# US 2010/0164020 A1 · Transistor with an embedded strain-inducing material having a gradually shaped configuration

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2010/0164020 A1
- Document ID: US20100164020A1
- Status: Published application
- Kind: A1
- Application number: 12/640,765
- Filed: 2009-12-17
- Published: 2010-07-01
- Earliest claimed: 2008-12-31
- Assignees: Advanced Micro Devices, Inc.
- Inventors: Stephan Kronholz; Vassilios Papageorgiou; Gunda Beernink
- Web page: https://patentgrep.com/patent/US20100164020A1

## CPC

- H10D 84/038: {using silicon technology, e.g. SiGe}
- H10D 30/797: {being in source or drain regions, e.g. SiGe source or drain}
- H10D 62/021: {Forming source or drain recesses by etching e.g. recessing by etching and then refilling}
- H10D 84/0128: {Manufacturing their channels}
- H10D 84/013: {Manufacturing their source or drain regions, e.g. silicided source or drain regions}
- H10D 84/0147: {Manufacturing their gate sidewall spacers}
- H10D 84/0167: {Manufacturing their channels}
- H10D 84/017: {Manufacturing their source or drain regions, e.g. silicided source or drain regions}
- H10D 84/0184: {Manufacturing their gate sidewall spacers}
- H10D: INORGANIC ELECTRIC SEMICONDUCTOR DEVICES

## Abstract

In a transistor, a strain-inducing semiconductor alloy, such as silicon/germanium, silicon/carbon and the like, may be positioned very close to the channel region by providing gradually shaped cavities which may then be filled with the strain-inducing semiconductor alloy. For this purpose, two or more “disposable” spacer elements of different etch behavior may be used in order to define different lateral offsets at different depths of the corresponding cavities. Consequently, enhanced uniformity and, thus, reduced transistor variability may be accomplished, even for sophisticated semiconductor devices.

## Claims

### Claim 1

A method, comprising:
forming a first plurality of recesses in a crystalline semiconductor region, said first plurality of recesses being offset from a gate electrode structure by a first sidewall spacer formed on sidewalls of said gate electrode structure, said first plurality of recesses extending to a first depth;
forming a second plurality of recesses in said crystalline semiconductor region, said second plurality of recesses being offset from said gate electrode structure by a second sidewall spacer formed on said first sidewall spacer, said second plurality of recesses extending to a second depth that is greater than said first depth; and
forming a strain-inducing semiconductor alloy in said first and second recesses by performing a selective epitaxial growth process.

### Claim 2 (depends on 1)

The method of claim 1, wherein said first plurality of recesses are formed prior to forming said second plurality of recesses.

### Claim 3 (depends on 1)

The method of claim 1, wherein forming said first plurality of recesses comprises forming a first spacer layer above said gate electrode structure and a second gate electrode structure formed above a second crystalline semiconductor region, forming a first mask to cover said first spacer layer formed above said second gate electrode structure and said second semiconductor region, forming said first sidewall spacer from said first spacer layer and removing material from said crystalline semiconductor region in the presence of said first sidewall spacer and said first mask.

### Claim 4 (depends on 3)

The method of claim 3, wherein forming said second plurality of recesses comprises removing said first mask, depositing a second spacer layer and forming said second sidewall spacer from said second spacer layer.

### Claim 5 (depends on 4)

The method of claim 4, further comprising forming a second mask above said second gate electrode structure and said second crystalline semiconductor region prior to forming said second sidewall spacer.

### Claim 6 (depends on 4)

The method of claim 4, further comprising forming a sidewall spacer at said second gate electrode structure on said first spacer layer and using said first spacer layer as an etch mask when forming said second plurality of recesses in said crystalline semiconductor region.

### Claim 7 (depends on 1)

The method of claim 1, wherein forming said first and second plurality of recesses comprises forming a first portion of said second plurality of recesses, removing at least a portion of said second sidewall spacer and commonly forming a second portion of said second plurality of recesses and said first plurality of recesses.

### Claim 8 (depends on 1)

The method of claim 1, wherein forming said strain-inducing semiconductor alloy comprises performing a first epitaxial growth process so as to fill said first recesses in the presence of said first sidewall spacer with a first portion of said strain-inducing semiconductor alloy and to fill a portion of said second plurality of recesses in the presence of said first and second sidewall spacers with a second portion of said strain-inducing semiconductor alloy.

