- Number: US 2010/0164308 A1
- Document ID: US20100164308A1
- Status: Published application
- Kind: A1
- Application number: 12/598,848
- Filed: 2007-06-01
- Published: 2010-07-01
- Earliest claimed: 2007-06-01
- Assignees: Vacuumschmelze GmbH & Co. KG
- Inventors: Lothar Zapf
- Web page: https://patentgrep.com/patent/US20100164308A1

## CPC

- H02K 15/03: having permanent magnets
- H01F 41/0253: {for manufacturing permanent magnets}
- H02K 1/276: Magnets embedded in the magnetic core, e.g. interior permanent magnets [IPM]
- Y10T 29/49012: Rotor
- H02K: DYNAMO-ELECTRIC MACHINES (dynamo-electric relays H01H53/00; conversion of DC or AC input power into surge output power {H03K3/53})
- H01F: MAGNETS; INDUCTANCES; TRANSFORMERS; SELECTION OF MATERIALS FOR THEIR MAGNETIC PROPERTIES
- Y10T: TECHNICAL SUBJECTS COVERED BY FORMER US CLASSIFICATION

## Abstract

The invention relates to a method for connecting a first joining partner (1) to a second joining partner (2). After provision of the first joining partner (1) and the second joining partner (2), a lacquer layer (11) is applied to the first joining partner (1). Then the first joining partner (1) and the second joining partner (2) are saturated together with an impregnating resin (8). The lacquer layer (11) is produced from a lacquer composition based on an epoxy resin mixture, a curing accelerator, a silane-based, epoxy-functional bonding agent, and a solvent. The epoxy resin mixture has 10 wt.-% to 94 wt.-% of at least one solid epoxy resin with a maximum epoxy count of 2 Eg/kg, 1 wt.-% to 50 wt.-% of at least one solid, multifunctional epoxy resin with an epoxy count >4 Eg/kg, and 5 wt.-% to 40 wt.-% of a phenol and/or kresol novolak with a melting point >30° C. After impregnation, the viscosity of the impregnating resin (8) is reduced such that the first joining partner (1) and the second joining partner (2) are connected to one another.

## Claims

### Claim 1

A method for bonding a first bonding partner to a second bonding partner, comprising:
providing the first bonding partner and the second bonding partner;
applying to the first bonding partner a coating comprising a lacquer composition, comprising
an epoxy resin mixture, comprising
10 to 94% by weight, based on the weight of the epoxy resin mixture, of at least one solid epoxy resin with an epoxide number not exceeding 2 Eq/kg,
1 to 50% by weight, based on the weight of the epoxy resin mixture, of at least one solid multifunctional epoxy resin with an epoxide number >4 Eq/kg, and
5 to 40% by weight, based on the weight of the epoxy resin mixture, of a phenol and/or cresol novolak with a melting point >30° C.,
a curing accelerator,
a silane-based epoxy functional adhesion promoter, and
a solvent;
placing the coated first bonding partner in contact with the second bonding partner;
impregnating the second bonding partner and the lacquer-coated first bonding partner combined with an impregnation resin; and
curing said impregnation resin, said lacquer coating, or both.

### Claim 2 (depends on 1)

The method as set forth in claim 1 wherein said epoxy resin mixture comprises:
1 to 80% by weight, based on the weight of the epoxy resin mixture, of a solid epoxy resin having an epoxide number <1 Eq/kg, and
1 to 80% by weight, based on the weight of the epoxy resin mixture, of a solid epoxy resin having an epoxide number ranging from 1 Eq/kg to 2 Eq/kg.

### Claim 3 (depends on 1)

The method as set forth in claim 1 wherein said epoxy resin mixture comprises
40 to 60% by weight, based on the weight of the epoxy resin mixture, of a solid epoxy resin with an epoxide number <1 Eq/kg,
20 to 40% by weight, based on the weight of the epoxy resin mixture, of a solid epoxy resin having an epoxide number ranging from 1 Eq/kg to 2 Eq/kg;
10 to 40% by weight, based on the weight of the epoxy resin mixture, of a solid multifunctional epoxy resin having an epoxide number >4 Eq/kg and
10 to 20% by weight, based on the weight of the epoxy resin mixture, of a phenol and/or cresol novolak with a melting point >30° C. lacquer.

### Claim 4 (depends on 1)

The method as set forth in claim 1, wherein said at least one solid epoxy resin having an epoxide number not exceeding 2 Eq/kg comprises a bisphenol-A and/or bisphenol-F based epoxy resin.

