# US 2010/0164133 A1 · Oxygen Tailoring of Polyethylene Resins

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2010/0164133 A1
- Document ID: US20100164133A1
- Status: Published application
- Kind: A1
- Application number: 12/722,180
- Filed: 2010-03-11
- Published: 2010-07-01
- Earliest claimed: 2001-11-30
- Assignees: Univation Technologies, LLC
- Inventors: Sandra D. Schregenberger; James F. Lottes; Pradeep P. Shirodkar; Porter C. Shannon
- Web page: https://patentgrep.com/patent/US20100164133A1

## CPC

- C08L 23/06: Polyethylene
- B29B 7/421: {with screw and additionally other mixing elements on the same shaft, e.g. paddles, discs, bearings, rotor blades of the Banbury type}
- B29C 48/022: {characterised by the choice of material}
- B29C 48/10: flexible, e.g. blown foils
- B29C 48/53: having a varying channel depth, e.g. varying the diameter of the longitudinal screw trunk
- C08F 8/06: Oxidation
- C08F 8/50: Partial depolymerisation
- C08F 110/02: Ethene
- C08L 23/04: Homopolymers or copolymers of ethene
- C08L 23/0815: {with aliphatic 1-olefins containing one carbon-to-carbon double bond}
- B29C 48/52: with an outer diameter varying along the longitudinal axis, e.g. for obtaining different thread clearance
- B29C 67/246: {Moulding high reactive monomers or prepolymers, e.g. by reaction injection moulding [RIM], liquid injection moulding [LIM] (casting monomers B29C39/006, mixing construction B29B7/74)}
- B29C 2791/005: Using a particular environment, e.g. sterile fluids other than air
- B29K 2023/06: {PE, i.e. polyethylene}
- B29K 2023/0641: {MDPE, i.e. medium density polyethylene}
- C08F 2810/10: including a reactive processing step which leads, inter alia, to morphological and/or rheological modifications, e.g. visbreaking
- C08L 2205/02: containing two or more polymers of the same C08L -group
- C08L 2205/025: containing two or more polymers of the same hierarchy C08L, and differing only in parameters such as density, comonomer content, molecular weight, structure
- C08L 2666/06: Homopolymers or copolymers of unsaturated hydrocarbons; Derivatives thereof
- C08L: COMPOSITIONS OF MACROMOLECULAR COMPOUNDS (compositions based on polymerisable monomers C08F, C08G; artificial filaments or fibres D01F; textile treating compositions D06)
- B29B: PREPARATION OR PRETREATMENT OF THE MATERIAL TO BE SHAPED; MAKING GRANULES OR PREFORMS; RECOVERY OF PLASTICS OR OTHER CONSTITUENTS OF WASTE MATERIAL CONTAINING PLASTICS
- B29C: SHAPING OR JOINING OF PLASTICS; SHAPING OF MATERIAL IN A PLASTIC STATE, NOT OTHERWISE PROVIDED FOR; AFTER-TREATMENT OF THE SHAPED PRODUCTS, e.g. REPAIRING (making preforms B29B11/00; making laminated products by combining previously unconnected layers which become one product whose layers will remain together B32B37/00 - B32B41/00)
- C08F: MACROMOLECULAR COMPOUNDS OBTAINED BY REACTIONS ONLY INVOLVING CARBON-TO-CARBON UNSATURATED BONDS
- B29K: INDEXING SCHEME ASSOCIATED WITH SUBCLASSES B29B, B29C OR B29D, RELATING TO MOULDING MATERIALS OR TO MATERIALS FOR {MOULDS, } REINFORCEMENTS, FILLERS OR PREFORMED PARTS, e.g. INSERTS

## Abstract

A process is provided for extruding a bimodal polyethylene resin. The process includes providing a polyethylene homopolymer or copolymer resin having a bimodal molecular weight distribution; conveying the resin through an extruder having a feed zone in which the resin is not melted, a melt-mixing zone in which at least a portion of the resin is melted, and a melt zone in which the resin is in a molten state, each zone being partially filled with the resin; and contacting the molten resin in the melt zone with a gas mixture of 8 to 40% by volume O2. The resin can be further pelletized. The oxygen-tailored resin can be used to make polyethylene films having improved bubble stability.

## Claims

### Claim at position 1

1-19. (canceled)

### Claim 20

A process for extruding a bimodal polyethylene resin, the process comprising:
(a) contacting monomers comprising ethylene under polymerization conditions with a supported bimetallic catalyst to produce a polyethylene resin having a bimodal molecular weight distribution;
(b) conveying the bimodal polyethylene resin through an extruder having a feed zone in which the resin is not melted, a melt-mixing zone in which at least a portion of the resin is melted, and a melt zone in which the resin is in a molten state, each zone being partially filled with the resin; and
(c) contacting the molten resin in the melt zone with a gas mixture comprising 8 to 40% by volume.

### Claim 21 (depends on 1)

The process of claim 1, wherein the bimodal polyethylene resin is a copolymer of ethylene and at least one comonomer selected from the group consisting of C3 to C12 alpha-olefins.

### Claim 22 (depends on 1)

The process of claim 1, wherein the bimodal polyethylene resin has a density of at least 0.93 g/cm3.

### Claim 23 (depends on 1)

The process of claim 1, wherein the bimodal polyethylene resin has a density of at least 0.945 g/cm3.

### Claim 24 (depends on 1)

The process of claim 1, wherein the bimodal polyethylene resin has a density of from 0.93 to 0.97 g/cm3.

### Claim 25 (depends on 1)

The process of claim 1, wherein the gas mixture comprises 10 to 35% by volume O2.

### Claim 26 (depends on 1)

The process of claim 1, wherein the gas mixture comprises 15 to 25% by volume O2.

### Claim 27 (depends on 8)

The process of claim 8, wherein the supported bimetallic catalyst comprises a non-metallocene transition metal catalyst and a metallocene transition metal catalyst.

### Claim 28 (depends on 8)

The process of claim 8, wherein the monomers comprise ethylene and at least one C3-C12 alpha olefin.

### Claim 29 (depends on 1)

The process of claim 1, further comprising after step (c) pelletizing the oxygen-treated resin.

### Claim 30 (depends on 1)

The process of claim 1, wherein the bimodal polyethylene resin comprises a low molecular weight component and a high molecular weight component where the relative weight fraction of the high molecular weight component to the low molecular weight component is in the range of from 1:9 to 9:1.