim 3 (depends on 1)

Method for manufacturing a permanent magnet of claim 1 wherein said processing chamber is heated to a temperature in a range of 900° C.˜1150° C. under a vacuum condition when the sintered magnet of Fe—B-rare earth elements family and the metal evaporating material having a primary component of Tb are arranged in the processing chamber.

### Claim 4 (depends on 1)

Method for manufacturing a permanent magnet of claim 1 comprising steps of arranging the sintered magnet of Fe—B-rare earth elements family in the processing chamber and heating the sintered magnet to a temperature in a range of 800° C.˜1100° C.; heating and evaporating the metal evaporating material including at least one of Dy and Tb arranged in said processing chamber or another processing chamber; and supplying and depositing the evaporated metal atoms onto the surface of the sintered magnet.

### Claim 5 (depends on 1)

Method for manufacturing a permanent magnet of claim 1 comprising steps of arranging the sintered magnet of Fe—B-rare earth elements family in the processing chamber; heating and evaporating the metal evaporating material including at least one of Dy and Tb arranged in said processing chamber or another processing chamber to a temperature in a range of 800° C.˜1200° C. after heating and holding the sintered magnet to a predetermined temperature; and supplying and depositing the evaporated metal atoms onto the surface of the sintered magnet.

### Claim 6 (depends on 1)

Method for manufacturing a permanent magnet of claim 1 wherein the sintered magnet and the metal evaporating material are arranged apart from each other when the sintered magnet and the metal evaporating material are arranged in the same processing chamber.

### Claim 7 (depends on 1)

Method for manufacturing a permanent magnet of claim 1 wherein a ratio of the total surface area of the metal evaporating material to the total surface area of the sintered magnet arranged in the processing chamber is set in a range of 1×10−4˜2×103.

### Claim 8 (depends on 1)

Method for manufacturing a permanent magnet of claim 1 wherein the supplying amount of the metal atoms is controlled by changing the specific surface area of the metal evaporating material arranged in the processing chamber to increase and decrease the amount of evaporation of the metal evaporating material under a constant temperature.

### Claim 9 (depends on 1)

Method for manufacturing a permanent magnet of claim 1 wherein the pressure in the processing chamber is kept at a predetermined reduced pressure before heating of the processing chamber containing the sintered magnet.

### Claim 10 (depends on 9)

Method for manufacturing a permanent magnet of claim 9 wherein the temperature in the processing chamber is kept at a predetermined temperature after reducing the pressure in the process chamber to a predetermined pressure.

### Claim 11 (depends on 1)

Method for manufacturing a permanent magnet of claim 1 wherein the surface of the sintered magnet is cleaned with using plasma before heating of the processing chamber containing the sintered magnet.

### Claim 12 (depends on 1)

Method for manufacturing a permanent magnet of claim 1 wherein heat treatment of the sintered magnet is performed at a temperature lower than said temperature after diffusing the metal atoms into grain boundary phases of the sintered magnet.

### Claim 13 (depends on 1)

Method for manufacturing a permanent magnet of claim 1 wherein the sintered magnet has an average diameter of grain of 1 μm˜5 μm or 7 μm˜20 μm.

### Claim 14 (depends on 1)

Method for manufacturing a permanent magnet of claim 1 wherein the sintered magnet does not contain Co.

### Claim 15

A permanent magnet comprising a sintered magnet of Fe—B-rare earth elements family and manufactured by evaporating metal evaporating material including at least one of Dy and Tb, depositing evaporated metal atoms onto a surface of the sintered magnet with controlling a supplying amount of the metal atoms; and diffusing the deposited metal atoms into grain boundary phases of the sintered magnet before formation of thin film of the metal evaporating material on the surface of the sintered magnet.

### Claim 16 (depends on 15)

A permanent magnet of claim 15 wherein the sintered magnet has an average diameter of grain of 1 μm˜5 μm or 7 μm˜20 μm.

### Claim 17 (depends on 15)

A permanent magnet of claim 15 wherein the sintered magnet does not contain Co.

### Claim 18 (depends on 16)

A permanent magnet of claim 16 wherein the sintered magnet does not contain Co.