# US 2010/0164014 A1 · Reduction of threshold voltage variation in transistors comprising a channel semiconductor alloy by reducing deposition non-uniformities

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2010/0164014 A1
- Document ID: US20100164014A1
- Status: Published application
- Kind: A1
- Application number: 12/637,112
- Filed: 2009-12-14
- Published: 2010-07-01
- Earliest claimed: 2008-12-31
- Assignees: Advanced Micro Devices, Inc.
- Inventors: Stephan Kronholz; Andreas Ott
- Web page: https://patentgrep.com/patent/US20100164014A1

## CPC

- H10D 84/038: {using silicon technology, e.g. SiGe}
- H10D 84/0128: {Manufacturing their channels}
- H10D 84/014: {the gate conductors having different materials or different implants}
- H10D 84/0167: {Manufacturing their channels}
- H10D 84/0177: {the gate conductors having different materials or different implants}
- H10D 86/01: Manufacture or treatment
- H10D: INORGANIC ELECTRIC SEMICONDUCTOR DEVICES

## Abstract

A threshold adjusting semiconductor material, such as a silicon/germanium alloy, may be provided selectively for one type of transistors on the basis of enhanced deposition uniformity. For this purpose, the semiconductor alloy may be deposited on the active regions of any transistors and may subsequently be patterned on the basis of a highly controllable patterning regime. Consequently, threshold variability may be reduced.

## Claims

### Claim 1

A method, comprising:
forming a layer of a silicon-containing semiconductor alloy on a first silicon-containing crystalline semiconductor region and a second silicon-containing crystalline semiconductor region;
removing said layer of silicon-containing semiconductor alloy selectively from said second silicon-containing crystalline semiconductor region;
forming a first gate electrode structure of a first transistor on said layer of a silicon-containing semiconductor alloy, said first gate electrode structure comprising a high-k dielectric gate insulation layer and a metal-containing gate electrode material formed on said high-k dielectric gate insulation layer; and
forming a second gate electrode structure of a second transistor above said second silicon-containing crystalline semiconductor region, said second gate electrode structure comprising a high-k dielectric gate insulation layer and a metal-containing gate electrode material formed on said high-k dielectric gate insulation layer of said second gate electrode structure.

### Claim 2 (depends on 1)

The method of claim 1, wherein removing said layer of silicon-containing semiconductor alloy comprises forming a hard mask layer selectively above said first silicon-containing crystalline semiconductor region and performing an etch process on the basis of said hard mask layer.

### Claim 3 (depends on 2)

The method of claim 2, wherein performing said etch process comprises applying a wet chemical etch recipe.

### Claim 4 (depends on 3)

The method of claim 3, wherein performing said etch process comprises applying a wet chemical etch recipe on the basis of tetra methyl ammonia hydroxide (TMAH).

### Claim 5 (depends on 1)

The method of claim 1, further comprising performing a further etch process to remove said hard mask layer.

### Claim 6 (depends on 1)

The method of claim 1, wherein forming said layer of silicon-containing semiconductor alloy comprises performing a selective epitaxial growth process to suppress material deposition on an isolation structure that laterally separates said first and second silicon-containing crystalline semiconductor regions.

### Claim 7 (depends on 1)

The method of claim 1, further comprising forming an isolation structure prior to forming said layer of silicon-containing semiconductor alloy, wherein said isolation structure laterally separates said first and second silicon-containing crystalline semiconductor regions.

### Claim 8 (depends on 1)

The method of claim 1, further comprising forming an isolation structure after forming said layer of silicon-containing semiconductor alloy, wherein said isolation structure laterally separates said first and second silicon-containing crystalline semiconductor regions.

### Claim 9 (depends on 1)

The method of claim 1, further comprising introducing a first dopant species in said first silicon-containing crystalline semiconductor region and a second dopant species in said second silicon-containing crystalline semiconductor region after forming said layer of silicon-containing semiconductor alloy.

### Claim 10 (depends on 9)

The method of claim 9, further comprising forming a mask layer above said layer of silicon-containing semiconductor alloy prior to introducing said first and second dopant species.