### Claim 5 (depends on 1)

The method as set forth in claim 1, wherein said multifunctional epoxide resin with an epoxide number >4 Eq/kg is selected from the group consisting of epoxy phenol novolaks, epoxy cresol novolaks, triglycidyl isocyanurates, and mixtures of two or more of these substances.

### Claim 6 (depends on 1)

The method as set forth in claim 1, wherein said curing accelerator comprises tertiary amines or imidazole derivatives.

### Claim 7 (depends on 6)

The method as set forth in claim 6 wherein said curing accelerator comprises 2 ethyl-4-imidazole.

### Claim 8 (depends on 1)

The method as set forth in claim 1, wherein said percentage of said silane-based epoxy functional adhesion promoter in relation to said epoxy resin mixture is 0.1% by weight to 5% by weight.

### Claim 9 (depends on 8)

The method as set forth in in claim 8 wherein said percentage of said silane-based epoxy functional adhesion promoter in relation to said epoxy resin mixture is 1% by weight to 3% by weight, based on the weight of the epoxy resin mixture.

### Claim 10 (depends on 1)

The method as set forth in claim 1, wherein said silane-based epoxy functional adhesion promoter is selected from the group consisting of γ-glycidyloxypropyltrimethoxysilane or β-(3,4-epoxycyclohexyl)-ethyltrimethoxysilane.

### Claim 11 (depends on 1)

The method as set forth in claim 1, wherein said solvent is selected from the group consisting of aliphatic and aromatic hydrocarbons, ethers, esters, glycol ethers, alcohols, ketones, and mixtures thereof.

### Claim 12 (depends on 1)

The method as set forth in claim 1, wherein said lacquer composition has a percentage of solids that ranges from 1% by weight to 50% by weight, based upon the weight of the lacquer composition.

### Claim 13 (depends on 12)

The method as set forth in claim 12 wherein said percentage of solids of the lacquer composition ranges from 10% by weight to 20% by weight, based upon the weight of the lacquer composition.

### Claim 14 (depends on 1)

The method as set forth in claim 1, wherein said lacquer composition additionally comprises at least one corrosion protection additive.

### Claim 15 (depends on 14)

The method as set forth in claim 14 wherein said at least one corrosion protection additive comprises zinc phosphate, zinc chromate, or zinc hydroxy phosphite.

### Claim 16 (depends on 1)

The method as set forth in claim 1, wherein said lacquer composition further comprises wherein a soluble dyestuff and/or a levelling agent and/or a defoamant.

### Claim 17 (depends on 1)

The method as set forth in claim 1, wherein said lacquer composition further comprises a non-metallic filler.

### Claim 18 (depends on 17)

The method as set forth in claim 17 wherein said non-metallic filler comprises at least one dispersible pigment and/or a substance of selected from the group consisting of silica flour, mica and talcum.

### Claim 19 (depends on 18)

The method as set forth in claim 18 wherein said dispersible pigment comprises carbon black and/or rutile and/or a dispersion aid.

### Claim 20 (depends on 18)

The method as set forth in claim 18, wherein said dispersible pigment further comprises a rheological additive and/or deposition aids.

### Claim 21 (depends on 20)

The method as set forth in claim 20 wherein said rheological additive and/or deposition aids comprises a bentonite or an aerosil.

### Claim 22 (depends on 1)

The method as set forth in claim 1, wherein said phenol and/or creosol cresol novolak has a melting point >100° C.

### Claim 23 (depends on 1)

The method as set forth in claim 1, wherein at a temperature of 25° C. said impregnation resin has a viscosity ranging from 50 mPa·s to 1000 mPa·s.

### Claim 24 (depends on 23)

The method as set forth in claim 23 wherein at a temperature of 25° C. said impregnation resin has a viscosity ranging from 200 mPa·s to 300 mPa·s.

### Claim 25 (depends on 1)

The method as set forth in claim 1 wherein said impregnation resin comprises a bisphenol-A epoxy resin that is liquid at a temperature of 20° C., and/or a bisphenol-F epoxy resin that is liquid at a temperature of 20° C.

### Claim 26 (depends on 1)

The method as set forth in claim 1, wherein said impregnation resin further comprises an amount of an epoxy-functional thinner effective to reduce the viscosity of the impregnation resin.

