# US 2010/0164096 A1 · Structures and Methods for Improving Solder Bump Connections in Semiconductor Devices

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2010/0164096 A1
- Document ID: US20100164096A1
- Status: Published application
- Kind: A1
- Application number: 12/344,711
- Filed: 2008-12-29
- Published: 2010-07-01
- Earliest claimed: 2008-12-29
- Assignees: International Business Machines Corporation
- Inventors: Timothy H. Daubenspeck; Jeffrey P. Gambino; Christopher D. Muzzy; Wolfgang Sauter; Timothy D. Sullivan
- Web page: https://patentgrep.com/patent/US20100164096A1

## CPC

- H10W 72/20: Bump connectors, e.g. solder bumps or copper pillars; Dummy bumps; Thermal bumps
- H10W 72/019: {of bond pads}
- H10W 72/90: Bond pads, in general
- H10W 72/01938: {in gaseous form, e.g. by CVD or PVD}
- H10W 72/221: {Structures or relative sizes}
- H10W 72/242: {relative to the surface, e.g. recessed, protruding}
- H10W 72/244: {relative to underlying supporting features, e.g. bond pads, RDLs or vias}
- H10W 72/252: {comprising solid metals or solid metalloids, e.g. PbSn, Ag or Cu}
- H10W 72/29: Bond pads specially adapted therefor
- H10W 72/923: {Bond pads having multiple stacked layers}
- H10W 72/931: {Shapes of bond pads}
- H10W 72/932: {Plan-view shape, i.e. in top view}
- H10W 72/934: {Cross-sectional shape, i.e. in side view}
- H10W 72/9415: {relative to the surface, e.g. recessed, protruding}
- H10W 72/952: {comprising metals or metalloids, e.g. PbSn, Ag or Cu}
- H10W 90/724: {between a chip and a stacked insulating package substrate, interposer or RDL}
- H10W: GENERIC PACKAGES, INTERCONNECTIONS, CONNECTORS OR OTHER CONSTRUCTIONAL DETAILS OF DEVICES COVERED BY CLASS H10

## Abstract

Structures with improved solder bump connections and methods of fabricating such structures are provided herein. The structure includes a via formed in a dielectric layer to expose a contact pad and a capture pad formed in the via and over the dielectric layer. The capture pad has openings over the dielectric layer to form segmented features. The solder bump is deposited on the capture pad and the openings over the dielectric layer.

## Claims

### Claim 1

A method of manufacturing a semiconductor structure, comprising:
forming a capture pad structure over an insulative material and contact pad;
segmenting the capture pad structure over the insulative material; and
forming a solder bump over the capture pad structure and between the segments.

### Claim 2 (depends on 1)

The method of claim 1, wherein the segmenting is provided by an etching process and the insulative material is a soft polymer layer.

### Claim 3 (depends on 1)

The method of claim 1, wherein the capture pad structure is formed by depositing layers.

### Claim 4 (depends on 3)

The method of claim 3, wherein the layers include one of:
a nickel material sandwiched between a gold layer and a barrier layer; and
a TiW/Cu/Ni structure.

### Claim 5 (depends on 4)

The method of claim 4, wherein the barrier layer is a TiW barrier layer.

### Claim 6 (depends on 1)

The method of claim 1, wherein the solder bump is a lead free solder bump.

### Claim 7 (depends on 1)

The method of claim 1, wherein the segmenting includes forming openings in the capture pad structure over the insulative material by an etching process.

### Claim 8 (depends on 7)

The method of claim 7, wherein the etching forms openings of various sizes in the capture pad structure to form the segments.

### Claim 9 (depends on 8)

The method of claim 8, wherein the etching forms openings of various shapes in the capture pad structure to form the segments.

### Claim 10

A method of manufacturing a package, comprising:
heating the package to a set temperature in order to form solder interconnection joints;
cooling the package to solidify the solder interconnection joints; and
terminating fatigue crack initiation in at least one segmented portion of a ball limiting metallurgy of the package.

### Claim 11 (depends on 10)

The method of claim 10, wherein the terminating the fatigue crack initiation is provided by movement of the at least one segmented portion.

### Claim 12 (depends on 11)

The method of claim 11, wherein the movement absorbs stresses, which cause the fatigue crack initiation.

### Claim 13 (depends on 12)

The method of claim 12, further comprising directing the stresses into an underlying flexible insulative material for flexibility of a ball limiting metallurgy or under bump metallurgy segments and away form metal pads, wires and interconnects thereby prevent the formation of white bumps.

### Claim 14 (depends on 10)

The method of claim 10, wherein the solder interconnection joints include lead free solder bumps.

### Claim 15

A lead free solder bump structure, comprising:
a via formed in a dielectric layer to expose a contact pad;
a capture pad formed in the via and over the dielectric layer, the capture pad having openings over the dielectric layer to form segmented features; and
a solder bump deposited on the capture pad and the openings over the dielectric layer.

### Claim 16 (depends on 15)

The structure of claim 15, further comprising a laminate bonded to the solder bump.

### Claim 17 (depends on 15)

The structure of claim 15, wherein the solder bump is a lead free solder bump.

### Claim 18 (depends on 15)

The structure of claim 15, wherein the capture pad is an under bump metallurgy or ball limiting metallurgy having a refractory metal base layer and a diffusion barrier to layer, and the contact pad is Al.

### Claim 19 (depends on 15)

The structure of claim 15, wherein the dielectric layer is a photosensitive polyimide formed over other insulative layers having pads and/or wires and metal vias.

### Claim 20 (depends on 15)

The structure of claim 15, wherein the openings are of various sizes and shapes.