# US 2010/0164135 A1 · Method for producing thermoplastic film

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2010/0164135 A1
- Document ID: US20100164135A1
- Status: Published application
- Kind: A1
- Application number: 11/916,214
- Filed: 2006-05-24
- Published: 2010-07-01
- Earliest claimed: 2005-05-30
- Assignees: FUJIFILM Corporation
- Inventors: Massaki Otoshi; Kiyokazu Hashimoto
- Web page: https://patentgrep.com/patent/US20100164135A1

## CPC

- G02B 5/3033: {in the form of a thin sheet or foil, e.g. Polaroid}
- B29C 48/08: flexible, e.g. films
- B29C 48/305: having a wide opening, e.g. for forming sheets
- B29C 48/625: characterised by the ratio of the threaded length of the screw to its outside diameter [L/D ratio]
- B29C 48/832: {Heating}
- B29C 48/91: Heating, e.g. for cross linking
- B29C 48/914: {Cooling drums}
- B29C 48/92: Measuring, controlling or regulating
- C08J 5/18: Manufacture of films or sheets
- C08L 1/10: Esters of organic acids {, i.e. acylates}
- C08L 1/14: Mixed esters, e.g. cellulose acetate-butyrate
- B29C 48/906: {using roller calibration}
- B29C 2948/92028: Force; Tension
- B29C 2948/92152: Thickness
- B29C 2948/92428: Calibration, after-treatment, or cooling zone
- B29C 2948/92438: Conveying, transporting or storage of articles
- B29C 2948/9259: Angular velocity
- B29C 2948/92647: Thickness
- B29C 2948/92704: Temperature
- B29C 2948/92895: Barrel or housing
- B29C 2948/92904: Die; Nozzle zone
- B29C 2948/92923: Calibration, after-treatment or cooling zone
- B29C 2948/92933: Conveying, transporting or storage of articles
- B29K 2001/00: Use of cellulose, modified cellulose or cellulose derivatives, e.g. viscose, as moulding material
- B29K 2001/12: {Cellulose acetate}
- C08J 2301/10: Esters of organic acids
- G02B: OPTICAL ELEMENTS, SYSTEMS OR APPARATUS
- B29C: SHAPING OR JOINING OF PLASTICS; SHAPING OF MATERIAL IN A PLASTIC STATE, NOT OTHERWISE PROVIDED FOR; AFTER-TREATMENT OF THE SHAPED PRODUCTS, e.g. REPAIRING (making preforms B29B11/00; making laminated products by combining previously unconnected layers which become one product whose layers will remain together B32B37/00 - B32B41/00)
- C08J: WORKING-UP; GENERAL PROCESSES OF COMPOUNDING; AFTER-TREATMENT NOT COVERED BY SUBCLASSES C08B, C08C, C08F, C08G or C08H (working, e.g. shaping, of plastics B29)
- C08L: COMPOSITIONS OF MACROMOLECULAR COMPOUNDS (compositions based on polymerisable monomers C08F, C08G; artificial filaments or fibres D01F; textile treating compositions D06)
- B29K: INDEXING SCHEME ASSOCIATED WITH SUBCLASSES B29B, B29C OR B29D, RELATING TO MOULDING MATERIALS OR TO MATERIALS FOR {MOULDS, } REINFORCEMENTS, FILLERS OR PREFORMED PARTS, e.g. INSERTS

## Abstract

There is provided a method for producing a thermoplastic film that has a small distribution of retardation and excels in optical properties. In the method for producing a thermoplastic film by after extruding a molten resin from a die into a sheet, and cooling and solidifying the extruded sheet on a rotating cooling drum, peeling the cellulose acylate film off the cooling drum, and taking off the film with a take-off roller, the tension of the cellulose acylate film at the take-off roller is set to 0.02 kgf/mm2 or lower.

