# US 2010/0164143 A1 · Nucleating agent and injection molding method of polyethylene terephalate

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2010/0164143 A1
- Document ID: US20100164143A1
- Status: Published application
- Kind: A1
- Application number: 12/648,540
- Filed: 2009-12-29
- Published: 2010-07-01
- Earliest claimed: 2005-12-29
- Assignees: Industrial Technology Research Institute
- Inventors: Hsun-Yu LI; Chih-Hsiang Lin; Chi Lung Wu; Hsin-Ching Kao
- Web page: https://patentgrep.com/patent/US20100164143A1

## CPC

- C08L 67/02: Polyesters derived from dicarboxylic acids and dihydroxy compounds (C08L67/06 takes precedence)
- B29C 45/0001: {characterised by the choice of material}
- B29K 2067/00: Use of polyesters {or derivatives thereof}, as moulding material
- B29K 2105/0005: {containing compounding ingredients (releasing, lubricating or separating agents B29C33/56, fibers B29K2105/08, B29K2105/12; fillers B29K2105/16, recycled material B29K2105/26)}
- C08K 3/36: Silica
- Y10T 428/2991: Coated
- Y10T 428/2998: including synthetic resin or polymer
- C08L: COMPOSITIONS OF MACROMOLECULAR COMPOUNDS (compositions based on polymerisable monomers C08F, C08G; artificial filaments or fibres D01F; textile treating compositions D06)
- B29C: SHAPING OR JOINING OF PLASTICS; SHAPING OF MATERIAL IN A PLASTIC STATE, NOT OTHERWISE PROVIDED FOR; AFTER-TREATMENT OF THE SHAPED PRODUCTS, e.g. REPAIRING (making preforms B29B11/00; making laminated products by combining previously unconnected layers which become one product whose layers will remain together B32B37/00 - B32B41/00)
- B29K: INDEXING SCHEME ASSOCIATED WITH SUBCLASSES B29B, B29C OR B29D, RELATING TO MOULDING MATERIALS OR TO MATERIALS FOR {MOULDS, } REINFORCEMENTS, FILLERS OR PREFORMED PARTS, e.g. INSERTS
- C08K: Use of inorganic or non-macromolecular organic substances as compounding ingredients (paints, inks, varnishes, dyes, polishes, adhesives C09)
- Y10T: TECHNICAL SUBJECTS COVERED BY FORMER US CLASSIFICATION

## Abstract

The invention relates to a nucleating agent for polyethylene terephthalate and injection molding method thereof. The nucleating agent comprises a SiO2 core grafted with bis(2-hydroxyethyl) terephthalate, which accelerates the crystallization of polyethylene terephthalate for injection molding.

## Claims

### Claim 1

An injection molding method for polyethylene terephthalate, comprising:
subjecting terephthalic acid, silicon oxide nanoparticles, and ethylene glycol to esterification to form a bis(2-hydroxyethyl) terephthalate monomer and a nucleating agent of polyethylene terephthalate, comprising:
a silicon oxide core, and
a plurality of bis(2-hydroxyethyl) terephthalate oligomers grafted on the surface of the silicon oxide core, said nucleating agent having the formula:
wherein n is an integer larger than 1,
polymerizing the bis(2-hydroxyethyl) terephthalate monomer to form the polyethylene terephthalate, wherein the polyethylene terephthalate and the bis(2-hydroxyethyl) terephthalate oligomers proceed an in-situ polymerization;
blending additives with the polyethylene terephthalate by an extruder and processing the blend into pellets,
melting the pellets and injecting the melt into a mold, and
cooling the mold to form an article.

### Claim 2 (depends on 1)

The injection molding method as claimed in claim 1, wherein the additives comprise chain extenders, solid-stating accelerators, impact modifiers, nucleation promoters, anti-hydrolysis additives, reinforcements, or flame retardants.

### Claim 3 (depends on 1)

The injection molding method as claimed in claim 1, wherein the mold is cooled by a water bath system.

### Claim 4 (depends on 1)

The injection molding method as claimed in claim 1, wherein the article is an engineering-grade plastic.

### Claim 5 (depends on 1)

The injection molding method as claimed in claim 1, wherein the article has a molecular weight of about 15000 to 20000.

### Claim 6 (depends on 1)

The injection molding method as claimed in claim 1, wherein the article has a molecular weight of about 18000.

### Claim 7 (depends on 1)

The injection molding method as claimed in claim 1, wherein the esterification is performed at a temperature lower than the polymerization of polyethylene terephthalate.

### Claim 8 (depends on 7)

The injection molding method as claimed in claim 7, wherein the esterification is performed at a temperature of about 150 to 200° C.

### Claim 9 (depends on 7)

The injection molding method as claimed in claim 7, wherein the polymerization of polyethylene terephthalate is performed at a temperature of about 250 to 300° C.

### Claim 10 (depends on 7)

The injection molding method as claimed in claim 7, wherein the article has a cold-crystallization peak temperature above 200° C.

### Claim 11 (depends on 7)

The injection molding method as claimed in claim 7, wherein the article has a semi-crystallization time of less than 1 minute at a temperature below 190° C.