# US 2010/0164121 A1 · Metallization system of a semiconductor device comprising extra-tapered transition vias

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2010/0164121 A1
- Document ID: US20100164121A1
- Status: Published application
- Kind: A1
- Application number: 12/634,216
- Filed: 2009-12-09
- Published: 2010-07-01
- Earliest claimed: 2008-12-31
- Assignees: Advanced Micro Devices, Inc.
- Inventors: Frank Feustel; Thomas Werner; Kai Frohberg
- Web page: https://patentgrep.com/patent/US20100164121A1

## CPC

- H10W 20/084: {for dual-damascene structures}
- H10W 20/082: {the openings being tapered via holes}
- H10W 20/088: {involving partial etching of via holes}
- H10W: GENERIC PACKAGES, INTERCONNECTIONS, CONNECTORS OR OTHER CONSTRUCTIONAL DETAILS OF DEVICES COVERED BY CLASS H10

## Abstract

In a metallization system of a semiconductor device, a transition via may be provided with an increased degree of tapering by modifying a corresponding etch sequence. For example, the resist mask for forming the via opening may be eroded once or several times in order to increase the lateral size of the corresponding mask opening. Due to the pronounced degree of tapering, enhanced deposition conditions may be accomplished during the subsequent electrochemical deposition process for commonly filling the via opening and a wide trench connected thereto.

## Claims

### Claim 1

A method, comprising:
forming an etch mask above a dielectric material of a first metallization layer of a semiconductor device, said etch mask comprising a mask opening having a first lateral size corresponding to a target lateral size at a bottom of a via to be formed in said dielectric material;
forming a via opening on the basis of said mask opening having said first lateral size so as to extend to a first depth in said dielectric material;
increasing said mask opening such that the mask opening has a second lateral size;
increasing said via opening on the basis of said mask opening having said second lateral size so as to extend to a second depth;
forming a trench above said via opening in said dielectric material so as to connect to said via opening; and
commonly filling said via opening and said trench with a metal-containing material, said via opening extending to a metal region of a second metallization layer located below said first metallization layer.

### Claim 2 (depends on 1)

The method of claim 1, further comprising increasing said mask opening such that the mask opening has a third lateral size and increasing said via opening on the basis of said mask opening having said third lateral size so as to extend to a third depth.

### Claim 3 (depends on 1)

The method of claim 1, wherein increasing the lateral size of said mask opening comprises providing said etch mask as a resist mask and performing a resist removal process.

### Claim 4 (depends on 1)

The method of claim 1, wherein forming said trench comprises forming a trench etch mask above said dielectric material and said via opening extending at least to said second depth and performing an etch process to obtain said trench and increase a depth of said via opening.

### Claim 5 (depends on 1)

The method of claim 1, wherein increasing said via opening further comprises performing an etch process on the basis of said etch mask and controlling said etch process by using an etch stop layer formed below said dielectric material.

### Claim 6 (depends on 1)

The method of claim 1, wherein said target lateral size is approximately equal to or less than a width of said metal region.

### Claim 7 (depends on 1)

The method of claim 1, wherein said via opening extending to said first depth is formed prior to forming said trench.

### Claim 8 (depends on 1)

The method of claim 1, wherein said trench is formed prior to forming said via opening.

### Claim 9 (depends on 1)

The method of claim 1, wherein said first depth is approximately 30 percent of a final depth of said via opening.

### Claim 10 (depends on 1)

The method of claim 1, wherein said target lateral size is approximately 100 nm or less.

### Claim 11

A method, comprising:
forming a via opening in a dielectric material of a first metallization layer of a semiconductor device, said via opening extending to a first depth and having a first lateral size;
forming a spacer element on sidewalls of said via opening; and
increasing a depth of said via opening so as to extend to a metal region of a second metallization layer that is formed below said first metallization layer.

### Claim 12 (depends on 11)

The method of claim 11, wherein forming said via opening comprises forming an etch mask having a mask opening, etching said via opening into said dielectric material on the basis of said etch mask and removing said etch mask.

### Claim 13 (depends on 12)

The method of claim 12, wherein forming said spacer element comprises depositing a spacer layer and etching said spacer layer so as to define a target width of a bottom of said via opening.

### Claim 14 (depends on 13)

The method of claim 13, further comprising forming an etch stop layer prior to depositing said spacer layer.

### Claim 15 (depends on 11)

The method of claim 11, wherein increasing the depth of said via opening comprises removing material of said spacer element and said dielectric material with a similar removal rate.

### Claim 16 (depends on 11)

The method of claim 11, further comprising forming a trench in said dielectric material above said via opening, wherein said via opening connects to said trench.

### Claim 17 (depends on 16)

The method of claim 16, wherein said trench is formed while increasing the depth of said via opening.

### Claim 18

A semiconductor device, comprising:
a first metallization layer formed above a substrate, said first metallization layer comprising a metal line having a first width;
a second metallization layer formed below said first metallization layer and comprising a second metal line having a second width that is less than said first width; and
a via extending from said first metal line to said second metal line, said via having a first lateral dimension at said first metal line and a second lateral dimension at said second metal line, said second lateral dimension being approximately 60 percent or less of said first lateral dimension.

### Claim 19 (depends on 18)

The semiconductor device of claim 18, wherein said second lateral dimension is approximately 100 nm or less.

### Claim 20 (depends on 18)

The semiconductor device of claim 18, wherein said second lateral dimension is approximately 40 percent or less of the said first lateral dimension.

### Claim 21 (depends on 18)

The semiconductor device of claim 18, wherein said first width is at least twice said second width.