### Claim 27 (depends on 1)

The method as set forth in claim 1, wherein said impregnation resin further comprises an anhydride curing agent.

### Claim 28 (depends on 27)

The method as set forth in claim 27 wherein said anhydride curing agent comprises a thin dicarbonic acid anhydride.

### Claim 29 (depends on 28)

The method as set forth in claim 28 wherein said thin dicarbonic acid anhydride is methyl cyclohexane di carbonic acid anhydride.

### Claim 30 (depends on 1)

The method as set forth in claim 1, wherein said impregnation resin further comprises a curing accelerator.

### Claim 31 (depends on 30)

The method as set forth in claim 30 wherein said curing accelerator comprises an imidazole derivative and/or a bortrichloride amine system.

### Claim 32 (depends on 1)

The method as set forth in claim 1 wherein said impregnating is done at an absolute pressure p1 smaller or equal to 1 hPa.

### Claim 33 (depends on 1)

The method as set forth in claim 1, wherein said second bonding partner comprises a recess, and wherein said placing the coated first bonding partner in contact with the second bonding partner comprises inserting said coated first bonding partner at least partly into said recess.

### Claim 34 (depends on 33)

The method as set forth in claim 33, wherein said recess comprises an opening passing through the second bonding partner.

### Claim 35 (depends on 34)

The method as set forth in claim 34, wherein said opening is closed off at one side before insertion of the first bonding partner.

### Claim 36 (depends on 35)

The method as set forth in claim 35, wherein said recess comprises an adhesive film which closes off one side of said opening in the second bonding partner.

### Claim 37 (depends on 33)

The method as set forth claim 33, wherein said placing the coated first bonding partner in contact with the second bonding partner further comprises totally closing off said recess in the second bonding partner after insertion of the first bonding partner and before impregnation.

### Claim 38 (depends on 37)

The method as set forth in claim 37, wherein said totally closing off comprises applying an adhesive film over an opening of the recess.

### Claim 39 (depends on 1)

The method as set forth in claim 1, further comprising removing any impregnation resin sticking to an outer surface of an assembly comprising the first bonding partner, the second bonding partner and the lacquer coating by flushing of the impregnation resin from the outer surface with a solvent, such that the impregnation resin remains in interstices of the assembly.

### Claim 40 (depends on 39)

The method as set forth in claim 39 wherein said interstices include a gap formed between the first bonding partner and the second bonding partner.

### Claim 41 (depends on 39)

The method as set forth in claim 39, wherein said second bonding partner comprises a sheet metal laminate.

### Claim 42

The method as set forth in any of the preceding claims wherein said curing of said impregnation resin, said lacquer, or both comprises pre-curing said first bonding partner, second bonding partner, lacquer coating together with the impregnation resin sticking thereto after impregnation is precured in a first curing step at an elevated first temperature.

### Claim 43 (depends on 42)

The method as set forth in claim 42, wherein said elevated first temperature ranges from 50° C. to 100° C.

### Claim 44 (depends on 42)

The method as set forth in claim 42, wherein said curing further comprises rotating said first bonding partner, second bonding partner, lacquer coating together with the impregnation resin sticking thereto after impregnation during the first curing step.

### Claim 45 (depends on 42)

The method as set forth in claim 42, wherein said curing of said impregnation resin, said lacquer, or both further comprises curing said first bonding partner, second bonding partner, lacquer coating together with the impregnation resin sticking thereto after impregnation in a second curing step at an elevated second temperature which is higher than said elevated first temperature.

### Claim 46 (depends on 45)

The method as set forth in claim 45, wherein said elevated second temperature ranges from 100° C. to 150° C.

### Claim 47 (depends on 45)

The method as set forth in claim 45, wherein said curing of said impregnation resin, said lacquer, or both further comprises rotating said first bonding partner, second bonding partner, lacquer coating together with the impregnation resin sticking thereto after impregnation during the second curing step.

### Claim 48 (depends on 1)

The method as set forth in claim 1, wherein said first bonding partner is a magnet or magnetizable body, and wherein said second bonding partner is a substrate body of a rotor to be produced for a permanent magnet synchronous machine.

### Claim 49 (depends on 48)

A substrate body of a rotor for a permanent magnet synchronous machine produced by the process of claim 48.

### Claim 50 (depends on 1)

The method as set forth in claim 1, further comprising reducing the viscosity of the impregnation resin prior to curing by contacting the impregnation resin with an epoxy functional thinner.