## Claims

### Claim at position 1

1-12. (canceled)

### Claim 13

A method for producing a thermoplastic film including the steps of extruding a molten resin from a die into a form of a sheet, cooling and solidifying the extruded sheet on a running or rotating cooling support, then peeling the film off the cooling support, and taking off the film with a take-off roller, the method comprising:
setting a take-off tension of the film on the take-off roller at 0.02 kgf/mm2 or lower.

### Claim 14 (depends on 13)

The method for producing a thermoplastic film according to claim 13, wherein a surface temperature of the take-off roller is controlled from Tg−110° C. to Tg−30° C., where Tg represents a glass transition temperature of the molten resin.

### Claim 15 (depends on 13)

The method for producing a thermoplastic film according to claim 13, wherein the take-off roller is a nip roller that nips and conveys the film with a pair of rotating rollers, or a suction roller that generates a suction force on a surface of a rotating roller to convey the film.

### Claim 16 (depends on 14)

The method for producing a thermoplastic film according to claim 14, wherein the take-off roller is a nip roller that nips and conveys the film with a pair of rotating rollers, or a suction roller that generates a suction force on a surface of a rotating roller to convey the film.

### Claim 17 (depends on 15)

The method for producing a thermoplastic film according to claim 15, wherein the suction roller is a crown roller having a larger diameter at a center portion in a film-width direction than at end portions, or a concave roller having a larger diameter at end portions in a film-width direction than at a center portion.

### Claim 18 (depends on 16)

The method for producing a thermoplastic film according to claim 16, wherein the suction roller is a crown roller having a larger diameter at a center portion in a film-width direction than at end portions, or a concave roller having a larger diameter at end portions in a film-width direction than at a center portion.

### Claim 19 (depends on 13)

The method for producing a thermoplastic film according to claim 13, wherein the film taken off by the take-off roller has an in-plane retardation Re of −10 nm through 90 nm, and a retardation Rth in a thickness direction of 0 through 90 nm.

### Claim 20 (depends on 18)

The method for producing a thermoplastic film according to claim 18, wherein the film taken off by the take-off roller has an in-plane retardation Re of −10 nm through 90 nm, and a retardation Rth in a thickness direction of 0 through 90 nm.

### Claim 21 (depends on 13)

The method for producing a thermoplastic film according to claim 13, wherein the film taken off by the take-off roller has a fluctuation of 10 nm or less in both a width direction and a length direction of the Re and Rth.

### Claim 22 (depends on 20)

The method for producing a thermoplastic film according to claim 20, wherein the film taken off by the take-off roller has a fluctuation of 10 nm or less in both a width direction and a length direction of the Re and Rth.

### Claim 23 (depends on 13)

The method for producing a thermoplastic film according to claim 13, wherein the thermoplastic film is a cellulose acylate film.

### Claim 24 (depends on 22)

The method for producing a thermoplastic film according to claim 22, wherein the thermoplastic film is a cellulose acylate film.

### Claim 25 (depends on 23)

The method for producing a thermoplastic film according to claim 23, wherein acylate group of the cellulose acylate film satisfies following substitution degrees:
2.0≦X+Y≦3.0,
0≦X≦2.0, and
1.223 Y≦2.9,
where X is the substitution degree of an acetyl group, and Y is the sum of substitution degrees of a propionyl group, a butyryl group, a pentanoyl group, and a hexanoyl group.

### Claim 26 (depends on 24)

The method for producing a thermoplastic film according to claim 24, wherein acylate group of the cellulose acylate film satisfies following substitution degrees:
2.0≦X+Y≦3.0,
0≦X≦2.0, and
1.2≦Y≦2.9,
where X is the substitution degree of an acetyl group, and Y is the sum of substitution degrees of a propionyl group, a butyryl group, a pentanoyl group, and a hexanoyl group.

### Claim 27 (depends on 23)

A method for producing a thermoplastic film, wherein the unstretched cellulose acylate film produced by the method of claim 23 is stretched by 1% or more and by 300% or less in at least one direction of the lengthwise direction and widthwise direction of the film.

### Claim 28 (depends on 27)

An optical compensation film for a liquid crystal display panel, wherein the cellulose acylate film produced by the method of claim 27 is used as a base material.