### Claim 9 (depends on 8)

The method of claim 8, wherein said first and second portions of said strain-inducing semiconductor alloy differ in at least a degree of in situ doping.

### Claim 10 (depends on 1)

The method of claim 1, wherein said strain-inducing semiconductor alloy is formed so as to induce a compressive strain in a channel region located in said crystalline semiconductor region below said gate electrode structure.

### Claim 11 (depends on 10)

The method of claim 10, wherein said semiconductor alloy comprises at least one of germanium and tin.

### Claim 12 (depends on 1)

The method of claim 1, wherein said strain-inducing semiconductor alloy is formed so as to induce a tensile strain in a channel region located in said crystalline semiconductor region below said gate electrode structure.

### Claim 13 (depends on 1)

The method of claim 1, wherein said first sidewall spacer is comprised of silicon dioxide and said second sidewall spacer is comprised of silicon nitride.

### Claim 14

A method, comprising:
forming a first spacer layer above a first semiconductor region having formed thereon a first gate electrode structure and above a second semiconductor region having formed thereon a second gate electrode structure;
selectively forming a first sidewall spacer from said first spacer layer on sidewalls of said first gate electrode structure;
performing a first etch process to form a plurality of cavities in said first semiconductor region on the basis of said first sidewall spacer;
forming a second sidewall spacer on said first sidewall spacer;
performing a second etch process to increase a depth of a portion of each of said plurality of cavities on the basis of said second sidewall spacer; and
forming a strain-inducing semiconductor alloy in said cavities.

### Claim 15 (depends on 14)

The method of claim 14, wherein forming said second sidewall spacer comprises depositing a second spacer layer above said first and second semiconductor regions and said first and second gate electrode structures and selectively forming said second sidewall spacer from said second spacer layer while masking said spacer layer above said second semiconductor region.

### Claim 16 (depends on 14)

The method of claim 14, wherein forming said second sidewall spacer comprises depositing a second spacer layer above said first and second semiconductor regions and said first and second gate electrode structures and forming said second sidewall spacer on said first sidewall spacer and on said first spacer layer formed above said second semiconductor region.

### Claim 17 (depends on 14)

The method of claim 14, wherein forming said strain-inducing semiconductor alloy comprises performing a first selective epitaxial growth process on the basis of said first and second sidewall spacers, removing said second sidewall spacer and performing a second selective epitaxial growth process on the basis of said first sidewall spacer.

### Claim 18 (depends on 17)

The method of claim 17, wherein said first and second epitaxial growth processes differ in at least one process parameter value.

### Claim 19 (depends on 18)

The method of claim 18, wherein said at least one different process parameter value determines an in situ doping of said strain-inducing semiconductor material.

### Claim 20 (depends on 14)

The method of claim 14, wherein said first spacer layer comprises silicon dioxide and said second spacer layer comprises silicon nitride.

### Claim 21

A semiconductor device, comprising:
a transistor formed above a substrate, said transistor comprising:
a gate electrode structure formed above a crystalline semiconductor region and comprising a gate electrode material;
a first strain-inducing semiconductor alloy formed in said crystalline semiconductor region and having a first depth and a first lateral offset from said gate electrode material; and
a second strain-inducing semiconductor alloy formed in said crystalline semiconductor region and having a second depth and a second lateral offset from said gate electrode material, said first and second depths being different and said first and second lateral offsets being different.

### Claim 22 (depends on 21)

The semiconductor device of claim 21, wherein said first and second strain-inducing semiconductor materials induce the same type of strain in a channel region of said transistor and wherein said first and second strain-inducing materials differ in at least one of a dopant concentration and a material composition.

### Claim 23 (depends on 22)

The semiconductor device of claim 22, wherein said strain-inducing semiconductor alloy induces a compressive strain in said channel region.

### Claim 24 (depends on 22)

The semiconductor device of claim 22, wherein strain-inducing semiconductor alloy induces a tensile strain in said channel region.

### Claim 25 (depends on 21)

The semiconductor device of claim 21, wherein a gate length of said gate electrode material is approximately 50 nm or less.