### Claim 11 (depends on 10)

The method of claim 10, further comprising removing said mask layer from above said second silicon-containing crystalline semiconductor region on the basis of an implantation mask used for introducing said first dopant species.

### Claim 12 (depends on 11)

The method of claim 11, further comprising forming an isolation structure laterally between said first and second silicon-containing crystalline semiconductor regions prior to forming said layer of silicon-containing semiconductor alloy.

### Claim 13 (depends on 11)

The method of claim 11, further comprising forming an isolation structure laterally between said first and second silicon-containing crystalline semiconductor regions after forming said layer of silicon-containing semiconductor alloy.

### Claim 14 (depends on 1)

The method of claim 1, wherein said semiconductor alloy comprises a silicon/germanium alloy.

### Claim 15

A method, comprising:
forming a threshold adjusting semiconductor material on first and second silicon-containing semiconductor regions;
introducing a dopant species in said second silicon-containing semiconductor region by using an implantation mask covering said first silicon-containing semiconductor region;
removing said threshold adjusting semiconductor material selectively from said second silicon-containing semiconductor region on the basis of said implantation mask; and
forming a first gate electrode structure of a first transistor on said threshold adjusting semiconductor material and a second gate electrode structure of a second transistor on said second silicon-containing semiconductor region, said first and second gate electrode structures comprising a high-k dielectric material and a metal-containing electrode material formed on said high-k dielectric material.

### Claim 16 (depends on 15)

The method of claim 15, wherein removing said threshold adjusting semiconductor material selectively from said second silicon-containing semiconductor region comprises forming a mask layer, patterning said mask layer by using said implantation mask and etching said threshold adjusting semiconductor material by using said patterned mask layer as an etch mask.

### Claim 17 (depends on 16)

The method of claim 16, wherein etching said threshold adjusting material comprises performing a wet chemical etch process.

### Claim 18 (depends on 17)

The method of claim 17, wherein said wet chemical etch process is performed on the basis of tetra methyl ammonia hydroxide (TMAH).

### Claim 19 (depends on 15)

The method of claim 15, further comprising forming an isolation structure laterally between said first and second silicon-containing semiconductor regions prior to forming said threshold adjusting semiconductor material.

### Claim 20 (depends on 15)

The method of claim 15, further comprising forming an isolation structure laterally between said first and second silicon-containing semiconductor regions after forming said threshold adjusting semiconductor material.

### Claim 21 (depends on 15)

The method of claim 15, wherein said threshold adjusting semiconductor material comprises a silicon/germanium alloy.

### Claim 22

A semiconductor device, comprising:
a first device region comprising a plurality of densely packed first P-channel transistors defining a pitch of approximately 100 nm or less, each of said first P-channel transistors being formed in and above a first silicon-containing semiconductor region and comprising a first layer of a threshold adjusting semiconductor alloy in a channel region of each of said first P-channel transistors; and
a second device region comprising a plurality of second P-channel transistors defining a pitch of more than 100 nm, each of said second P-channel transistors being formed in and above a second silicon-containing semiconductor region and comprising a second layer of said threshold adjusting semiconductor alloy in a channel region of each of said second P-channel transistors, wherein a degree of uniformity of at least one of a material composition and a layer thickness of said first and second layers of said threshold adjusting semiconductor alloy is approximately plus/minus 2 percent.

### Claim 23 (depends on 22)

The semiconductor device of claim 22, wherein said gate electrode structures of said first and second P-channel transistors comprise a high-k dielectric material formed above said first and second layers of threshold adjusting semiconductor material, respectively, and a metal-containing electrode material formed on said high-k dielectric material.

### Claim 24 (depends on 22)

The semiconductor device of claim 22, wherein a target thickness of said layer of threshold adjusting semiconductor material is approximately 10 nm or less.

### Claim 25 (depends on 24)

The semiconductor device of claim 24, wherein said threshold adjusting semiconductor material comprises a silicon/germanium alloy with a germanium concentration of approximately 20 atomic percent or more.