# US 2010/0164016 A1 · Adjusting of strain caused in a transistor channel by semiconductor material provided for threshold adjustment

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2010/0164016 A1
- Document ID: US20100164016A1
- Status: Published application
- Kind: A1
- Application number: 12/648,744
- Filed: 2009-12-29
- Published: 2010-07-01
- Earliest claimed: 2008-12-31
- Assignees: Globalfoundries Inc.
- Inventors: Stephan Kronholz; Thorsten Kammler; Gunda Beernink; Carsten Reichel
- Web page: https://patentgrep.com/patent/US20100164016A1

## CPC

- H10D 62/832: being Group IV materials comprising two or more elements, e.g. SiGe
- H10D 30/608: {having non-planar bodies, e.g. having recessed gate electrodes}
- H10D 30/751: {having composition variations in the channel regions}
- H10D 30/792: {comprising applied insulating layers, e.g. stress liners}
- H10D 30/797: {being in source or drain regions, e.g. SiGe source or drain}
- H10D 62/021: {Forming source or drain recesses by etching e.g. recessing by etching and then refilling}
- H10D 62/822: comprising only Group IV materials heterojunctions, e.g. Si/Ge heterojunctions
- H10D: INORGANIC ELECTRIC SEMICONDUCTOR DEVICES

## Abstract

The threshold voltage of a sophisticated transistor may be adjusted by providing a specifically designed semiconductor alloy in the channel region of the transistor, wherein a negative effect of this semiconductor material with respect to inducing a strain component in the channel region may be reduced or over-compensated for by additionally incorporating a strain-adjusting species. For example, a carbon species may be incorporated in the channel region, the threshold voltage of which may be adjusted on the basis of a silicon/germanium alloy of a P-channel transistor. Consequently, sophisticated metal gate electrodes may be formed in an early manufacturing stage.

## Claims

### Claim 1

A method, comprising:
forming a layer of a silicon-containing semiconductor alloy on a silicon-containing crystalline semiconductor region, said semiconductor alloy comprising a first non-silicon species;
introducing a second non-silicon species into at least one of said layer of silicon-containing semiconductor alloy and said silicon-containing crystalline semiconductor region, said second non-silicon species having the same valence as silicon and being different from said first non-silicon species; and
forming a gate electrode structure of a transistor above said layer of a silicon-containing semiconductor alloy, said gate electrode structure comprising a high-k dielectric gate insulation layer and a metal-containing gate electrode material formed on said high-k dielectric gate insulation layer.

### Claim 2 (depends on 1)

The method of claim 1, wherein said first non-silicon species comprises germanium and said second non-silicon species comprises carbon.

### Claim 3 (depends on 1)

The method of claim 1, wherein introducing said second non-silicon species comprises performing an ion implantation process.

### Claim 4 (depends on 3)

The method of claim 3, wherein a maximum concentration of said second non-silicon species is positioned within said layer of a semiconductor alloy.

### Claim 5 (depends on 3)

The method of claim 3, wherein a maximum concentration of said second non-silicon species is positioned below said layer of a semiconductor alloy.

### Claim 6 (depends on 1)

The method of claim 1, wherein introducing said second non-silicon species comprises performing an epitaxial growth process.

### Claim 7 (depends on 6)

The method of claim 6, wherein said layer of a semiconductor alloy is formed during at least a portion of said epitaxial growth process.

### Claim 8 (depends on 1)

The method of claim 1, further comprising forming cavities in said silicon-containing semiconductor region offset from said gate electrode structure and filling said cavities with a second semiconductor alloy that induces strain in a channel region positioned below said gate electrode structure.

### Claim 9 (depends on 8)

The method of claim 8, wherein said second semiconductor alloy comprises said first non-silicon species.

### Claim 10 (depends on 1)

The method of claim 1, further comprising masking a second silicon-containing semiconductor region when forming said layer of semiconductor alloy and introducing said second non-silicon species into at least one of said layer of semiconductor alloy and said silicon-containing semiconductor region.

### Claim 11 (depends on 10)

The method of claim 10, wherein masking said second silicon-containing semiconductor region comprises forming a hard mask above said second silicon-containing semiconductor region prior to forming said layer of semiconductor alloy.

### Claim 12 (depends on 11)

The method of claim 11, further comprising forming a resist mask above said second silicon-containing semiconductor region prior to introducing said second non-silicon species.

### Claim 13 (depends on 11)

The method of claim 11, wherein said hard mask is used as a mask when introducing said second non-silicon species.

### Claim 14 (depends on 13)

The method of claim 13, wherein said second non-silicon species is introduced by performing an implantation process.

### Claim 15

A method, comprising:
forming a threshold-adjusting semiconductor material on a silicon-containing semiconductor region;
providing a strain-adjusting species at least in said threshold-adjusting semiconductor material; and
forming a gate electrode structure of a transistor above said threshold-adjusting semiconductor material, said gate electrode structure comprising a high-k dielectric material formed at least above said threshold-adjusting semiconductor material, said gate electrode structure further comprising a metal-containing electrode material formed above said high-k dielectric material.

### Claim 16 (depends on 15)

The method of claim 15, wherein providing said strain-adjusting species comprises performing an implantation process to introduce a non-silicon species having the same valence as silicon.

### Claim 17 (depends on 16)

The method of claim 16, wherein said implantation process is performed on the basis of a resist mask used for introducing a dopant species into said silicon-containing semiconductor region.

### Claim 18 (depends on 16)

The method of claim 16, further comprising forming an implantation mask after forming said threshold-adjusting semiconductor material and performing said implantation process on the basis of said implantation mask.

### Claim 19 (depends on 15)

The method of claim 15, wherein providing said strain-adjusting species comprises incorporating a non-silicon species during an epitaxial growth process that is performed to form said threshold-adjusting semiconductor material.

### Claim 20 (depends on 15)

The method of claim 15, wherein said threshold-adjusting semiconductor material comprises a silicon/germanium alloy.

### Claim 21

A transistor, comprising:
a silicon-containing semiconductor region formed above a substrate;
a gate electrode structure formed above said silicon-containing semiconductor region, said gate electrode structure comprising a high-k gate insulation layer and a metal-containing electrode material formed on said high-k gate insulation layer; and
a channel region comprising a threshold-adjusting semiconductor material comprising a first tetravalent non-silicon species that is in contact with said high-k gate insulation layer, said channel region further comprising a strain adjustment tetravalent non-silicon species that is different from a said first non-silicon species.

### Claim 22 (depends on 21)

The semiconductor device of claim 21, wherein said strain adjustment species is carbon.

### Claim 23 (depends on 21)

The semiconductor device of claim 21, wherein said first non-silicon species comprises germanium.

### Claim 24 (depends on 23)

The semiconductor device of claim 23, wherein a concentration of said first non-silicon species is approximately 20 atomic percent or more.

### Claim 25 (depends on 24)

The semiconductor device of claim 24, wherein a concentration of said strain-adjusting species is approximately one atomic percent or more.
